Thermal Degradation Mechanism of a Thermostable Polyester Stabilized with an Open-Cage Oligomeric Silsesquioxane

被引:30
作者
Bautista, Yolanda [1 ]
Gozalbo, Ana [1 ]
Mestre, Sergio [1 ]
Sanz, Vicente [1 ]
机构
[1] Jaume I Univ, Univ Inst Ceram Technol, Castellon de La Plana 12006, Spain
来源
MATERIALS | 2018年 / 11卷 / 01期
关键词
oligomeric silsesquioxane; thermal degradation; open cage structure; thermostable polyester; FTIR volatiles analysis; UNSATURATED POLYESTER; THERMOGRAVIMETRIC ANALYSIS; FIRE BEHAVIOR; RESINS; PYROLYSIS; KINETICS; NANOCOMPOSITES; DECOMPOSITION; COMPOSITES; HYBRIDS;
D O I
10.3390/ma11010022
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
A polyester composite was prepared through the polymerization of an unsaturated ester resin with styrene and an open-cage oligomeric silsesquioxane with methacrylate groups. The effect of the open-cage oligomeric silsesquioxane on the thermal stability of the thermostable polyester was studied using both thermogravimetric analysis and differential thermal analysis. The results showed that the methacryl oligomeric silsesquioxane improved the thermal stability of the polyester. The decomposition mechanism of the polyester/oligomer silsesquioxane composite was proposed by Fourier transform infrared spectroscopy (FTIR) analysis of the volatiles.
引用
收藏
页数:13
相关论文
共 37 条
  • [1] Thermal degradation studies of novel diethylene glycol based unsaturated polyesters in air
    Agrawal, JP
    Sarwade, DB
    Makashir, PS
    Mahajan, RR
    Dendage, PS
    [J]. POLYMER DEGRADATION AND STABILITY, 1998, 62 (01) : 9 - 14
  • [2] Anderson D.A., 1959, Journal of Applied Polymer Science, V1, P192, DOI 10.1002/app.1959.070010210
  • [3] THERMAL-STABILITY AND DEGRADATION STUDIES OF POLYESTER RESINS
    BANSAL, RK
    MITTAL, J
    SINGH, P
    [J]. JOURNAL OF APPLIED POLYMER SCIENCE, 1989, 37 (07) : 1901 - 1908
  • [4] Thermal degradation and fire behaviour of unsaturated polyester with chain ends modified by dicyclopentadiene
    Baudry, A
    Dufay, J
    Regnier, N
    Mortaigne, B
    [J]. POLYMER DEGRADATION AND STABILITY, 1998, 61 (03) : 441 - 452
  • [5] Improvement in Char Strength with an Open Cage Silsesquioxane Flame Retardant
    Bautista, Yolanda
    Gozalbo, Ana
    Mestre, Sergio
    Sanz, Vicente
    [J]. MATERIALS, 2017, 10 (06)
  • [6] Investigation of thermal degradation mechanism of an aliphatic polyester using pyrolysis-gas chromatography-mass spectrometry and a kinetic study of the effect of the amount of polymerisation catalyst
    Bikiaris, D. N.
    Chrissafis, K.
    Paraskevopoulos, K. M.
    Triantafyllidis, K. S.
    Antonakou, E. V.
    [J]. POLYMER DEGRADATION AND STABILITY, 2007, 92 (04) : 525 - 536
  • [7] The influence of the nature of POSSs cage's periphery on the thermal stability of a series of new bridged POSS/PS nanocomposites
    Blanco, Ignazio
    Bottino, Francesco A.
    [J]. POLYMER DEGRADATION AND STABILITY, 2015, 121 : 180 - 186
  • [8] Bruins P.F., 1976, Unsaturated polyester technology
  • [9] Thermooxidative degradation of an unsaturated polyester resin - The effect of oxygen pressure on the kinetics
    Budrugeac, P
    Segal, E
    [J]. JOURNAL OF THERMAL ANALYSIS, 1997, 49 (01): : 183 - 191
  • [10] DEGRADATION OF POLY(ETHYLENE TEREPHTHALATE)
    BUXBAUM, LH