Effect of Intercritical Annealing on the Microstructural and Mechanical Behaviours of Dual-Phase Steels

被引:1
作者
Osman, Nora
Sajuri, Zainuddin [1 ]
Mohamed, Intan Fadhlina [1 ]
Omar, Mohd Zaidi [1 ]
Junaidi, Syarif [2 ]
机构
[1] Univ Kebangsaan Malaysia, Fac Engn & Built Environm, Bangi, Malaysia
[2] Univ Sharjah, Coll Engn, Dept Mech & Nucl Engn, Sharjah 27272, U Arab Emirates
来源
JURNAL KEJURUTERAAN | 2020年 / 32卷 / 04期
关键词
Dual-phase steel; instability strain; intercritical annealing; intermediate quenching; martensite volume fraction; WORK-HARDENING BEHAVIOR; TENSILE PROPERTIES; MARTENSITE MORPHOLOGY; AUSTENITE FORMATION; VOLUME FRACTION; HEATING RATE; STRENGTH; TEMPERATURE;
D O I
10.17576/jkukm-2020-32(4)-10
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The automotive industry is the main consumer of dual-phase (DP) steels which have relatively impressive mechanical strength. DP steels are also known to have good ductility and load-bearing property because of their hard martensitic microstructure in soft ferrite grains. The main objective of this study is to determine the mechanical behaviour of DP steels with various martensite volume fractions. A heat treatment with an intermediate quenching procedure followed by three different intercritical temperatures is conducted to produce various ferrite-martensite containing DP steels with different martensite volume fractions (V-m). V-m affects the mechanical properties of steel, such as work hardening, ultimate tensile strength, yield strength and hardness. The results of the experiments conducted in this study prove that excellent work hardening and ductility are observed for DP steels with a low amount of martensite phase. Meanwhile, DP steels with high V. exhibit high tensile strength and hardness with low ductility. Considere criterion is used to analyse the work hardening behaviour of DP steels. Results indicate that a one-stage work hardening takes place in DP steels; according to Considere criterion, instability strain or uniform elongation is also slightly increased by decreasing the martensite volume fraction or increasing the work hardening rate.
引用
收藏
页码:71 / 78
页数:8
相关论文
共 33 条
[1]   Dislocation Mechanics of High-Rate Deformations [J].
Armstrong, Ronald W. ;
Li, Qizhen .
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2015, 46A (10) :4438-4453
[2]   Influence of martensite content and morphology on tensile and impact properties of high-martensite dual-phase steels [J].
Bag, A ;
Ray, KK ;
Dwarakadasa, ES .
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1999, 30 (05) :1193-1202
[3]   Effect of holding time at an intercritical temperature on the microstructure and tensile properties of a ferrite-martensite dual phase steel [J].
Balbi, M. ;
Alvarez-Armas, I ;
Armas, A. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2018, 733 :1-8
[4]  
Balliger N. K., 2014, MET SCI, V15, P95
[5]   Temperature dependence of strain hardening and plastic instability behaviors in austenitic stainless steels [J].
Byun, TS ;
Hashimoto, N ;
Farrell, K .
ACTA MATERIALIA, 2004, 52 (13) :3889-3899
[6]   Deformation and fracture mechanisms in fine- and ultrafine-grained ferrite/martensite dual-phase steels and the effect of aging [J].
Calcagnotto, Marion ;
Adachi, Yoshitaka ;
Ponge, Dirk ;
Raabe, Dierk .
ACTA MATERIALIA, 2011, 59 (02) :658-670
[7]   Influence of martensite morphology on the work-hardening behavior of high strength ferrite-martensite dual-phase steel [J].
Das, Debdulal ;
Chattopadhyay, Partha Protim .
JOURNAL OF MATERIALS SCIENCE, 2009, 44 (11) :2957-2965
[8]   Effects of inter-critical temperatures on martensite morphology, volume fraction and mechanical properties of dual-phase steels obtained from direct and continuous annealing cycles [J].
Ghaheri, Ali ;
Shafyei, Ali ;
Honarmand, Mehrdad .
MATERIALS & DESIGN, 2014, 62 :305-319
[9]   Effect of chemical composition, martensite volume fraction and tempering on tensile behaviour of dual phase steels [J].
Gunduz, Suleyman .
MATERIALS LETTERS, 2009, 63 (27) :2381-2383
[10]   The effects of the initial martensite microstructure on the microstructure and tensile properties of intercritically annealed Fe-9Mn-0.05C steel [J].
Han, Jeongho ;
Lee, Seung-Joon ;
Jung, Jae-Gil ;
Lee, Young-Kook .
ACTA MATERIALIA, 2014, 78 :369-377