Thiosulfate-copper-ammonia leaching of pure gold and pressure oxidized concentrate

被引:5
作者
Porvali, Antti [1 ]
Rintala, Lotta [1 ]
Aromaa, Jari [1 ]
Kaartinen, Tommi [2 ]
Forsen, Olof [1 ]
Lundstrom, Mari [1 ]
机构
[1] Aalto Univ, Dept Mat Sci & Engn, POB 16200, Aalto 00076, Finland
[2] VTT Tech Res Ctr Finland, Biologinkuja 7, Espoo 02150, Finland
来源
PHYSICOCHEMICAL PROBLEMS OF MINERAL PROCESSING | 2017年 / 53卷 / 02期
基金
芬兰科学院;
关键词
gold leaching; thiosulfate; quartz crystal microbalance; OXIDATION; KINETICS; MECHANISM; SURFACES; IONS; ORES; PH;
D O I
10.5277/ppmp170231
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
In this research cyanide-free leaching of pure gold and pressure oxidized refractory gold concentrate by thiosulfate-copper-ammonia solutions were examined. A quartz crystal microbalance (QCM) was used to study gold leaching as a factorial series where the best gold leaching rate (2.987 mg/(cm(2).h)) was achieved with a solution consisting of 0.2 M (NH4)(2)S2O3, 1.2 M NH3, 0.01 M CuSO4 and 0.4 M Na2SO4. Temperature had the greatest effect on the gold leaching rate. An increase in thiosulfate concentration (0.1-0.2 M) increased gold dissolution. The combined effect of temperature and ammonia concentration had a statistically significant effect on the gold leaching rate at 0.1 M M2S2O3. Combination of applied potential and NH3:S2O3 ratio had a statistically significant effect on the gold leaching rate at 0.2 M M2S2O3. An increase in applied potential decreased the gold dissolution rate at low ammonia concentrations but increased it at high concentrations. A pressure oxidized gold concentrate was leached for 6 hours in the batch reactor leaching experiments. The effect of rotative velocity (1.26-1.56 m/s) and slurry density (10-30 wt%) was investigated at the following leaching parameters: 0.2 M Na2S2O3, 0.6 M NH3, 0.01 M CuSO4, 0.4 M Na2SO4. Lower slurry density (10 wt%) resulted in a higher Au leaching efficiency. An increase in the rotation rate did not have an effect on the final Au leaching recovery. The best Au leaching efficiency (89%) was achieved with 590 rpm mixing, 1.56 m/s rotative velocity and 10 wt% slurry density.
引用
收藏
页码:1079 / 1091
页数:13
相关论文
共 48 条
[21]  
INTEC LTD, 2009, INT GOLD PROC
[22]   Identification of surface species that inhibit and passivate thiosulfate leaching of gold [J].
Jeffrey, M. I. ;
Watling, K. ;
Hope, G. A. ;
Woods, R. .
MINERALS ENGINEERING, 2008, 21 (06) :443-452
[23]   Kinetic aspects of gold and silver leaching in ammonia-thiosulfate solutions [J].
Jeffrey, MI .
HYDROMETALLURGY, 2001, 60 (01) :7-16
[24]  
LALANCETTE J-M., 2015, Method and a system for gold extraction with halogens, Patent No. [US 9051626 B2, 9051626]
[25]   COPPER-CATALYZED THIOSULFATE LEACHING OF LOW-GRADE GOLD ORES [J].
LANGHANS, JW ;
LEI, KPV ;
CARNAHAN, TG .
HYDROMETALLURGY, 1992, 29 (1-3) :191-203
[26]   The long term fate and environmental significance of contaminant metals released by the January and March 2000 mining tailings dam failures in Maramures County, upper Tisa Basin, Romania [J].
Macklin, MG ;
Brewer, PA ;
Balteanu, D ;
Coulthard, TJ ;
Driga, B ;
Howard, AJ ;
Zaharia, S .
APPLIED GEOCHEMISTRY, 2003, 18 (02) :241-257
[27]  
Marsden J., 2006, The chemistry of gold extraction, P651
[28]  
MKS DATA ANALYTICS SOLUTIONS, MODD 8 0 9 1
[29]  
Moyes J, 2010, United States Patent, Patent No. [US 7858056 B2, 7858056]
[30]   Thiosulphate as an alternative to cyanide for gold processing - issues and impediments [J].
Muir, DM ;
Aylmore, MG .
TRANSACTIONS OF THE INSTITUTIONS OF MINING AND METALLURGY SECTION C-MINERAL PROCESSING AND EXTRACTIVE METALLURGY, 2004, 113 (01) :2-12