Role of cold rolled followed by annealing on improvement of hydrogen induced cracking resistance in pipeline steel

被引:31
|
作者
Mohtadi-Bonab, M. A. [1 ]
Eskandari, M. [2 ]
Szpunar, J. A. [3 ]
机构
[1] Univ Bonab, Dept Mech Engn, Velayat Highway, Bonab, Iran
[2] Shahid Chamran Univ Ahvaz, Fac Engn, Dept Mat Sci & Engn, Ahvaz, Iran
[3] Univ Saskatchewan, Dept Mech Engn, 57 Campus Dr, Saskatoon, SK S7N5A9, Canada
基金
加拿大自然科学与工程研究理事会;
关键词
Hydrogen induced cracking; Crystallographic texture; X-ray diffraction; Pole figure; Electron backscatter diffraction; STRESS-CORROSION CRACKING; CRYSTALLOGRAPHIC TEXTURE; MICROSTRUCTURE; SUSCEPTIBILITY; PERMEATION; INCLUSIONS; FRACTURE; GROWTH;
D O I
10.1016/j.engfailanal.2018.04.044
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
In this study, we investigated the effect of cold rolled followed by annealing on hydrogen induced cracking susceptibility in an API X60 pipeline steel. To this, we carried out cold rolling on X60 steel up to 20%, 50% and 90% in thickness reduction to change the microstructure and texture of steel. Then, we annealed all specimens at 850 degrees C for 90 s. We studied all tested specimens by electron backscatter and X-ray diffraction techniques. EBSD results showed that the grain refinement process was properly done via cold rolling and annealing treatments in tested specimens. However, the dislocation density was high for all tested steels. Moreover, electrochemical hydrogen charging experiment on tested steels proved that all specimens were still highly susceptible to hydrogen induced cracking. Therefore, we increased the annealing temperature and its duration of the 90% cold rolled specimen (the specimen with finest grains) up to 950 degrees C for 5 min. Interestingly, there was no HIC crack on this steel after hydrogen charging experiment. EBSD measurements on this steel showed strong textures of {100}//ND and {111}//ND. As a result, such strong textures, low Kernel Average Misorientation data, a high proportion of recovered grains and coincidence site lattice boundaries were recognized as the most important reasons for the highest HIC resistance in the mentioned steel.
引用
收藏
页码:172 / 181
页数:10
相关论文
共 50 条
  • [31] Important Factors on the Failure of Pipeline Steels with Focus on Hydrogen Induced Cracks and Improvement of Their Resistance: Review Paper
    Mohtadi-Bonab, M. A.
    Ghesmati-Kucheki, H.
    METALS AND MATERIALS INTERNATIONAL, 2019, 25 (05) : 1109 - 1134
  • [32] Effect of Microstructure on Hydrogen Induced Cracking Behavior of a High Deformability Pipeline Steel
    Shi, Xian-bo
    Yan, Wei
    Wang, Wei
    Zhao, Lian-yu
    Shan, Yi-yin
    Yang, Ke
    JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2015, 22 (10) : 937 - 942
  • [33] Texture, local misorientation, grain boundary and recrystallization fraction in pipeline steels related to hydrogen induced cracking
    Mohtadi-Bonab, M. A.
    Eskandari, M.
    Szpunar, J. A.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2015, 620 : 97 - 106
  • [34] The mechanism of failure by hydrogen induced cracking in an acidic environment for API 5L X70 pipeline steel
    Mohtadi-Bonab, M. A.
    Szpunar, J. A.
    Basu, R.
    Eskandari, M.
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2015, 40 (02) : 1096 - 1107
  • [35] Effect of different microstructural parameters on hydrogen induced cracking in an API X70 pipeline steel
    M. A. Mohtadi-Bonab
    M. Eskandari
    R. Karimdadashi
    J. A. Szpunar
    Metals and Materials International, 2017, 23 : 726 - 735
  • [36] Effect of microstructure on hydrogen embrittlement and hydrogen-induced cracking behaviour of a high-strength pipeline steel weldment
    Zhang, Peng
    Laleh, Majid
    Hughes, Anthony E.
    Marceau, Ross K. W.
    Hilditch, Tim
    Tan, Mike Yongjun
    CORROSION SCIENCE, 2024, 227
  • [37] Characterization of inclusions of X80 pipeline steel and its correlation with hydrogen-induced cracking
    Xue, H. B.
    Cheng, Y. F.
    CORROSION SCIENCE, 2011, 53 (04) : 1201 - 1208
  • [38] Hydrogen-Induced Cracking of Laser Beam and Gas Metal Arc Welds on API X65 Steel
    Lee, Junghoon
    Kim, Myeonghyun
    Park, Yeongdo
    Park, Cheolho
    Kim, Cheolhee
    Kang, Namhyun
    KOREAN JOURNAL OF METALS AND MATERIALS, 2019, 57 (08): : 491 - 498
  • [39] Effect of manganese content and microstructure on the susceptibility of X70 pipeline steel to hydrogen cracking
    Hejazi, D.
    Haq, A. J.
    Yazdipour, N.
    Dunne, D. P.
    Calka, A.
    Barbaro, F.
    Pereloma, E. V.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2012, 551 : 40 - 49
  • [40] Contribution of the microtexture evolution induced by plastic deformation on the resistance of a hot-rolled pipeline steel to flat cleavage fracture and to brittle delamination cracking
    Tankoua, F.
    Crepin, J.
    Thibaux, P.
    Cooreman, S.
    Gourgues-Lorenzon, A-F
    INTERNATIONAL JOURNAL OF FRACTURE, 2022, 233 (02) : 211 - 237