Dynamic vulcanization of natural rubber/high-density polyethylene blends: Effect of compatibilization, blend ratio and curing system

被引:81
作者
Nakason, Charoen
Nuansomsri, Krungjit
Kaesaman, Azizon
Kiatkamjornwong, Suda [1 ]
机构
[1] Chulalongkorn Univ, Fac Sci, Dept Imaging & Printing Technol, Multidisciplinary Program Petrochem & Polymer Sci, Bangkok 10330, Thailand
[2] Prince Songkla Univ, Fac Sci & Technol, Dept Rubber Technol & Polymer Sci, Pattani 94000, Thailand
关键词
natural rubber (NR); thermoplastic vulcanizate (TPV); high-density polyethylene; compatibilizers;
D O I
10.1016/j.polymertesting.2006.05.001
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Thermoplastic vulcanizates (TPVs) based on NR/HDPE blends with various types of blend compatibilizers were prepared. It was found that TPVs with phenolic resin (i.e., SP-1045 and HRJ-10518) compatibilizers showed higher tensile strength, elongation at break and tendency to recover from prolonged extension than those of the TPV without a compatibilizer. This may be attributed to Chroman ring structures from the reaction of NR and phenolic molecules. The TPVs with modified phenolic resins (PhSP-PE and PhHRJ-PE) showed higher tensile strength and elongation at break than those of the TPVs with un-modified phenolic rein and without a compatibilizer. A reaction took place through trace quantities of un-saturation in the HDPE molecules and methylol groups in the phenolic molecules. Also, the remaining methylol groups in the phenolic molecules were capable of reacting with NR molecules and produced a linkage between NR and HDPE molecules. Therefore, it was found that the TPV with PhHRJ-PE gave the highest tensile strength and elongation at break. Increasing the content of the NR gave an increased trend of elongation at break but decreasing trends in permanent set (expressed as tension set), tensile strength and hardness. Various vulcanization systems were also used to prepare the TPV, with a mixed curing system showing the highest shear stress and tensile strength, whilst the sulphur curing system gave the lowest values, and the peroxide curing system exhibited intermediate values. (C) 2006 Elsevier Ltd. All rights reserved.
引用
收藏
页码:782 / 796
页数:15
相关论文
共 27 条
[1]   Dynamically vulcanized thermoplastic elastomers [J].
AbdouSabet, S ;
Puydak, RC ;
Rader, CP .
RUBBER CHEMISTRY AND TECHNOLOGY, 1996, 69 (03) :476-494
[2]   BLENDING OF NATURAL-RUBBER WITH LINEAR LOW-DENSITY POLYETHYLENE [J].
ABDULLAH, I ;
AHMAD, S ;
SULAIMAN, CS .
JOURNAL OF APPLIED POLYMER SCIENCE, 1995, 58 (07) :1125-1133
[3]   NATURAL RUBBER-HDPE BLENDS WITH LIQUID NATURAL-RUBBER AS A COMPATIBILIZER .1. THERMAL AND MECHANICAL-PROPERTIES [J].
AHMAD, S ;
ABDULLAH, I ;
SULAIMAN, CS ;
KOHJIYA, S ;
YOON, JR .
JOURNAL OF APPLIED POLYMER SCIENCE, 1994, 51 (08) :1357-1363
[4]   SHORT FIBER-REINFORCED THERMOPLASTIC ELASTOMERS FROM BLENDS OF NATURAL-RUBBER AND POLYETHYLENE [J].
AKHTAR, S ;
DE, PP ;
DE, SK .
JOURNAL OF APPLIED POLYMER SCIENCE, 1986, 32 (05) :5123-5146
[5]   Thermoplastic elastomers from blends of polystyrene and natural rubber: morphology and mechanical properties [J].
Asaletha, R ;
Kumaran, MG ;
Thomas, S .
EUROPEAN POLYMER JOURNAL, 1999, 35 (02) :253-271
[6]   In situ compatibilization of polyamide 6/natural rubber blends with maleic anhydride [J].
Carone, E ;
Kopcak, U ;
Gonçalves, MC ;
Nunes, SP .
POLYMER, 2000, 41 (15) :5929-5935
[7]  
Dahlan HM, 2000, J APPL POLYM SCI, V78, P1776, DOI 10.1002/1097-4628(20001205)78:10<1776::AID-APP90>3.0.CO
[8]  
2-G
[9]   Radiation crosslinked thermoplastics natural rubber (TPNR) foams [J].
Ghazali, Z ;
Johnson, AF ;
Dahlan, KZ .
RADIATION PHYSICS AND CHEMISTRY, 1999, 55 (01) :73-79
[10]   Thermoplastic elastomers based on polypropylene/natural rubber and polypropylene/recycle rubber blends [J].
Ismail, H ;
Suryadiansyah .
POLYMER TESTING, 2002, 21 (04) :389-395