Solubility and diffusivity of protium in internally nitrided iron alloys
被引:0
作者:
Miyamura, H
[1
]
Hirai, K
[1
]
Hirose, K
[1
]
Kikuchi, S
[1
]
机构:
[1] Univ Shiga Prefecture, Hikone, Shiga 5228533, Japan
来源:
PRICM 4: FORTH PACIFIC RIM INTERNATIONAL CONFERENCE ON ADVANCED MATERIALS AND PROCESSING, VOLS I AND II
|
2001年
关键词:
protium;
hydrogen;
diffusion;
nitride;
precipitate;
lattice distortion;
D O I:
暂无
中图分类号:
T [工业技术];
学科分类号:
08 ;
摘要:
Some Fe-Ti and Fe-V alloys were internally nitrided by a plasma-treatment and their solubilities and diffusivities of protium were measured by an electrochemical method, using a 6M KOH electrolyte, NiOOH/Ni(OH)(2) counter electrode and Hg/HgO reference electrode. The protium solubility in the alloys increased by internal nitriding. Diffusivities of protium, in the internally nitrided alloys at ambient temperatures were in the order of 10(-9) cm(2)/s, which was much smaller than those in pure iron. Its activation energy was 30-40 kJ/mol. These values suggest that protium, in the internally nitrided iron alloys was supposed to be trapped and stabilized at the sites around the nitride precipitates, which had lower site-energies than that in pure iron.