Empirical Prediction of Carbon-Steel Degradation Rates on an Offshore Oil and Gas Facility: Predicting CO2 Erosion-Corrosion Pipeline Failures Before They Occur

被引:16
作者
Barker, R. [1 ]
Hu, X.
Neville, A. [2 ]
Cushnaghan, S. [3 ]
机构
[1] Univ Leeds, Sch Mech Engn, Inst Engn Thermofluids Surfaces & Interfaces, Leeds LS2 9JT, W Yorkshire, England
[2] Univ Leeds, Leeds LS2 9JT, W Yorkshire, England
[3] Shell UK Ltd, London, England
来源
SPE JOURNAL | 2014年 / 19卷 / 03期
关键词
DIOXIDE CORROSION; MECHANISTIC MODEL; JET IMPINGEMENT; MILD-STEEL;
D O I
10.2118/163143-PA
中图分类号
TE [石油、天然气工业];
学科分类号
0820 ;
摘要
Various sections of carbon-steel pipework removed from an offshore facility were found to have experienced severe degradation, partly attributed to an insufficient inhibitor dose rate, as discussed in a previous case study (Hu et al. 2011b). An investigation was conducted to compare the predictive capability of an empirical model generated with data from a submerged-impinging-jet laboratory apparatus. The model was assessed in its ability to determine the rate of thickness loss for carbon-steel pipework subjected to a CO2-containing erosion-corrosion environment, reviewing to what extent the prediction agrees with inspection data. The investigation considers whether the developed tool could have predicted pipework failures on the facility, comparing it with the degradation rate calculated from a leak that occurred within the past 2 years. The program of experiments set out to create a means of prediction with the material-loss data from submerged-impinging-jet tests over a range of conditions replicating those within the line. Information pertaining to the temperature, production rate, and sand loading was collated for the offshore facility. These data were used along with mass-loss results to predict the degradation rate on the asset as a function of time over a 5-year period. This in turn was used to predict the total thickness loss of the pipework wall as a function of time. Consideration was also given to the current use of inhibition (10 ppm Inhibitor A) as well as the predicted thickness losses as a function of time had a candidate inhibitor been used instead (50 ppm Inhibitor B). Limitations of the model are presented, along with suggestions for ways to develop the model further.
引用
收藏
页码:425 / 436
页数:12
相关论文
共 34 条
  • [1] Al-Mutahar F.M., 2012, CORROSION 2012
  • [2] [Anonymous], 2005, M506 NORSOK
  • [3] [Anonymous], CORROSION 2008
  • [4] Numerical and experimental investigation of the relative erosion severity between plugged tees and elbows in dilute gas/solid two-phase flow
    Chen, Xianghui
    McLaury, Brenton S.
    Shirazi, Siarnack A.
    [J]. WEAR, 2006, 261 (7-8) : 715 - 729
  • [5] de Waard C., CORROSION, V47, P976
  • [6] de Waard C., 2003, CORROSION 2003
  • [7] de Waard C., 1993, CORROSION 93
  • [8] CARBONIC-ACID CORROSION OF STEEL
    DEWAARD, C
    MILLIAMS, DE
    [J]. CORROSION, 1975, 31 (05) : 177 - 181
  • [9] Efird K.D., 2006, CORROSION 2006
  • [10] Efird K.D., 2000, CORROSION 2000