Fracture mechanism of metal electrode integrated on a chip and fabrication of a poly(ethylene terephthalate) electrophoresis microchip

被引:1
|
作者
Liu, Chong [1 ,2 ]
Li, Jing-Min [1 ]
Liu, Jun-Shan [1 ]
Wang, Li-Ding [1 ,2 ]
Hao, Zhen-Xia [3 ]
Chen, Heng-Wu [3 ]
机构
[1] Dalian Univ Technol, Key Lab Micro Nano Technol & Syst Liaoning Prov, Dalian, Peoples R China
[2] Dalian Univ Technol, Key Lab Precis & Nontradit Machining Technol, Minist Educ, Dalian, Peoples R China
[3] Zhejiang Univ, Inst Microanalyt Syst, Dept Chem, Hangzhou 310058, Zhejiang, Peoples R China
基金
国家高技术研究发展计划(863计划); 国家自然科学基金重大项目; 中国国家自然科学基金;
关键词
Electrode fracture; Polymer deformation behavior; Synchronous observation; Finite element simulation; ELECTROCHEMICAL DETECTION; PLASMA;
D O I
10.1016/j.talanta.2009.05.048
中图分类号
O65 [分析化学];
学科分类号
070302 ; 081704 ;
摘要
Thermal bonding is an important technique to fabricate polymer electrophoresis microchip. However, the metal electrodes deposited on polymer substrate can readily fracture during the thermal bonding. In this paper, poly(ethylene terephthalate) (PET) was exploited to fabricate the electrophoresis microchip with an integrated gold electrode for amperometric detection. The fracture of the gold electrode was studied through FEA (finite element analysis) simulations, the potentially risk positions on the electrode were shown. The calculation results were tested by bonding experiments and were proven to be consistent with the experiments. Besides, an optimal bonding temperature for PET chip was also presented based on FEA simulations and bonding experiments. Considering the low surface properties of PET, oxygen plasma-assisted thermal bonding technique was used to enhance bonding. Upon treated for 150 s, the PET substrates could be thermally bonded at 62 degrees C without electrode fracture. The fabricated PET chips were demonstrated for detection of standard glucose solution. Satisfactory reproducibility was achieved. and the RSD values of peak height and migration time of the PET CE chips were 0.51% and 2.17%, respectively. (C) 2009 Published by Elsevier B.V.
引用
收藏
页码:1341 / 1347
页数:7
相关论文
共 50 条
  • [1] Modification of amorphous poly(ethylene terephthalate) surface by UV light and plasma for fabrication of an electrophoresis chip with an integrated gold microelectrode
    Hao, Zhenxia
    Chen, Hengwu
    Zhu, Xiaoying
    Li, Jingmin
    Liu, Chong
    JOURNAL OF CHROMATOGRAPHY A, 2008, 1209 (1-2) : 246 - 252
  • [2] Design and fabrication of poly(dimethylsiloxane) electrophoresis microchip with integrated electrodes
    C. C. Liu
    D. F. Cui
    Microsystem Technologies, 2005, 11 : 1262 - 1266
  • [3] Design and fabrication of poly(dimethylsiloxane) electrophoresis microchip with integrated electrodes
    Liu, CC
    Cui, DF
    MICROSYSTEM TECHNOLOGIES-MICRO-AND NANOSYSTEMS-INFORMATION STORAGE AND PROCESSING SYSTEMS, 2005, 11 (12): : 1262 - 1266
  • [4] A new fabrication process for a microchip electrophoresis device integrated with a three-electrode electrochemical detector
    Tsai, DM
    Lin, KW
    Zen, JM
    Chen, HY
    Hong, RH
    ELECTROPHORESIS, 2005, 26 (15) : 3007 - 3012
  • [5] DEFORMATION AND FRACTURE OF POLY(ETHYLENE-TEREPHTHALATE)
    SIMS, GLA
    JOURNAL OF PHYSICS D-APPLIED PHYSICS, 1976, 9 (06) : 1053 - 1062
  • [6] Electrochemical detection of anions on an electrophoresis microchip with integrated silver electrode
    Yan, JL
    Yang, XR
    Wang, EK
    ELECTROANALYSIS, 2005, 17 (13) : 1222 - 1226
  • [7] FATIGUE-FRACTURE MECHANISM OF SLOWLY NOTCHED POLY(ETHYLENE-TEREPHTHALATE) POLYMERS
    YEH, JT
    LIN, YT
    HUANG, SS
    POLYMER BULLETIN, 1994, 33 (03) : 361 - 368
  • [9] PHOTOCHEMICAL DECOMPOSITION MECHANISM OF POLY(ETHYLENE TEREPHTHALATE
    DAY, M
    WILES, DM
    JOURNAL OF POLYMER SCIENCE PART B-POLYMER LETTERS, 1971, 9 (09): : 665 - &
  • [10] SOME OBSERVATIONS ON FRACTURE OF POLY(ETHYLENE TEREPHTHALATE) FILM
    FERGUSON, RJ
    WILLIAMS, JG
    POLYMER, 1973, 14 (03) : 103 - 106