AC Flashover Voltage Model for Polluted Suspension Insulators and an Experimental Investigation in Salt Fog

被引:15
作者
Dong, Bingbing [1 ]
Zhang, Zhu [1 ]
Xiang, Nianwen [1 ]
Yang, Hejun [1 ]
Xu, Shuiqing [1 ]
Cheng, Tingli [1 ]
机构
[1] Hefei Univ Technol, Sch Elect Engn & Automat, Hefei 230009, Peoples R China
基金
中国国家自然科学基金;
关键词
Insulator; fog accretion; additional salt deposit density; pollution level; flashover voltage; SURFACE CONDUCTIVITY; LEAKAGE CURRENT; PERFORMANCE; PORCELAIN; COMPONENTS;
D O I
10.1109/ACCESS.2020.3030326
中图分类号
TP [自动化技术、计算机技术];
学科分类号
0812 ;
摘要
In recent years, the electrical performance of polluted suspension insulators operating in coastal foggy regions has attracted wide attention because of the occurrence of flashover. Surface wetting by salt fog accretion increases the surface conductivity and degrades theflashover voltage of insulators. Normally, the effect of conductivity under fog condition and pre-contamination on the flashover of polluted insulators are analyzed separately. Therefore, this does not reveal the flashover characteristic in salt fog, which requires further research. This paper describes salt fog experiments with an AC test voltage conducted using suspension insulators in a 110-kV power system. The electrical strength performance of insulators with salt fog treatments is analyzed, and the effects of salt deposit density (SDD) and the fog water conductivity (FWC) on the flashover of three types of suspension insulators are studied. The concept of additional SDD is proposed to quantify analyze the effects of salt fog. The results show that there is less dependence on FWC at higher pollution levels than at lower pollution levels. That is, the effect of FWC on 50% ACflashover voltage (U50) can be neglected for SDD >0.15 mg/cm2, whereas FWC has a strong effect on U50 for SDD <0.15 mg/cm2. FWC has a greater influence on U50 of ceramic insulators than on that of silicone rubber insulator. A model for calculating the critical flashover voltage of insulators is proposed by considering the combined effect of FWC and pre-polluting SDD.
引用
收藏
页码:187411 / 187418
页数:8
相关论文
共 25 条
[1]  
[Anonymous], 2013, 42013 IEEE
[2]  
[Anonymous], 2013, IEC-60507-2013
[3]   Insulator Selection for AC Overhead Lines With Respect to Contamination [J].
Baker, A. C. ;
Farzaneh, M. ;
Gorur, R. S. ;
Gubanski, S. M. ;
Hill, R. J. ;
Karady, G. G. ;
Schneider, H. M. .
IEEE TRANSACTIONS ON POWER DELIVERY, 2009, 24 (03) :1633-1641
[4]   Measurement of Saturated Water Absorption of the Contamination Layer Deposited on Insulator Surface [J].
Cao, Bin ;
Wang, Liming ;
Yin, Fanghui .
IEEE SENSORS JOURNAL, 2019, 19 (22) :10804-10811
[5]   A Low-Cost Evaluation and Correction Method for the Soluble Salt Components of the Insulator Contamination Layer [J].
Cao, Bin ;
Wang, Liming ;
Yin, Fanghui .
IEEE SENSORS JOURNAL, 2019, 19 (13) :5266-5273
[6]   Investigations on Leakage Current and Phase Angle Characteristics of Porcelain and Polymeric Insulator under Contaminated Conditions [J].
Chandrasekar, S. ;
Kalaivanan, C. ;
Cavallini, Andrea ;
Montanari, Gian Carlo .
IEEE TRANSACTIONS ON DIELECTRICS AND ELECTRICAL INSULATION, 2009, 16 (02) :574-583
[7]   Probes for spot measurement of surface conductivity on polluted insulators [J].
Chrzan, K. L. ;
Stec, C. ;
Farzaneh, M. .
IET SCIENCE MEASUREMENT & TECHNOLOGY, 2007, 1 (05) :295-300
[8]   Frequency Distribution of Leakage Current on Silicone Rubber Insulator in Salt-Fog Environments [J].
Du, B. X. ;
Liu, Yong .
IEEE TRANSACTIONS ON POWER DELIVERY, 2009, 24 (03) :1458-1464
[9]  
Farzaneh M., 2009, INSULATORS ICING POL
[10]   Outdoor HV composite polymeric insulators [J].
Hackam, R .
IEEE TRANSACTIONS ON DIELECTRICS AND ELECTRICAL INSULATION, 1999, 6 (05) :557-585