Effect of grinding with diamond-disc and -bur on the mechanical behavior of a Y-TZP ceramic

被引:52
作者
Pereira, G. K. R. [1 ]
Amaral, M. [2 ]
Simoneti, R. [1 ]
Rocha, G. C. [1 ]
Cesar, P. F. [3 ]
Valandro, L. F. [1 ]
机构
[1] Univ Fed Santa Maria, Fac Odontol, BR-97015372 Santa Maria, RS, Brazil
[2] Sao Paulo State Univ UNESP, Fac Odontol, Inst Sci & Technol, Sao Jose Dos Campos, Brazil
[3] Univ Sao Paulo, Fac Odontol, Sao Paulo, Brazil
关键词
Grinding; Zirconium oxide partially stabilized by yttrium; Mechanical properties; LOW-TEMPERATURE DEGRADATION; FLEXURAL STRENGTH; MARTENSITIC-TRANSFORMATION; ZIRCONIA; SURFACE; RELIABILITY; STABILITY; STRESSES; FAILURE; TESTS;
D O I
10.1016/j.jmbbm.2014.05.010
中图分类号
R318 [生物医学工程];
学科分类号
0831 ;
摘要
This study compared the effects of grinding on the surface micromorphology, phase transformation (t -> m), biaxial flexural strength and structural reliability (Weibull analysis) of a Y-TZP (Lava) ceramic using diamond-discs and -burs. 170 discs (15 x 1.2 mm) were produced and divided into 5 groups: without treatment (Ctrl, as-sintered), and ground with 4 different systems: extra-fine (25 mu m, Xfine) and coarse diamond-bur (181 mu m, Coarse), 600-grit (25 mu m, D600) and 120-grit diamond-disc (160 mu m, D120). Grinding with burs was performed using a contra-angle handpiece (T2-Revo R170, Sirona), while for discs (Allied) a Polishing Machine (Ecomet, Buehler) was employed, both under water-cooling. Micromorphological analysis showed distinct patterns generated by grinding with discs and burs, independent of grit size. There was no statistical difference for characteristic strength values (MPa) between smaller grit sizes (D600 - 1050.08 and Xfine - 1171.33), although they presented higher values compared to Ctrl (917.58). For bigger grit sizes, a significant difference was observed (Coarse - 1136.32>D120-727.47). Weibull Modules were statistically similar between the tested groups. Within the limits of this study, from a micromorphological point-of-view, the treatments performed did not generate similar effects, so from a methodological point-of-view, diamond-discs should not be employed to simulate clinical abrasion performed with diamond-burs on Y-TZP ceramics. (C) 2014 Elsevier Ltd. All rights reserved.
引用
收藏
页码:133 / 140
页数:8
相关论文
共 45 条
[1]   Bridging the gap between clinical failure and laboratory fracture strength tests using a fractographic approach [J].
Aboushelib, Moustafa N. ;
Feilzer, Albert J. ;
Kleverlaan, Cees J. .
DENTAL MATERIALS, 2009, 25 (03) :383-391
[2]   Resin-ceramic bonding: a review of the literature [J].
Blatz, MB ;
Sadan, A ;
Kern, M .
JOURNAL OF PROSTHETIC DENTISTRY, 2003, 89 (03) :268-274
[3]   Flexural strength and failure modes of layered ceramic structures [J].
Borba, Marcia ;
de Araujo, Maico D. ;
de Lima, Erick ;
Yoshimura, Humberto N. ;
Cesar, Paulo F. ;
Griggs, Jason A. ;
Della Bona, Alvaro .
DENTAL MATERIALS, 2011, 27 (12) :1259-1266
[4]   Low-temperature degradation of Zirconia and implications for biomedical implants [J].
Chevalier, Jerome ;
Gremillard, Laurent ;
Deville, Sylvain .
ANNUAL REVIEW OF MATERIALS RESEARCH, 2007, 37 (1-32) :1-32
[5]  
Crespo AA., 1997, ESTATISTICA FACIL
[6]   Fracture toughness versus micro-tensile bond strength testing of adhesive-dentin interfaces [J].
De Munck, Jan ;
Luehrs, Anne-Katrin ;
Poitevin, Andre ;
Van Ende, Annelies ;
Van Meerbeek, Bart .
DENTAL MATERIALS, 2013, 29 (06) :635-644
[7]   Weibull analysis and flexural strength of hot-pressed core veneered ceramic structures [J].
Della Bona, A ;
Anusavice, KJ ;
DeHoff, PH .
DENTAL MATERIALS, 2003, 19 (07) :662-669
[8]  
Della Bona Alvaro, 2005, J. Appl. Oral Sci., V13, P1, DOI 10.1590/S1678-77572005000100002
[9]   State of the art of zirconia for dental applications [J].
Denry, Isabelle ;
Kelly, J. Robert .
DENTAL MATERIALS, 2008, 24 (03) :299-307
[10]   Influence of surface finish and residual stresses on the ageing sensitivity of biomedical grade zirconia [J].
Deville, S ;
Chevalier, J ;
Gremillard, L .
BIOMATERIALS, 2006, 27 (10) :2186-2192