Investigation on the microstructure and properties of W-10 wt% Cu prepared by sintering and infiltration

被引:21
作者
Ahangarkani, M. [1 ]
Zangeneh-madar, K. [1 ]
机构
[1] Malek Ashlar Univ Technol, Dept Mat, Tehran 158751774, Iran
关键词
W-Cu composite; Activated sintering; Ni and Co additive; Infiltration; Electrical resistivity; Tensile strength; TUNGSTEN PARTICLE-SIZE; IMPROVEMENT;
D O I
10.1016/j.ijrmhm.2018.03.015
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In the present study, Three tungsten powder mixtures with average particle size of 6 mu m containing 0.05, 0.25 and 0.05 wt% of activators (Ni and Co) were used to fabricate W-10 wt% Cu composites by sintering and infiltration method. The mechanically mixed powder mixtures were compressed under CIP to prepare green compacts of cylindrical shape. Then, green compacts were sintered at 1350-1600 degrees C for 4 h and then infiltrated/ penetrated by liquid copper under the hydrogen atmosphere in order to obtain W-10 wt% Cu composites. The sintered samples as well as its infiltrated compacts were characterized by scanning electron microscopy (SEM), EDS and XRD methods. Investigation the physical and mechanical properties carried out by density and electrical resistivity measurement and also tensile test. The obtained results exhibited that Ni doped samples achieved to density of 15.05-15.70 g/cm(3) at lower sintering temperature rather than Co containing specimens. Also, it was found that activating capability of additives depend on its concentration as well as sintering temperature. The microstructural observations revealed mutual dependency of mechanical properties of composite and W-W contiguity. Maximum tensile strength for Ni and Co containing composite was measured about 650 and 619 MPa, respectively.
引用
收藏
页码:1 / 9
页数:9
相关论文
共 24 条
[11]   ENHANCED LOW-TEMPERATURE SINTERING OF TUNGSTEN [J].
GERMAN, RM ;
MUNIR, ZA .
METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1976, 7 (12) :1873-1877
[12]  
Gupta K. P., 2000, J PHS EQIL, V2, P396
[13]   Tungsten-copper composite production by activated sintering and infiltration [J].
Hamidi, A. Ghaderi ;
Arabi, H. ;
Rastegari, S. .
INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2011, 29 (04) :538-541
[14]   Activated sintering of nickel-doped tungsten: Approach by grain boundary structural transition [J].
Hwang, NM ;
Park, YJ ;
Kim, DY ;
Yoon, DY .
SCRIPTA MATERIALIA, 2000, 42 (05) :421-425
[15]   An experimental investigation on the W-Cu composites [J].
Ibrahim, A. ;
Abdallah, M. ;
Mostalfa, S. F. ;
Hegazy, A. Abousree .
MATERIALS & DESIGN, 2009, 30 (04) :1398-1403
[16]   PHASE-EQUILIBRIA EFFECTS ON THE ENHANCED LIQUID-PHASE SINTERING OF TUNGSTEN-COPPER [J].
JOHNSON, JL ;
GERMAN, RM .
METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1993, 24 (11) :2369-2377
[17]   Effects of tungsten particle size and copper content on densification of liquid-phase-sintered W-Cu [J].
Johnson, JL ;
Brezovsky, JJ ;
German, RM .
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2005, 36A (10) :2807-2814
[18]   Role of solid-state skeletal sintering during processing of Mo-Cu composites [J].
Johnson, JL ;
German, RM .
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2001, 32 (03) :605-613
[19]   EFFECT OF COBALT ADDITION ON THE LIQUID-PHASE SINTERING OF W-CU PREPARED BY THE FLUIDIZED-BED REDUCTION METHOD [J].
JOO, SK ;
LEE, SW ;
IHN, TH .
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1994, 25 (08) :1575-1578
[20]   THE PROPERTIES OF TUNGSTEN PROCESSED BY CHEMICALLY ACTIVATED SINTERING [J].
LI, CJ ;
GERMAN, RM .
METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1983, 14 (10) :2031-2041