Degradation of plasma-treated poly(p-phenylene benzobisoxazole) fiber and its adhesion with bismaleimide resin

被引:6
作者
Liu, Zhe [1 ]
Chen, Ping [1 ,2 ]
Zhang, Xiaoliang [1 ]
Yu, Qi [2 ]
机构
[1] Dalian Univ Technol, Sch Chem Engn, Minist Educ, Key Lab Mat Modificat Laser Ion & Electron Beams, Dalian 116024, Peoples R China
[2] Shenyang Aerosp Univ, Liaoning Key Lab Adv Polymer Matrix Composites Mf, Shenyang 110136, Peoples R China
基金
中国国家自然科学基金;
关键词
DIELECTRIC BARRIER DISCHARGE; REINFORCED POLYMER COMPOSITES; SURFACE MODIFICATION; OXYGEN PLASMA; PBO FIBERS; MECHANICAL-PROPERTIES; FILM; WETTABILITY; BEHAVIOR;
D O I
10.1039/c3ra46192k
中图分类号
O6 [化学];
学科分类号
0703 ;
摘要
Degradation of poly(p-phenylene benzobisoxazole) (PBO) fiber which was modified by oxygen dielectric barrier discharge (oxy-DBD) plasma as well as its adhesion with bismaleimide (BMI) resin were studied in this paper. Surface changes of PBO fibers before and after plasma treatment were investigated by X-ray photoelectron spectroscopy (XPS), atomic force microscopy (AFM) and single fiber tensile strength (SFTS). Aging behaviors were obviously detected upon chemical changes while the morphology and surface roughness changed little. Oxygen content and O/C ratio of the fibers reduced a lot, which were from 24.83% and 0.350 to 20.88% and 0.268 after aging in air for 30 days, respectively. Furthermore, the adhesion of oxy-DBD plasma-treated PBO fibers reinforced BMI composites dropped dramatically in the first 5 aging days but had no obviously changes during 5-30 days, and the degradation ratio was about 18%. Otherwise, the damage to the tensile strength of single fibers caused by oxy-DBD plasma can be ignored with only 4.8% reduction and showed little change during the aging time (30 days). However, the aging effects did not recover the fiber surfaces to the original state, indicating that some permanent changes were generated in the fiber surfaces. Furthermore, the water absorption varied from different composites and all the samples had good humid resistance properties.
引用
收藏
页码:3893 / 3899
页数:7
相关论文
共 28 条
  • [1] Hydrophilization and hydrophobic recovery of PDMS by oxygen plasma and chemical treatment - An SEM investigation
    Bodas, Dhananjay
    Khan-Malek, Chantal
    [J]. SENSORS AND ACTUATORS B-CHEMICAL, 2007, 123 (01) : 368 - 373
  • [2] Dielectric barrier discharge for surface treatment: application to selected polymers in film and fibre form
    Borcia, G
    Anderson, CA
    Brown, NMD
    [J]. PLASMA SOURCES SCIENCE & TECHNOLOGY, 2003, 12 (03) : 335 - 344
  • [3] Chen JR, 1999, J APPL POLYM SCI, V72, P1327
  • [4] Modification of the surface properties of a polypropylene (PP) film using an air dielectric barrier discharge plasma
    Cui, NY
    Brown, NMD
    [J]. APPLIED SURFACE SCIENCE, 2002, 189 (1-2) : 31 - 38
  • [5] Dirk H., 2008, NUCL INSTRUM METH B, V2003, P281
  • [6] Durability of the wettability properties of a polypropylene film with a low-pressure CH4-O2 plasma treatment
    Garcia, D.
    Fenollar, O.
    Lopez, R.
    Sanchis, R.
    Balart, R.
    [J]. JOURNAL OF APPLIED POLYMER SCIENCE, 2008, 110 (02) : 1201 - 1207
  • [7] The aging of atmospheric plasma-treated ultrahigh-modulus polyethylene fibers
    Jensen, C
    Zhang, C
    Qiu, Y
    [J]. COMPOSITE INTERFACES, 2003, 10 (2-3) : 277 - 285
  • [8] Oxygen and nitrogen plasma hydrophilization and hydrophobic recovery of polymers
    Jokinen, Ville
    Suvanto, Pia
    Franssila, Sami
    [J]. BIOMICROFLUIDICS, 2012, 6 (01):
  • [9] Application of plasma technologies in fibre-reinforced polymer composites: A review of recent developments
    Li, RZ
    Ye, L
    Mai, YW
    [J]. COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING, 1997, 28 (01) : 73 - 86
  • [10] Statistical analysis of the effect of dielectric barrier discharge (DBD) operating parameters on the surface processing of poly(methylmethacrylate) film
    Liu, CZ
    Brown, NMD
    Meenan, BJ
    [J]. SURFACE SCIENCE, 2005, 575 (03) : 273 - 286