The influence of Zn on the deposition of HA on sol-gel derived bioactive glass

被引:0
|
作者
Du, Rui Lin
Chang, Jiang
机构
[1] Chinese Acad Sci, Shanghai Inst Ceram, Biomat & Tissue Engn Ctr, Shanghai 200050, Peoples R China
[2] Chinese Acad Sci, Grad Sch, Shanghai 200050, Peoples R China
关键词
zinc; hydroxyapatite; bioactive glass;
D O I
暂无
中图分类号
R318 [生物医学工程];
学科分类号
0831 ;
摘要
To evaluate the influence of Zn on the formation of hydroxyapatite (HA), zinc-containing glass 58S4Z was prepared by substitution of CaO with 4 wt% ZnO in 58S bioactive glass, and Zn-containing simulated body fluid (ZnSBF) was prepared as soaking fluid. During the soaking, all samples could induce the deposition of HA, but 58S4Z in SBF and 58S in ZnSBF showed lower formation rate of HA than 58S in SBF, which suggests that both the Zn in glass and the Zn2+ in soaking fluid retarded the deposition of HA. The ICP and EDS analysis results indicated that the main factor was the preferential reaction of Zn2+ with PO43-, which resulted in a decrease of the PO43- concentration in soaking fluid and the nucleation of HA. Besides the inhibitory effect of Zn2+ in the soaking fluid, Zn in 58S4Z glass caused a lower release rate of Ca2+ in the initial soaking periods because of the lower CaO content as compared with 58S, and resulted in a lower nucleation rate of HA. The results suggested that small amount of Zn in bioactive glass retarded the nucleation of HA, but with the exhaustion of Zn2+ by PO43-, it did not affect the long-term deposition of HA in SBF.
引用
收藏
页码:229 / 236
页数:8
相关论文
共 50 条
  • [1] Bioactive behaviour of sol-gel derived antibacterial bioactive glass
    Bellantone, M
    Hench, LL
    BIOCERAMICS, 2000, 192-1 : 617 - 620
  • [2] Bioactive and biocompatible pieces of HA/sol-gel glass mixtures obtained by the gel-casting method
    Padilla, S
    Sánchez-Salcedo, S
    Vallet-Regí, M
    JOURNAL OF BIOMEDICAL MATERIALS RESEARCH PART A, 2005, 75A (01) : 63 - 72
  • [3] A novel sol-gel derived bioactive glass featuring antibacterial properties
    Bellantone, M
    Coleman, NJ
    Hench, LL
    BIOCERAMICS, 2000, 192-1 : 597 - 600
  • [4] Mophology character of the sol-gel derived bioactive glass in SBF solution
    Zhang, XK
    Liu, W
    Chen, XF
    CHINESE JOURNAL OF CHEMICAL PHYSICS, 2004, 17 (04) : 495 - 498
  • [5] Bioactive glass prepared by sol-gel emulsion
    Delben, J. R. J.
    Pereira, K.
    Oliveira, S. L.
    Alencar, L. D. S.
    Hernandes, A. C.
    Delben, A. A. S. T.
    JOURNAL OF NON-CRYSTALLINE SOLIDS, 2013, 361 : 119 - 123
  • [6] Coupling sol-gel with electrospray deposition: Towards nanotextured bioactive glass coatings
    Mueller, V
    Jobbagy, M.
    Djurado, E.
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2021, 41 (14) : 7288 - 7300
  • [7] Characterization of the bioactive and mechanical behavior of dental ceramic/sol-gel derived bioactive glass mixtures
    Abbasi, Zahra
    Bahrololoum, Mohammad E.
    Bagheri, Rafat
    Shariat, Mohammad H.
    JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2016, 54 : 115 - 122
  • [8] Primary osteoblast cell response to sol-gel derived bioactive glass foams
    P. Valerio
    M. H. R. Guimaráes
    M. M. Pereira
    M. F. Leite
    A. M. Goes
    Journal of Materials Science: Materials in Medicine, 2005, 16 : 851 - 856
  • [9] Cuttlefish Bone-Derived Biphasic Calcium Phosphate Scaffolds Coated with Sol-Gel Derived Bioactive Glass
    Neto, Ana S.
    Brazete, Daniela
    Ferreira, Jose M. F.
    MATERIALS, 2019, 12 (17)
  • [10] Influence of network modifiers in an acetate based sol-gel bioactive glass system
    Fernando, Delihta
    Attik, Nina
    Cresswell, Mark
    Mokbel, Ilham
    Pradelle-Plasse, Nelly
    Jackson, Phil
    Grosgogeat, Brigitte
    Colon, Pierre
    MICROPOROUS AND MESOPOROUS MATERIALS, 2018, 257 : 99 - 109