First-principles study of the polar (111) surface of Fe3O4

被引:78
|
作者
Zhu, L. [1 ]
Yao, K. L.
Liu, Z. L.
机构
[1] Huazhong Univ Sci & Technol, Dept Phys, Wuhan 430074, Peoples R China
[2] Chinese Acad Sci, Int Ctr Mat Phys, Shenyang 110015, Peoples R China
[3] Nanjing Univ, State Key Lab Coordinat Chem, Nanjing 210093, Peoples R China
关键词
D O I
10.1103/PhysRevB.74.035409
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
We performed a systematic full-potential density functional theory study with the generalized gradient and local density approximation+U approaches on five possible (1x1) terminations of the low-index polar (111) surface of Fe3O4. Applying the concepts of first-principles thermodynamics, we analyze the composition, the structure, and the stability of the Fe3O4 (111) orientation at equilibrium with an arbitrary oxygen environment. The densities of states of the unrelaxed and relaxed Fe3O4 (111) surfaces were calculated and compared with that of bulk Fe3O4. The calculations reveal that the Fe-oct2-Fe-tet1-O1-terminated surface is energetically favored, showing metallic properties. The Fe-oct1-O2-terminated surface is more active than the other two Fe-terminated surfaces, showing half-metallic properties, similar to bulk Fe3O4. The Fe-tet1-O1-terminated surface, the O-terminated surfaces, and the surfaces with vacancy defects all show metallic properties.
引用
收藏
页数:10
相关论文
共 50 条
  • [31] First-principles study of the hydrogen adsorption and diffusion on ordered Ni3Fe(111) surface and in the bulk
    Li, Juan
    Xie, Yao-Ping
    Chen, Ye-Xin
    Wang, Bao-Wu
    Zhao, Shi-Jin
    INTERMETALLICS, 2014, 44 : 64 - 72
  • [32] First-principles study of the (110) polar surface of cubic PbTiO3
    Zhang, Jian-Min
    Pang, Qing
    Xu, Ke-Wei
    Ji, Vincent
    COMPUTATIONAL MATERIALS SCIENCE, 2009, 44 (04) : 1360 - 1365
  • [33] A STEM study of twin defects in Fe3O4(111)/YZO(111)
    Gilks, D.
    Lari, L.
    Matsuzaki, K.
    Evans, R.
    McKenna, K.
    Susaki, T.
    Lazarov, V. K.
    ELECTRON MICROSCOPY AND ANALYSIS GROUP CONFERENCE 2013 (EMAG2013), 2014, 522
  • [34] Epitaxial growth of Au and Pt on Fe3O4(111) surface
    Gatel, C.
    Snoeck, E.
    SURFACE SCIENCE, 2007, 601 (04) : 1031 - 1039
  • [35] Fe3O4(111) surface structure determined by LEED crystallography
    Ritter, M.
    Weiss, W.
    Surface Science, 1999, 432 (01): : 81 - 94
  • [36] Single Gold Atom Adsorption on the Fe3O4(111) Surface
    Yu, Xiaohu
    Wang, Sheng-Guang
    Li, Yong-Wang
    Wang, Jianguo
    Jiao, Haijun
    JOURNAL OF PHYSICAL CHEMISTRY C, 2012, 116 (19): : 10632 - 10638
  • [37] Fe3O4(111) surface structure determined by LEED crystallography
    Ritter, M
    Weiss, W
    SURFACE SCIENCE, 1999, 432 (1-2) : 81 - 94
  • [38] Polar Spinel-Perovskite Interfaces: an atomistic study of Fe3O4(111)/SrTiO3(111) structure and functionality
    Gilks, Daniel
    McKenna, Keith P.
    Nedelkoski, Zlatko
    Kuerbanjiang, Balati
    Matsuzaki, Kosuke
    Susaki, Tomofumi
    Lari, Leonardo
    Kepaptsoglou, Demie
    Ramasse, Quentin
    Tear, Steve
    Lazarov, Vlado K.
    SCIENTIFIC REPORTS, 2016, 6
  • [39] Polar Spinel-Perovskite Interfaces: an atomistic study of Fe3O4(111)/SrTiO3(111) structure and functionality
    Daniel Gilks
    Keith P. McKenna
    Zlatko Nedelkoski
    Balati Kuerbanjiang
    Kosuke Matsuzaki
    Tomofumi Susaki
    Leonardo Lari
    Demie Kepaptsoglou
    Quentin Ramasse
    Steve Tear
    Vlado K. Lazarov
    Scientific Reports, 6
  • [40] Effect of Defects Disorder on the Half-Metallicity, Magnetic Properties, and Gap States of Fe3O4: a First-Principles Study
    O. Mounkachi
    R. Lamouri
    M. Hamedoun
    H. Ez-Zahraouy
    E. Salmani
    A. Benyoussef
    Journal of Superconductivity and Novel Magnetism, 2017, 30 : 3221 - 3224