Erosion-corrosion resistance of engineering materials in various test conditions

被引:131
|
作者
Rajahram, S. S. [1 ]
Harvey, T. J. [1 ]
Wood, R. J. K. [1 ]
机构
[1] Univ Southampton, Sch Engn Sci, Natl Ctr Adv Tribol Southampton, Southampton SO17 1BJ, Hants, England
基金
英国工程与自然科学研究理事会;
关键词
Slurry pot erosion tester; Erosion-corrosion; Error analysis; Synergy; NICKEL-ALUMINUM BRONZE; SLURRY EROSION; STAINLESS-STEEL; MASS-LOSS; VELOCITY; WEAR; PARTICLES; ENERGIES; COATINGS; BEHAVIOR;
D O I
10.1016/j.wear.2009.01.052
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
Erosion-corrosion is a complex phenomenon which involves the interaction between the mechanical processes of solid particle erosion and the electrochemical processes of corrosion. A whole range of issues is faced by a designer when trying to obtain relevant information on erosion-corrosion performance of a material. Amongst the constraints are the dispersed test conditions and test rigs available in the literature making comparisons and quantifying erosion-corrosion wear rates of different materials very difficult. The aim of this work is to evaluate the repeatability of erosion-corrosion experiments and to investigate the role of different parameters influencing erosion-corrosion. The materials tested in this work are stainless steel (SS316L/UNS S31603), carbon steel (AISI 1020/UNS G10200) and nickel-aluminium bronze (NAB/UNS C63200). A slurry pot erosion tester was used as the test apparatus and test parameters such as erodent size, erodent concentration, flow velocity and test solutions were varied to study their effect on erosion-corrosion. SEM analysis showed that a similar erosion-corrosion mechanism is seen for SS316L and NAB with formation of multiple extruded lips and platelets typically seen for erosion dominated material. In contrast the surface of AISI 1020 revealed the formation of craters, pits and shallow indentations which suggests that corrosion mechanism has a dominant influence on the material. Error rates in tests were found to have an average of 5.5% which are relatively low indicating good repeatability of test measurements and data from the test rig. The erosion-corrosion resistance of AISI 1020, SS316L and NAB were compared and it was found that SS316L showed the lowest erosion-corrosion mass loss rates in all test conditions followed by NAB and then AISI 1020. However in terms of synergistic ranking, NAB showed the best resistance to the combined action of erosion and corrosion with the highest negative synergy value. Positive synergy was evident for AISI 1020 in 3.5% NaCl and SS316L in 0.3 M HCl. A wear map is presented to evaluate erosion-corrosion trends of the materials. This work combines the assessment of test repeatability, variation in test conditions and comparison of material performance which are key stages in a material selection process. (C) 2009 Elsevier B.V. All rights reserved.
引用
收藏
页码:244 / 254
页数:11
相关论文
共 50 条
  • [1] Erosion-Corrosion of Materials in Industrial Equipment: A Review
    Rao, Padmalatha
    Mulky, Lavanya
    CHEMELECTROCHEM, 2023, 10 (16)
  • [2] Erosion-corrosion mechanism and comparison of erosion-corrosion performance of API steels
    Islam, Md. Aminul
    Farhat, Zoheir
    WEAR, 2017, 376 : 533 - 541
  • [3] Erosion-corrosion assessment of materials for use in the resources industry
    Jones, M.
    Llewellyn, R. J.
    WEAR, 2009, 267 (11) : 2003 - 2009
  • [4] A brief review on the erosion-corrosion behavior of engineering materials
    Kuruvila, Roshan
    Kumaran, S. Thirumalai
    Khan, M. Adam
    Uthayakumar, M.
    CORROSION REVIEWS, 2018, 36 (05) : 435 - 447
  • [5] A study on the erosion-corrosion behaviour of engineering materials used in the geothermal industry
    Brownlie, F.
    Hodgkiess, T.
    Pearson, A.
    Galloway, A. M.
    WEAR, 2021, 477
  • [6] Erosion-corrosion interactions and their effect on marine and offshore materials
    Wood, Robert J. K.
    WEAR, 2006, 261 (09) : 1012 - 1023
  • [7] Cavitation erosion and erosion-corrosion resistance of austenitic stainless steel by plasma transferred arc welding
    Zhang, S.
    Wang, S.
    Wu, C. L.
    Zhang, H.
    Guan, M.
    Tan, J. Z.
    ENGINEERING FAILURE ANALYSIS, 2017, 76 : 115 - 124
  • [8] Full factorial investigation on the erosion-corrosion resistance of UNS S31603
    Rajahram, S. S.
    Harvey, T. J.
    Wood, R. J. K.
    TRIBOLOGY INTERNATIONAL, 2010, 43 (11) : 2072 - 2083
  • [9] Erosion-corrosion resistance of various stainless steel grades in high-temperature sulfuric acid solution
    Lindgren, M.
    Siljander, S.
    Suihkonen, R.
    Pohjanne, P.
    Vuorinen, J.
    WEAR, 2016, 364 : 10 - 21
  • [10] Investigation of erosion-corrosion mechanisms of UNS S31603 using FIB and TEM
    Rajahram, S. S.
    Harvey, T. J.
    Walker, J. C.
    Wang, S. C.
    Wood, R. J. K.
    TRIBOLOGY INTERNATIONAL, 2012, 46 (01) : 161 - 173