Characteristics of Fine Oxide Particles Produced by Ti/M (M=Mg and Zr) Complex Deoxidation in Fe-10mass%Ni Alloy
被引:33
|作者:
Karasev, Andrey V.
[1
]
Suito, Hideaki
[1
]
机构:
[1] Tohoku Univ, Inst Multiclisplinary Res Adv Mat, Aoba Ku, Sendai, Miyagiken 9808577, Japan
关键词:
inclusion;
cluster;
particle size distribution;
Ti;
Zr and Mg deoxidation;
primary and secondary deoxidation;
D O I:
10.2355/isijinternational.48.1507
中图分类号:
TF [冶金工业];
学科分类号:
0806 ;
摘要:
Characteristics of oxide particles produced by Ti/M (M=Mg and Zr) complex deoxidation have been studied in an Fe-10mass%Ni alloy as a function of holding time at 1 600 degrees C, followed by quenching. The size distributions for the particles having different compositions are compared with the particle size distribution in single deoxidation with Ti, Mg or Zr. In most experiments the composition of particles precipitated during rapid quenching was found to be non-equilibrium phase. The formation mechanism of primary and secondary deoxidation particles and the difference in the compositions of non-clustered and clustered particles are discussed. The effects of Ti addition, method of deoxidation and holding time at 1 600 degrees C on particle size distributions in Ti/M complex deoxidation experiments are studied.