Structure of the oxide film on Ti-6Ta alloy after immersion test in 8 mol/L boiling nitric acid medium

被引:12
作者
Guo, Dizi [1 ]
Yang, Yingli [1 ]
Wu, Jinping [1 ]
Zhao, Bin [1 ]
Zhao, Hengzhang [1 ]
Su, Hangbiao [1 ]
Lu, Yafeng [1 ]
机构
[1] Northwest Inst Nonferrous Met Res, Xian 710016, Shaanxi, Peoples R China
关键词
Titanium alloy; Hot corrosion; Oxidation; CORROSION BEHAVIOR; TITANIUM; IRRADIATION;
D O I
10.1016/j.elspec.2013.08.013
中图分类号
O433 [光谱学];
学科分类号
0703 ; 070302 ;
摘要
By using X-ray photoelectron spectroscopy (XPS), X-ray diffractometer (XRD) and scanning electron microscopy (SEM), we investigate the corrosion behavior and the structure of the oxide film of Ti-6Ta alloy that is subjected to the immersion corrosion test in 8 mol/L boiling nitric acid for 432 h. Based on the phase constitution indentified by depth profile XPS, the oxide film could be divided into three sub-layers along its thickness direction: the chemical stable TiO2 and Ta2O5 are present in layer I; the sub-oxide Ti2O3 and TaO are present in the layer II and layer III, and the high valence oxide evolutes from their sub-oxide gradually. Owing to the shielding effect of Ta2O5, the corrosion rate of the Ti-6Ta alloy decreases from 0.051 mm/y to 0.014 mm/y with increasing immersion time, showing an excellent corrosion resistance in 8 mol/L boiling nitric acid. (C) 2013 Elsevier B.V. All rights reserved.