Bonding effectiveness to different chemically pre-treated dental zirconia

被引:58
作者
Inokoshi, Masanao [1 ,2 ]
Poitevin, Andre [1 ,2 ]
De Munck, Jan [1 ,2 ]
Minakuchi, Shunsuke [3 ]
Van Meerbeek, Bart [1 ,2 ]
机构
[1] Univ Leuven, KU Leuven, Dept Oral Hlth Sci, KU Leuven BIOMAT, B-3000 Leuven, Belgium
[2] Univ Hosp Leuven, B-3000 Leuven, Belgium
[3] Tokyo Med & Dent Univ, Grad Sch Med & Dent Sci, Bunkyo Ku, Tokyo 1138549, Japan
关键词
Zirconia; Bond strength; Tribochemical silica sandblasting; Silane; Composite cement; Ageing; RESIN CEMENT; LUTING CEMENTS; SURFACE TREATMENTS; ADHESIVE RESIN; AIR ABRASION; STRENGTH; CERAMICS; OXIDE; MONOMER; DURABILITY;
D O I
10.1007/s00784-013-1152-7
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
The objective of this study was to evaluate the effect of different chemical pre-treatments on the bond durability to dental zirconia. Fully sintered IPS e.max ZirCAD (Ivoclar Vivadent) blocks were subjected to tribochemical silica sandblasting (CoJet, 3M ESPE). The zirconia samples were additionally pre-treated using one of four zirconia primers/adhesives (Clearfil Ceramic Primer, Kuraray Noritake; Monobond Plus, Ivoclar Vivadent; Scotchbond Universal, 3M ESPE; Z-PRIME Plus, Bisco). Finally, two identically pre-treated zirconia blocks were bonded together using composite cement (RelyX Ultimate, 3M ESPE). The specimens were trimmed at the interface to a cylindrical hourglass and stored in distilled water (7 days, 37 A degrees C), after which they were randomly tested as is or subjected to mechanical ageing involving cyclic tensile stress (10 N, 10 Hz, 10,000 cycles). Subsequently, the micro-tensile bond strength was determined, and SEM fractographic analysis performed. Weibull analysis revealed the highest Weibull scale and shape parameters for the 'Clearfil Ceramic Primer/mechanical ageing' combination. Chemical pre-treatment of CoJet (3M ESPE) sandblasted zirconia using Clearfil Ceramic Primer (Kuraray Noritake) and Monobond Plus (Ivoclar Vivadent) revealed a significantly higher bond strength than when Scotchbond Universal (3M ESPE) and Z-PRIME Plus (Bisco) were used. After ageing, Clearfil Ceramic Primer (Kuraray Noritake) revealed the most stable bond durability. Combined mechanical/chemical pre-treatment, the latter with either Clearfil Ceramic Primer (Kuraray Noritake) or Monobond Plus (Ivoclar Vivadent), resulted in the most durable bond to zirconia. As a standard procedure to durably bond zirconia to tooth tissue, the application of a combined 10-methacryloyloxydecyl dihydrogen phosphate/silane ceramic primer to zirconia is clinically highly recommended.
引用
收藏
页码:1803 / 1812
页数:10
相关论文
共 41 条
[31]   A practical and systematic review of Weibull statistics for reporting strengths of dental materials [J].
Quinn, Janet B. ;
Quinn, George D. .
DENTAL MATERIALS, 2010, 26 (02) :135-147
[32]  
Symynck J, 2011, NEW TECHNOLOGIES PRO, V18, P43
[33]   Cooperation of phosphate monomer and silica modification on zirconia [J].
Tanaka, R. ;
Fujishima, A. ;
Shibata, Y. ;
Manabe, A. ;
Miyazaki, T. .
JOURNAL OF DENTAL RESEARCH, 2008, 87 (07) :666-670
[34]   Adhesion/cementation to zirconia and other non-silicate ceramics: Where are we now? [J].
Thompson, Jeffrey Y. ;
Stoner, Brian R. ;
Piascik, Jeffrey R. ;
Smith, Robert .
DENTAL MATERIALS, 2011, 27 (01) :71-82
[35]  
WEIBULL W, 1951, J APPL MECH-T ASME, V18, P293
[36]   Effect of air abrasion and dye on the surface element ratio and resin bond of zirconia ceramic [J].
Xie, Z. G. ;
Meng, X. F. ;
Xu, L. N. ;
Yoshida, K. ;
Luo, X. P. ;
Gu, N. .
BIOMEDICAL MATERIALS, 2011, 6 (06)
[37]   Influence of air-abrasion on zirconia ceramic bonding using an adhesive composite resin [J].
Yang, B. ;
Barloi, A. ;
Kern, M. .
DENTAL MATERIALS, 2010, 26 (01) :44-50
[38]   Bonding of dual-cured resin cement to zirconia ceramic using phosphate acid ester monomer and zirconate coupler [J].
Yoshida, K ;
Tsuo, Y ;
Atsuta, M .
JOURNAL OF BIOMEDICAL MATERIALS RESEARCH PART B-APPLIED BIOMATERIALS, 2006, 77B (01) :28-33
[39]  
Yoshida Keiichi, 2007, J Prosthodont, V16, P370, DOI 10.1111/j.1532-849X.2007.00221.x
[40]  
Yoshida T, 2012, DENT MAT S1, V28, pe38, DOI [10.1016/j.dental.2012.07.092, DOI 10.1016/J.DENTAL.2012.07.092]