Bonding effectiveness to different chemically pre-treated dental zirconia

被引:56
|
作者
Inokoshi, Masanao [1 ,2 ]
Poitevin, Andre [1 ,2 ]
De Munck, Jan [1 ,2 ]
Minakuchi, Shunsuke [3 ]
Van Meerbeek, Bart [1 ,2 ]
机构
[1] Univ Leuven, KU Leuven, Dept Oral Hlth Sci, KU Leuven BIOMAT, B-3000 Leuven, Belgium
[2] Univ Hosp Leuven, B-3000 Leuven, Belgium
[3] Tokyo Med & Dent Univ, Grad Sch Med & Dent Sci, Bunkyo Ku, Tokyo 1138549, Japan
关键词
Zirconia; Bond strength; Tribochemical silica sandblasting; Silane; Composite cement; Ageing; RESIN CEMENT; LUTING CEMENTS; SURFACE TREATMENTS; ADHESIVE RESIN; AIR ABRASION; STRENGTH; CERAMICS; OXIDE; MONOMER; DURABILITY;
D O I
10.1007/s00784-013-1152-7
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
The objective of this study was to evaluate the effect of different chemical pre-treatments on the bond durability to dental zirconia. Fully sintered IPS e.max ZirCAD (Ivoclar Vivadent) blocks were subjected to tribochemical silica sandblasting (CoJet, 3M ESPE). The zirconia samples were additionally pre-treated using one of four zirconia primers/adhesives (Clearfil Ceramic Primer, Kuraray Noritake; Monobond Plus, Ivoclar Vivadent; Scotchbond Universal, 3M ESPE; Z-PRIME Plus, Bisco). Finally, two identically pre-treated zirconia blocks were bonded together using composite cement (RelyX Ultimate, 3M ESPE). The specimens were trimmed at the interface to a cylindrical hourglass and stored in distilled water (7 days, 37 A degrees C), after which they were randomly tested as is or subjected to mechanical ageing involving cyclic tensile stress (10 N, 10 Hz, 10,000 cycles). Subsequently, the micro-tensile bond strength was determined, and SEM fractographic analysis performed. Weibull analysis revealed the highest Weibull scale and shape parameters for the 'Clearfil Ceramic Primer/mechanical ageing' combination. Chemical pre-treatment of CoJet (3M ESPE) sandblasted zirconia using Clearfil Ceramic Primer (Kuraray Noritake) and Monobond Plus (Ivoclar Vivadent) revealed a significantly higher bond strength than when Scotchbond Universal (3M ESPE) and Z-PRIME Plus (Bisco) were used. After ageing, Clearfil Ceramic Primer (Kuraray Noritake) revealed the most stable bond durability. Combined mechanical/chemical pre-treatment, the latter with either Clearfil Ceramic Primer (Kuraray Noritake) or Monobond Plus (Ivoclar Vivadent), resulted in the most durable bond to zirconia. As a standard procedure to durably bond zirconia to tooth tissue, the application of a combined 10-methacryloyloxydecyl dihydrogen phosphate/silane ceramic primer to zirconia is clinically highly recommended.
引用
收藏
页码:1803 / 1812
页数:10
相关论文
共 50 条
  • [1] Bonding effectiveness to different chemically pre-treated dental zirconia
    Masanao Inokoshi
    André Poitevin
    Jan De Munck
    Shunsuke Minakuchi
    Bart Van Meerbeek
    Clinical Oral Investigations, 2014, 18 : 1803 - 1812
  • [2] Durable bonding to mechanically and/or chemically pre-treated dental zirconia
    Inokoshi, Masanao
    Kameyama, Atsushi
    De Munck, Jan
    Minakuchi, Shunsuke
    Van Meerbeek, Bart
    JOURNAL OF DENTISTRY, 2013, 41 (02) : 170 - 179
  • [3] Bonding Effectiveness to Differently Sandblasted Dental Zirconia
    Bielen, Vincent
    Inokoshi, Masanao
    De Munck, Jan
    Zhang, Fei
    Vanmeensel, Kim
    Minakuchi, Shunsuke
    Vleugels, Jozef
    Naert, Ignace
    Van Meerbeek, Bart
    JOURNAL OF ADHESIVE DENTISTRY, 2015, 17 (03) : 235 - 242
  • [4] Simple Heat Treatment of Zirconia Ceramic Pre-Treated with Silane Primer to Improve Resin Bonding
    Ha, Jung-Yun
    Son, Jun Sik
    Kim, Kyo-Han
    Kwon, Tae-Yub
    JOURNAL OF NANOSCIENCE AND NANOTECHNOLOGY, 2015, 15 (01) : 587 - 590
  • [5] Effect of heat treatment of dental zirconia ceramic treated with three different primers on the bonding durability of resin cement
    Ha, Jung-Yun
    Son, Jun Sik
    Kim, Young Kyung
    Kim, Kyo-Han
    Kwon, Tae-Yub
    MACROMOLECULAR RESEARCH, 2013, 21 (01) : 71 - 77
  • [6] Bonding Efficacy of 4-META/MMA-TBB Resin to Surface-treated Highly Translucent Dental Zirconia
    Shimizu, Haruki
    Inokoshi, Masanao
    Takagaki, Tomohiro
    Uo, Motohiro
    Minakuchi, Shunsuke
    JOURNAL OF ADHESIVE DENTISTRY, 2018, 20 (05) : 453 - 459
  • [7] Mechanical Properties and Bonding Potential of Partially Stabilized Zirconia Treated with Different Chemomechanical Treatments
    EI-Korashy, Dalia I.
    Ei-Refai, Dina A.
    JOURNAL OF ADHESIVE DENTISTRY, 2014, 16 (04) : 365 - 376
  • [8] Laser controlled melting of pre-treated zirconia surface
    Yilbas, B. S.
    Akhtar, S. S.
    Karatas, C.
    APPLIED SURFACE SCIENCE, 2011, 257 (15) : 6912 - 6918
  • [9] Resistance to bond degradation between dual-cure resin cements and pre-treated sintered CAD-CAM dental ceramics
    Osorio, Raquel
    Castillo-de Oyaguee, Raquel
    Monticelli, Francesca
    Osorio, Estrella
    Toledano, Manuel
    MEDICINA ORAL PATOLOGIA ORAL Y CIRUGIA BUCAL, 2012, 17 (04): : E669 - E677
  • [10] Association of Different Primers and Resin Cements for Adhesive Bonding to Zirconia Ceramics
    Maeda, Fernando Akio
    Bello-Silva, Marina Stella
    Eduardo, Carlos de Paula
    Miranda Junior, Walter Gomes
    Cesar, Paulo Francisco
    JOURNAL OF ADHESIVE DENTISTRY, 2014, 16 (03) : 261 - 265