Role of cold rolled followed by annealing on improvement of hydrogen induced cracking resistance in pipeline steel

被引:31
|
作者
Mohtadi-Bonab, M. A. [1 ]
Eskandari, M. [2 ]
Szpunar, J. A. [3 ]
机构
[1] Univ Bonab, Dept Mech Engn, Velayat Highway, Bonab, Iran
[2] Shahid Chamran Univ Ahvaz, Fac Engn, Dept Mat Sci & Engn, Ahvaz, Iran
[3] Univ Saskatchewan, Dept Mech Engn, 57 Campus Dr, Saskatoon, SK S7N5A9, Canada
基金
加拿大自然科学与工程研究理事会;
关键词
Hydrogen induced cracking; Crystallographic texture; X-ray diffraction; Pole figure; Electron backscatter diffraction; STRESS-CORROSION CRACKING; CRYSTALLOGRAPHIC TEXTURE; MICROSTRUCTURE; SUSCEPTIBILITY; PERMEATION; INCLUSIONS; FRACTURE; GROWTH;
D O I
10.1016/j.engfailanal.2018.04.044
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
In this study, we investigated the effect of cold rolled followed by annealing on hydrogen induced cracking susceptibility in an API X60 pipeline steel. To this, we carried out cold rolling on X60 steel up to 20%, 50% and 90% in thickness reduction to change the microstructure and texture of steel. Then, we annealed all specimens at 850 degrees C for 90 s. We studied all tested specimens by electron backscatter and X-ray diffraction techniques. EBSD results showed that the grain refinement process was properly done via cold rolling and annealing treatments in tested specimens. However, the dislocation density was high for all tested steels. Moreover, electrochemical hydrogen charging experiment on tested steels proved that all specimens were still highly susceptible to hydrogen induced cracking. Therefore, we increased the annealing temperature and its duration of the 90% cold rolled specimen (the specimen with finest grains) up to 950 degrees C for 5 min. Interestingly, there was no HIC crack on this steel after hydrogen charging experiment. EBSD measurements on this steel showed strong textures of {100}//ND and {111}//ND. As a result, such strong textures, low Kernel Average Misorientation data, a high proportion of recovered grains and coincidence site lattice boundaries were recognized as the most important reasons for the highest HIC resistance in the mentioned steel.
引用
收藏
页码:172 / 181
页数:10
相关论文
共 50 条
  • [41] Sour corrosion performance and sensitivity to hydrogen induced cracking in the X70 pipeline steel: Effect of microstructural variation and pearlite percentage
    Anijdan, S. H. Mousavi
    Sabzi, M.
    Park, N.
    Lee, Unhae
    INTERNATIONAL JOURNAL OF PRESSURE VESSELS AND PIPING, 2022, 199
  • [42] On the role of crystallographic texture in mitigating hydrogen-induced cracking in pipeline steels
    Venegas, V.
    Caleyo, F.
    Baudin, T.
    Espina-Hernandez, J. H.
    Hallen, J. M.
    CORROSION SCIENCE, 2011, 53 (12) : 4204 - 4212
  • [43] Hydrogen-Induced Cracking Susceptibility and Hydrogen Trapping Efficiency of theWelded MS X70 Pipeline Steel in H2S Environment
    Zhao Xiaoyu
    Huang Feng
    Gan Lijun
    Hu Qian
    Liu Jing
    ACTA METALLURGICA SINICA, 2017, 53 (12) : 1579 - 1587
  • [44] Hydrogen-Induced Cracking Resistance of Novel Cu-Bearing Pipeline Steels
    Shi Xianbo
    Yan Wei
    Wang Wei
    Shan Yiyin
    Yang Ke
    ACTA METALLURGICA SINICA, 2018, 54 (10) : 1343 - 1349
  • [45] Stress Oriented Hydrogen Induced Cracking of Linepipe Steel
    Kim, Wan Keun
    Park, Gyu Tae
    Kim, Kyoo Young
    JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2011, 18 : 121 - 128
  • [46] Investigation of the hydrogen-induced cracking of E690 steel welded joint in simulated seawater
    Fan, Endian
    Zhao, Qiyue
    Wang, Shuoyang
    Liu, Bo
    Yang, Ying
    Huang, Yunhua
    Luo, Hong
    Li, Xiaogang
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2022, 854
  • [47] Evolution of microstructure and texture in pipeline steels at different TMCP procedures with regard to hydrogen induced cracking
    Pourazizi, Reza
    Davani, Reza Khatib Zadeh
    Mohtadi-Bonab, M. A.
    Szpunar, J. A.
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2021, 46 (78) : 38741 - 38754
  • [48] Experimental observations of nucleation and crack growth paths of hydrogen-induced cracking in pipeline steel
    Entezari, Ehsan
    Velazquez, Jorge Luis Gonzalez
    Mohtadi-Bonab, M. A.
    Lopez, Diego Rivas
    Zuniga, Manuel Alejandro Beltran
    Davani, Reza Khatib Zadeh
    Szpunar, Jerzy
    ENGINEERING FAILURE ANALYSIS, 2023, 154
  • [49] Influence of precipitation behavior on mechanical properties and hydrogen induced cracking during tempering of hot-rolled API steel for tubing
    Moon, Joonoh
    Choi, Jongmin
    Han, Seong-Kyung
    Huh, Sungyul
    Kim, Seong-Ju
    Lee, Chang-Hoon
    Lee, Tae-Ho
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2016, 652 : 120 - 126
  • [50] Important Factors on the Failure of Pipeline Steels with Focus on Hydrogen Induced Cracks and Improvement of Their Resistance: Review Paper
    M. A. Mohtadi-Bonab
    H. Ghesmati-Kucheki
    Metals and Materials International, 2019, 25 : 1109 - 1134