Oxidation protection of gamma-titanium aluminide using glass-ceramic coatings

被引:85
作者
Sarkar, S. [1 ]
Datta, S. [1 ]
Das, S. [1 ]
Basu, D. [1 ]
机构
[1] Cent Glass & Ceram Res Inst, Bio Ceram & Coating Div, Kolkata 700032, India
关键词
gamma-TiAl; Glass-ceramics; Coatings; Processing; Isothermal oxidation; HIGH-TEMPERATURE OXIDATION; BEHAVIOR; RESISTANCE; ALLOYS; AL; 900-DEGREES-C; IMPROVEMENT; AIR; CR; SI;
D O I
10.1016/j.surfcoat.2008.12.029
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
gamma-TiAl intermetallic alloys are presently considered an efficient structural material for advanced turbine blades and aero-engine components due to their various advantages compared to the traditionally used superalloys. However. their poor oxidation resistance at temperatures >750 degrees C severely limits their wider application. The present study dealt with the improvement of oxidation resistance of this alloy by applying impervious glass-ceramic coatings by vitreous enameling technique. Results showed that MgO-SiO2-TiO2 glass-ceramic coating could offer excellent oxidation resistance to gamma-TiAl at 800 degrees C even up to 100 h with negligible weight gain (similar to 0.10 mg/cm(2)) compared to that of the bare alloy (similar to 1.3 mg/cm(2)). The coatings those were belonging from BaO-MgO-SiO2, ZnO-Al2O3-SiO2 and BaO-SiO2 systems also extend appreciable improvement in the oxidation resistance of the alloy at 800 degrees C upto 100 h. At further higher temperature such as at 1000 degrees C, the ABK-13 and ABK-103 glass-ceramic coatings offered significant protection to the alloy up to 25 h of exposure in air with minimum weight gain (similar to 0.34 mg/cm(2)). However, after that the coated layers started to peel off from the alloy surface. (C) 2008 Elsevier B.V. All rights reserved.
引用
收藏
页码:1797 / 1805
页数:9
相关论文
共 30 条
[1]  
ANDRUS RL, Patent No. 5298332
[2]   Oxidation subscale of gamma-titanium aluminide [J].
Beye, R ;
Verwerft, M ;
DeHosson, JTM ;
Gronsky, R .
ACTA MATERIALIA, 1996, 44 (10) :4225-4231
[3]   The oxidation and protection of gamma titanium aluminides [J].
Brady, MP ;
Brindley, WJ ;
Smialek, JL ;
Locci, IE .
JOM-JOURNAL OF THE MINERALS METALS & MATERIALS SOCIETY, 1996, 48 (11) :46-50
[4]  
Clemens H, 2000, ADV ENG MATER, V2, P551, DOI 10.1002/1527-2648(200009)2:9<551::AID-ADEM551>3.0.CO
[5]  
2-U
[6]   A new high temperature resistant glass-ceramic coating for gas turbine engine components [J].
Datta, S ;
Das, S .
BULLETIN OF MATERIALS SCIENCE, 2005, 28 (07) :689-696
[7]   Hydrogen permeation in gamma titanium aluminides [J].
Estupinan, H. A. ;
Uribe, I. ;
Sundaram, P. A. .
CORROSION SCIENCE, 2006, 48 (12) :4216-4222
[8]   Review of the effect of alloy composition on the growth rates of scales formed during oxidation of gamma titanium aluminide alloys [J].
Fergus, JW .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2002, 338 (1-2) :108-125
[9]   Oxidation behavior of γ-TiAl coated with zirconia thermal barriers [J].
Gauthier, V ;
Dettenwanger, F ;
Schütze, M .
INTERMETALLICS, 2002, 10 (07) :667-674
[10]   Oxidation behavior of TiAl/TiAl-SiC gradient coatings on gamma titanium aluminides [J].
Gong, SK ;
Xu, HB ;
Yu, QH ;
Zhou, CG .
SURFACE & COATINGS TECHNOLOGY, 2000, 130 (01) :128-132