Evolution of wear damage in gross sliding fretting of a nitrided high-carbon high-chromium steel

被引:14
|
作者
Duan, Yong [1 ,2 ]
Qu, Shengguan [1 ,2 ]
Jia, Siyu [1 ,2 ]
Li, Xiaoqiang [1 ,2 ]
机构
[1] South China Univ Technol, Natl Engn Res Ctr Near Net Shape Forming Met Mat, Guangzhou 510640, Peoples R China
[2] South China Univ Technol, Sch Mech & Automot Engn, Guangzhou 510640, Guangdong, Peoples R China
关键词
Fretting wear; Gross sliding; Evolution; Nitrides; ABRASIVE WEAR; BEHAVIOR; TI-6AL-4V; HARDNESS; DEBRIS; MICROSTRUCTURE; OXIDATION; ALLOY; LAYER; DRY;
D O I
10.1016/j.wear.2020.203548
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
Fretting wear tests were performed to examine the evolution of fretting wear damage of the nitrided high-carbon high-chromium X210CrW12 steel against GCr15 steel ball, and to identify the role of nitrides (converted carbides) in fretting wear characteristics. The nitrided layer was characterized by optical microscope (OM), scanning electron microscope (SEM), energy-dispersive spectroscopy (EDS), electron probe microanalyses (EPMA), X-ray diffraction (XRD), and microhardness analysis. The worn surfaces were evaluated by SEM, EDS and 3D optical profiler. The results indicated that the initial carbides in the nitrided layer undergone a transformation into nitrides during nitriding. The nitrided specimens showed excellent wear resistance compared to the steel balls, and their wear damage was mainly caused by the adhesive/abrasive action of oxidized particles. Coarse nitrides led to the rapid wear of steel balls, and acted as barriers against the grooving of oxidized particles. Higher loading conditions of 40 N and 80 N induced the generation of central smooth zone and W-shaped wear scar. The formation of the central smooth zone was very beneficial for reducing the wear rate and friction co-efficient, thus the expected increase in wear volume with increasing applied load from 40 N to 80 N was not observed.
引用
收藏
页数:13
相关论文
共 50 条
  • [1] Evolution of the Fretting Wear Damage of a Complex Phase Compound Layer for a Nitrided High-Carbon High-Chromium Steel
    Duan, Yong
    Qu, Shengguan
    Jia, Siyu
    Li, Xiaoqiang
    METALS, 2020, 10 (10) : 1 - 12
  • [2] Fretting wear behavior of the high-carbon high-chromium X210CrW12 steel: Influence of counterbody material
    Duan, Yong
    Qu, Shengguan
    Jia, Siyu
    Li, Xiaoqiang
    WEAR, 2021, 486
  • [3] Effects of ultrasonic surface rolling processing on microstructure and wear properties of high-carbon high-chromium steel
    Duan, Yong
    Qu, Shengguan
    Jia, Siyu
    Li, Xiaoqiang
    SURFACE & COATINGS TECHNOLOGY, 2021, 422
  • [4] Effect of Titanium Addition on As Cast Structure and Macrosegregation of High-Carbon High-Chromium Steel
    Razavinejad, Reza
    Firoozi, Sadegh
    Mirbagheri, Seyed Mohammad Hossein
    STEEL RESEARCH INTERNATIONAL, 2012, 83 (09) : 861 - 869
  • [5] Carbide Fragmentation and Dissolution in a High-Carbon High-Chromium Steel Using Hot Rolling Process: Microstructure Evolution, Wear, High-Temperature Oxidation, and Chloride-Induced Corrosion Properties
    Shahsanaei, Majid
    Pour-Ali, Sadegh
    Kiani-Rashid, Ali-Reza
    Virtanen, Sannakaisa
    CORROSION, 2018, 74 (09) : 958 - 970
  • [6] Effect of copper addition on the characteristics of high-carbon and high-chromium steels
    Kang, Jun-Yun
    Heo, Yoon-Uk
    Kim, Hoyoung
    Suh, Dong-Woo
    Son, Dongmin
    Lee, Dong Hee
    Lee, Tae-Ho
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2014, 614 : 36 - 44
  • [7] Rotational fretting wear of ion nitrided medium carbon steel
    Luo, J.
    Wang, Y. D.
    Song, C.
    Mo, J. L.
    Zhu, M. H.
    MANUFACTURING SCIENCE AND ENGINEERING, PTS 1-5, 2010, 97-101 : 1532 - 1541
  • [8] Wear damage of Alloy 690TT in partial and gross slip fretting regimes at high temperature
    Xin, L.
    Yang, B. B.
    Li, J.
    Lu, Y. H.
    Shoji, T.
    WEAR, 2017, 390-391 : 71 - 79
  • [9] Effect of molybdenum and chromium contents on sliding wear of high-chromium white cast iron at high temperature
    Pinho, Karin Faria
    Boher, Christine
    Scandian, Cherlio
    LUBRICATION SCIENCE, 2013, 25 (02) : 153 - 162
  • [10] Characterization of high-carbon high-chromium tool steel/low-carbon steel friction-welded joints for industrial tooling applications
    Rajendran, T. Packiaraj
    Hynes, N. Rajesh Jesudoss
    Christopher, T.
    JOURNAL OF THE BRAZILIAN SOCIETY OF MECHANICAL SCIENCES AND ENGINEERING, 2018, 40 (06)