Reactive air brazing of YSZ ceramic with novel Al2O3 nanoparticles reinforced Ag-CuO-Al2O3 composite filler: Microstructure and joint properties

被引:60
作者
Si, Xiaoqing [1 ]
Cao, Jian [1 ]
Song, Xiaoguo [1 ]
Qu, Yang [1 ]
Feng, Jicai [1 ]
机构
[1] Harbin Inst Technol, State Key Lab Adv Welding & Joining, Harbin 150001, Peoples R China
基金
中国国家自然科学基金;
关键词
Reactive air brazing; Yttria-stabilized zirconia; Composite filler; Microstructure; Mechanical properties; OXIDE FUEL-CELL; AG-CU-TI; DENTAL RESIN COMPOSITES; SILICATE SEALING GLASS; MECHANICAL-PROPERTIES; THERMAL-EXPANSION; STEEL JOINTS; INTERFACIAL MICROSTRUCTURE; STAINLESS-STEEL; HOLDING TIME;
D O I
10.1016/j.matdes.2016.10.062
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The YSZ ceramic coatedwith a copper layer (similar to 5 mu m) was successfully reactive air brazed using novel Al2O3 nanoparticles (NPs) reinforced Ag-CuO-Al2O3 composite filler. The effects of Al2O3 NPs content on the interfacial microstructure and joint properties were investigated. When the content of Al2O3 NPs was 8 wt.%, YSZ joints obtained fine interfacial microstructure and optimal mechanical properties. The coefficient of thermal expansion of composite filler was calculated to be 16.26 x 10(-6) K-1, presenting a decline of 12.1% compared to that of AgCuO base filler. The hardness and modulus values of braze joint slightly increased to 2.6 GPa and 164 GPa, respectively, possessing a better ability to resist deformation. Consequently, the YSZ joint possessed a maximum shear strength of 60 MPa, which was 25 MPa (similar to 71%) higher than that of the joints brazed using Ag-CuO base filler. The leakage rate of YSZ-tube/AgCuO-8Al(2)O(3)/YSZ-block samples was measured to be 3.2 +/- 0.9 x 10(-10) Pa m(3) s(-1), which met the leakage rate requirements for vacuum tight components (less than 10(-9) Pa m(3) s(-1)). It implied that this novel method was an effective way to obtain hermetic YSZ joints. (C) 2016 Elsevier Ltd. All rights reserved.
引用
收藏
页码:176 / 184
页数:9
相关论文
共 50 条
  • [41] New sealing concept for planar solid oxide fuel cells
    Weil, K. Scott
    Hardy, John S.
    Koeppel, Brian J.
    [J]. JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2006, 15 (04) : 427 - 432
  • [42] Effects of thermal cycling and thermal aging on the hermeticity and strength of silver-copper oxide air-brazed seals
    Weil, KS
    Coyle, CA
    Darsell, JT
    Xia, GG
    Hardy, JS
    [J]. JOURNAL OF POWER SOURCES, 2005, 152 (01) : 97 - 104
  • [43] Wong CP, 1999, J APPL POLYM SCI, V74, P3396, DOI 10.1002/(SICI)1097-4628(19991227)74:14<3396::AID-APP13>3.0.CO
  • [44] 2-3
  • [45] Joining of Si3N4 to Si3N4 using a AuPd(Co, Ni)-V filler alloy and the interfacial reactions
    Xiong, Hua-Ping
    Chen, Bo
    Pan, Yu
    Zhao, Hai-Sheng
    Guo, Wan-Lin
    [J]. CERAMICS INTERNATIONAL, 2014, 40 (03) : 4141 - 4148
  • [46] Effects of different whiskers on the reinforcement of dental resin composites
    Xu, HHK
    Quinn, JB
    Smith, DT
    Giuseppetti, AA
    Eichmiller, FC
    [J]. DENTAL MATERIALS, 2003, 19 (05) : 359 - 367
  • [47] Indentation modulus and hardness of whisker-reinforced heat-cured dental resin composites
    Xu, HHK
    Smith, DT
    Schumacher, G
    Eichmiller, FC
    Antonucci, JM
    [J]. DENTAL MATERIALS, 2000, 16 (04) : 248 - 254
  • [48] Cu + TiB2 composite filler for brazing Al2O3 and Ti-6Al-4V alloy
    Yang, Minxuan
    Lin, Tiesong
    He, Peng
    [J]. JOURNAL OF ALLOYS AND COMPOUNDS, 2012, 512 (01) : 282 - 289
  • [49] Interfacial microstructure and strengthening mechanism of BN-doped metal brazed Ti/SiO2-BN joints
    Yang, Z. W.
    Zhang, L. X.
    Ren, W.
    Lei, M.
    Feng, J. C.
    [J]. JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2013, 33 (04) : 759 - 768
  • [50] Investigation on silver electric adhesive doped with Al2O3 ceramic particles for sealing planar solid oxide fuel cell
    Zhou, Xiaoliang
    Sun, Kening
    Yan, Yan
    Le, Shiru
    Zhang, Naiqing
    Sun, Wang
    Wang, Peng
    [J]. JOURNAL OF POWER SOURCES, 2009, 192 (02) : 408 - 413