Microstructure and Mechanical Properties of Laser-Welded DP Steels Used in the Automotive Industry

被引:21
作者
He, Hanbing [1 ]
Forouzan, Farnoosh [1 ]
Volpp, Joerg [2 ]
Robertson, Stephanie M. [2 ]
Vuorinen, Esa [1 ]
机构
[1] Lulea Univ Technol, Div Mat Sci, S-97187 Lulea, Sweden
[2] Lulea Univ Technol, Div Prod & Prod Dev, S-97187 Lulea, Sweden
关键词
laser welding; dual phase steel; similar; dissimilar welded joints; microhardness; tensile properties; fatigue;
D O I
10.3390/ma14020456
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The aim of this work was to investigate the microstructure and the mechanical properties of laser-welded joints combined of Dual Phase DP800 and DP1000 high strength thin steel sheets. Microstructural and hardness measurements as well as tensile and fatigue tests have been carried out. The welded joints (WJ) comprised of similar/dissimilar steels with similar/dissimilar thickness were consisted of different zones and exhibited similar microstructural characteristics. The trend of microhardness for all WJs was consistent, characterized by the highest value at hardening zone (HZ) and lowest at softening zone (SZ). The degree of softening was 20 and 8% for the DP1000 and DP800 WJ, respectively, and the size of SZ was wider in the WJ combinations of DP1000 than DP800. The tensile test fractures were located at the base material (BM) for all DP800 weldments, while the fractures occurred at the fusion zone (FZ) for the weldments with DP1000 and those with dissimilar sheet thicknesses. The DP800-DP1000 weldment presented similar yield strength (YS, 747 MPa) and ultimate tensile strength (UTS, 858 MPa) values but lower elongation (EI, 5.1%) in comparison with the DP800-DP800 weldment (YS 701 MPa, UTS 868 MPa, EI 7.9%), which showed similar strength properties as the BM of DP800. However, the EI of DP1000-DP1000 weldment was 1.9%, much lower in comparison with the BM of DP1000. The DP800-DP1000 weldment with dissimilar thicknesses showed the highest YS (955 MPa) and UTS (1075 MPa) values compared with the other weldments, but with the lowest EI (1.2%). The fatigue fractures occurred at the WJ for all types of weldments. The DP800-DP800 weldment had the highest fatigue limit (348 MPa) and DP800-DP1000 with dissimilar thicknesses had the lowest fatigue limit (<200 MPa). The fatigue crack initiated from the weld surface.
引用
收藏
页码:1 / 14
页数:14
相关论文
共 50 条
  • [21] Reinforcement of laser-welded stainless steels by surface mechanical attrition treatment
    Chen, A. Y.
    Jia, Y. Q.
    Pan, D.
    Li, X.
    Lu, J.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2013, 571 : 161 - 166
  • [22] Microstructure and Mechanical Properties of Laser-Welded Joints between DP590 Dual-Phase Steel and 304 Stainless Steel with Preset Nickel Coating
    Zhang, Hua
    Xu, Jiahui
    Hao, Desheng
    Esmail, Othman Mohammed Ali Othman
    MATERIALS, 2023, 16 (07)
  • [23] Weldability, microstructure and mechanical properties of laser-welded selective laser melted 304 stainless steel joints
    Jingjing Yang
    Yun Wang
    Fangzhi Li
    Wenpu Huang
    Guanyi Jing
    Zemin Wang
    Xiaoyan Zeng
    JournalofMaterialsScience&Technology, 2019, 35 (09) : 1817 - 1824
  • [24] Weldability, microstructure and mechanical properties of laser-welded selective laser melted 304 stainless steel joints
    Yang, Jingjing
    Wang, Yun
    Li, Fangzhi
    Huang, Wenpu
    Jing, Guanyi
    Wang, Zemin
    Zeng, Xiaoyan
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2019, 35 (09) : 1817 - 1824
  • [25] Experimental and numerical study on local mechanical properties and failure analysis of laser welded DP980 steels
    Jia, Qiang
    Guo, Wei
    Li, Weidong
    Peng, Peng
    Zhu, Ying
    Zou, Guisheng
    Peng, Yun
    Tian, Zhiling
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2017, 680 : 378 - 387
  • [26] Influence of stress corrosion on the mechanical properties of laser-welded titanium
    Ferreira, Nancy de Assis
    Senna, Plinio Mendes
    Baptista do Lago, Dalva Cristina
    de Senna, Lilian Ferreira
    Sampaio-Filho, Helio Rodrigues
    JOURNAL OF PROSTHETIC DENTISTRY, 2016, 115 (03) : 356 - 362
  • [27] Influence of Welding Parameters on the Mechanical Properties of a Laser-Welded Joint
    Siltanen, Jukka
    17TH NORDIC LASER MATERIALS PROCESSING CONFERENCE (NOLAMP17), 2019, 36 : 232 - 239
  • [28] Microstructure and Hardness Profiles of Bifocal Laser-Welded DP-HSLA Steel Overlap Joints
    Grajcar, A.
    Matter, P.
    Stano, S.
    Wilk, Z.
    Rozanski, M.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2017, 26 (04) : 1920 - 1928
  • [29] Microstructure and Hardness Profiles of Bifocal Laser-Welded DP-HSLA Steel Overlap Joints
    A. Grajcar
    P. Matter
    S. Stano
    Z. Wilk
    M. Różański
    Journal of Materials Engineering and Performance, 2017, 26 : 1920 - 1928
  • [30] Microstructural evolution and mechanical properties of laser-welded joints of medium manganese steel
    Cao, Yang
    Luo, Chong
    Zhao, Lin
    Peng, Yun
    Song, Liang
    Ma, Cheng-yong
    Tian, Zhi-ling
    Zhong, Min-lin
    Wang, Yan-jie
    JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2020, 27 (01) : 75 - 87