Erosion and corrosion resistance of plasma electrolytic oxidized 6082 aluminum alloy surface at low and high temperatures

被引:14
作者
Algahtani, Ali [1 ,2 ]
Mahmoud, Essam R., I [3 ,4 ]
机构
[1] King Khalid Univ, Dept Mech Engn, Abha, Saudi Arabia
[2] King Khalid Univ, RCAMS, Abha, Saudi Arabia
[3] Islamic Univ Madinah, Dept Mech Engn, Madinah, Saudi Arabia
[4] CMRDI, Cairo, Egypt
来源
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T | 2019年 / 8卷 / 03期
关键词
6082-T6 Al alloy; Plasma electrolytic oxidizing; Erosion; Microstructure; Wear resistance; Corrosion resistance; HYBRID-MMCS LAYER; CERAMIC COATINGS; PROCESSING PARAMETERS; CURRENT-DENSITY; OXIDATION PEO; MAGNESIUM; BEHAVIOR; WEAR; MICROSTRUCTURE; FABRICATION;
D O I
10.1016/j.jmrt.2019.02.017
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
This paper embodies the findings of a study on improving the surface tribology of Al alloy 6082-T6 through plasma electrolytic oxidation (PEO) process. The surface macro/microstructure and composition were investigated. Electrochemical measurements were performed at temperatures of 20 and 80 degrees C using an inductively coupled plasma and open circuit potential tests after immersion in 3.5%NaCl solution. The erosion tests were performed with water carrying sand particles at different sand loadings (200 and 1000 mg/l) and temperatures (20 and 80 degrees C). After erosion experiments, the weight loss measurements were recorded, and the worn surfaces were assessed through SEM study and profilometry analysis. The micro-hardness of the coated layer and the substrate were measured before and after the erosion test. The formed PEO layer of 40 mu m thick was almost sound, uniform, well adhered to the substrate and consisted mainly of alumina phases (alpha-Al2O3, gamma-Al2O3). The relative proportions of alpha-Al2O3 to gamma-Al2O3 were 31: 79%. The PEO coating shows much better corrosion and erosion resistance and less surface damage compared to the aluminum substrate, especially at elevated temperature and high sand loading. The PEO hardness increases as the distance from the substrate increases until near the middle of the coating. (C) 2019 The Authors. Published by Elsevier B.V.
引用
收藏
页码:2699 / 2709
页数:11
相关论文
共 38 条
[1]   Fabrication of multifunctional black PEO coatings on AA7075 for spacecraft applications [J].
Arunnellaiappan, T. ;
Krishna, Rama L. ;
Anoop, S. ;
Rani, Uma R. ;
Rameshbabu, N. .
SURFACE & COATINGS TECHNOLOGY, 2016, 307 :735-746
[2]   Erosion and erosion-corrosion performance of cast and thermally sprayed nickel-aluminium bronze [J].
Barik, RC ;
Wharton, JA ;
Wood, RJK ;
Tan, KS ;
Stokes, KR .
WEAR, 2005, 259 (1-6) :230-242
[3]   A review on the mechanical methods for evaluating coating adhesion [J].
Chen, Zhaoxiang ;
Zhou, Kun ;
Lu, Xuehong ;
Lam, Yee Cheong .
ACTA MECHANICA, 2014, 225 (02) :431-452
[4]   Plasma electrolytic oxidation of magnesium and its alloys: Mechanism, properties and applications [J].
Darband, Gh. Barati ;
Aliofkhazraei, M. ;
Hamghalam, P. ;
Valizade, N. .
JOURNAL OF MAGNESIUM AND ALLOYS, 2017, 5 (01) :74-132
[5]   The mechanics of composite corrugated structures: A review with applications in morphing aircraft [J].
Dayyani, I. ;
Shaw, A. D. ;
Saavedra Flores, E. L. ;
Friswell, M. I. .
COMPOSITE STRUCTURES, 2015, 133 :358-380
[6]   Increasing thickness and protective properties of PEO-coatings on aluminum alloy [J].
Egorkin, V. S. ;
Gnedenkov, S. V. ;
Sinebryukhov, S. L. ;
Vyaliy, I. E. ;
Gnedenkov, A. S. ;
Chizhikov, R. G. .
SURFACE & COATINGS TECHNOLOGY, 2018, 334 :29-42
[7]   Plasma Electrolytic Oxidation Coatings on Titanium Formed with Microsecond Current Pulses [J].
Gnedenkov, S. V. ;
Sinebryukhov, S. L. ;
Puz, A. V. ;
Gnedenkov, A. S. ;
Vyaliy, I. E. ;
Mashtalyar, D. V. ;
Egorkin, V. S. .
PHYSICS AND TECHNOLOGY OF NANOSTRUCTURED MATERIALS II, 2014, 213 :149-153
[8]   Composite polymer-containing protective coatings on magnesium alloy MA8 [J].
Gnedenkov, S. V. ;
Sinebryukhov, S. L. ;
Mashtalyar, D. V. ;
Egorkin, V. S. ;
Sidorova, M. V. ;
Gnedenkov, A. S. .
CORROSION SCIENCE, 2014, 85 :52-59
[9]  
Grazyna M. N, 2005, J MATER PROCESS TECH, V162-163, P367, DOI DOI 10.1016/J.JMATPROTEC.2005.02.115
[10]  
Grubb JF, 2011, ATI CORR SOL C