Synthesis and characterization of Ti3AlC2

被引:646
作者
Tzenov, NV [1 ]
Barsoum, MW [1 ]
机构
[1] Drexel Univ, Dept Mat Engn, Philadelphia, PA 19104 USA
关键词
D O I
10.1111/j.1151-2916.2000.tb01281.x
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Polycrystalline bulk samples of Ti3Al1.1C1.8 have been fabricated by reactively hot isostatically pressing a mixture of titanium, graphite, and Al4C3 powders at a pressure of 70 MPa and temperature of 1400 degrees C for 16 h, The hot isostatically pressed samples are predominantly single phase (containing similar to 4 vol% Al2O3), fully dense, and have a grain size of similar to 25 mu m. This carbide is similar to Ti3SiC2, with which it is isostructural, and has an unusual combination of properties. It is relatively soft (Vickers hardness of similar to 3.5 GPa) and elastically stiff (Young's modulus of 297 GPa and shear modulus of 124 GPa); yet, it is lightweight (density of 4.2 g/cm(3)) and easily machinable, The room-temperature electrical resistivity is 0.35 +/- 0.03 mu Omega.m and decreases linearly as the temperature decreases. The temperature coefficient of resistivity is 0.0031 K-1. The coefficient of thermal expansion, in the temperature range of 25 degrees-1200 degrees C, is 9.0 (+/- 0.2) x 10(-6) K-1. The roomtemperature compressive and flexural strengths are 560 +/- 20 and 375 +/- 15 MPa, respectively. In contrast to flexure, where the failure is brittle, the failure in compression is noncatastrophic and is accompanied by some plasticity. The origin of that plasticity is believed to be the formation of a ''shear" band that is oriented at an angle of similar to 45 degrees to the applied load. Ti3Al1.1C1.8 also is a highly damage-tolerant material; a 10-kg-load Vickers indentation made in a bar 1.5 mm thick reduces the post-indentation flexural strength by similar to 7%, This material also is quite resistant to thermal shock. At temperatures of >1000 degrees C, the deformation in compression is accompanied by significant plasticity and very respectable ultimate compressive stresses (200 MPa at 1200 degrees C).
引用
收藏
页码:825 / 832
页数:8
相关论文
共 26 条
[1]  
Barsoum MW, 1997, J MATER SYNTH PROCES, V5, P197
[2]   Fabrication and characterization of M2SnC (M = Ti, Zr, Hf and Nb) [J].
Barsoum, MW ;
Yaroschuk, G ;
Tyagi, S .
SCRIPTA MATERIALIA, 1997, 37 (10) :1583-1591
[3]   Layered machinable ceramics for high temperature applications [J].
Barsoum, MW ;
Brodkin, D ;
ElRaghy, T .
SCRIPTA MATERIALIA, 1997, 36 (05) :535-541
[4]   Room-temperature ductile carbides [J].
Barsoum, MW ;
El-Raghy, T .
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1999, 30 (02) :363-369
[5]   Oxidation of Ti3SiC2 in air [J].
Barsoum, MW ;
ElRaghy, T ;
Ogbuji, LUJT .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1997, 144 (07) :2508-2516
[6]   Thermal properties of Ti3SiC2 [J].
Barsoum, MW ;
El-Raghy, T ;
Rawn, CJ ;
Porter, WD ;
Wang, H ;
Payzant, EA ;
Hubbard, CR .
JOURNAL OF PHYSICS AND CHEMISTRY OF SOLIDS, 1999, 60 (04) :429-439
[7]   Synthesis and characterization of a remarkable ceramic: Ti3SiC2 [J].
Barsoum, MW ;
ElRaghy, T .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1996, 79 (07) :1953-1956
[8]  
BARSOUM MW, IN PRESS METALL MAT
[9]   MICROSTRUCTURE-STRENGTH PROPERTIES IN CERAMICS .1. EFFECT OF CRACK SIZE ON TOUGHNESS [J].
COOK, RF ;
LAWN, BR ;
FAIRBANKS, CJ .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1985, 68 (11) :604-615
[10]   Processing and mechanical properties of Ti3SiC2:: I, reaction path and microstructure evolution [J].
El-Raghy, T ;
Barsoum, MW .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1999, 82 (10) :2849-2854