Aluminum titanate based composite porous ceramics with both high porosity and mechanical strength prepared by a special two-step sintering method

被引:17
作者
Wang, Yirong [1 ,2 ]
Wang, Xueqian [1 ,2 ]
Liu, Chuanbao [3 ]
Su, Xiaopo [1 ,2 ]
Yu, Chengye [1 ,2 ]
Su, Yanjing [1 ,2 ]
Qiao, Lijie [1 ,2 ]
Bai, Yang [1 ,2 ]
机构
[1] Univ Sci & Technol Beijing, Beijing Adv Innovat Ctr Mat Genome Engn, Beijing 100083, Peoples R China
[2] Univ Sci & Technol Beijing, Inst Adv Mat & Technol, Beijing 100083, Peoples R China
[3] Univ Sci & Technol Beijing, Sch Mat Sci & Engn, Beijing 100083, Peoples R China
基金
中国国家自然科学基金;
关键词
Al2TiO5; Porous ceramics; Two-step sintering; Mechanical property; SOLID-STATE REACTION; OXIDE FUEL-CELL; ELECTRICAL-PROPERTIES; PORE STRUCTURES; GRAIN-GROWTH; MICROSTRUCTURE; TIO2; BEHAVIOR; POWDER; AL2O3;
D O I
10.1016/j.jallcom.2020.157193
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
In this work, we develop a two-step sintering technology special for porous ceramics to resolve the contradiction between porosity and mechanical strength. It contains a first long-time sintering at the relatively low temperature (T-1) and a second fast sintering at higher temperature (T-2). Porous ceramics of aluminum titanate-strontium feldspar-mullite (ASM) ternary composite were prepared by this method, and exhibit both high porosity and high mechanical strength. The effects of T-1 and T-2 on the phase composition, microstructure, porosity, pore size distribution, mechanical strength and thermal expansion coefficient (TEC) of ASM porous ceramics are systematically studied. The sample sintered at T-1 = 1400 degrees C & T-2 = 1500 degrees C shows optimum performance: the porosity, bulk density, and mean pore diameter (D-50) are 63.48%, 1.20 g/cm3 and 15.94 mm, respectively; while the flexural strength reaches 9.22 MPa and the TEC is 2.9 x 10(-6)/K. The two-step sintering technology provides a powerful tool to develop porous ceramics with excellent comprehensive properties. (c) 2020 Elsevier B.V. All rights reserved.
引用
收藏
页数:9
相关论文
共 49 条
[41]   Preparation of porous Al2TiO5-Mullite ceramic by starch consolidation casting and its corrosion resistance characterization [J].
Xu, Guogang ;
Chen, Zhiwei ;
Zhang, Xueying ;
Cui, Hongzhi ;
Zhang, Zhihui ;
Zhan, Xiaoyuan .
CERAMICS INTERNATIONAL, 2016, 42 (12) :14107-14112
[42]   Effect of two-step sintering on micro-honeycomb BaTiO3 ceramics prepared by freeze-casting process [J].
Xu, Tingting ;
Wang, Chang-An .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2016, 36 (10) :2647-2652
[43]   Synthesis of low-cost porous ceramic microspheres from waste gangue for dye adsorption [J].
Yan, Shu ;
Pan, Yiming ;
Wang, Lu ;
Liu, Jingjing ;
Zhang, Zaijuan ;
Huo, Wenlong ;
Yang, Jinlong ;
Huang, Yong .
JOURNAL OF ADVANCED CERAMICS, 2018, 7 (01) :30-40
[44]   Heat and water recovery from flue gas: Application of micro-porous ceramic membrane tube bundles in gas-fired power plant [J].
Yang, Boran ;
Chen, Haiping .
CHEMICAL ENGINEERING AND PROCESSING-PROCESS INTENSIFICATION, 2019, 137 :116-127
[45]   In situ porous alumina/aluminum titanate ceramic composite prepared by spark plasma sintering from nanostructured powders [J].
Yang, Yong ;
Wang, You ;
Tian, Wei ;
Wang, Zheng ;
Li, Chong-gui ;
Zhao, Yue ;
Bian, Han-min .
SCRIPTA MATERIALIA, 2009, 60 (07) :578-581
[46]   Processing and piezoelectric properties of porous PZT ceramics [J].
Zeng, Tao ;
Dong, XianLin ;
Chen, ShuTao ;
Yang, Hong .
CERAMICS INTERNATIONAL, 2007, 33 (03) :395-399
[47]   Microstructure and electrical properties of porous PZT ceramics derived from different pore-forming agents [J].
Zhang, H. L. ;
Li, Jing-Feng ;
Zhang, Bo-Ping .
ACTA MATERIALIA, 2007, 55 (01) :171-181
[48]   An initial study on SiCw-reinforced Al2TiO5 composites [J].
Zhang, YJ ;
Yin, YS .
MATERIALS LETTERS, 2000, 46 (2-3) :147-148
[49]   Aluminum titanate-calcium dialuminate composites with low thermal expansion and high strength [J].
Zhao, Genfa ;
Bai, Yang ;
Qiao, Lijie .
JOURNAL OF ALLOYS AND COMPOUNDS, 2016, 656 :1-4