Effect of two types of iron MMTs on the flame retardation of LDPE composite

被引:31
作者
Deng, Cong [1 ]
Zhao, Jing [1 ]
Deng, Cheng-Liang [1 ]
Lv, Qiang [1 ]
Chen, Li [1 ]
Wang, Yu-Zhong [1 ]
机构
[1] Sichuan Univ, Coll Chem, Analyt & Testing Ctr,State Key Lab Polymer Mat En, Ctr Degradable & Flame Retardant Polymer Mat,Natl, Chengdu 610064, Peoples R China
关键词
Iron; MMT; Intumescent flame retardant; LDPE; SILICATE CLAY NANOCOMPOSITES; LOW-DENSITY; THERMAL-DEGRADATION; FIRE RETARDANCY; POLYETHYLENE; BEHAVIOR; SYSTEM; STABILITY; MECHANISM; CATALYST;
D O I
10.1016/j.polymdegradstab.2014.03.001
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
Both MMT synthesized by hydrothermal method (Fe-OMMT) and MMT prepared by modifying MMT using Fe3+ (Fe-MMT) were used to prepare flame-retardant low-density polyethylene (FR-LOPE) together with an intumescent flame retardant (IFR). The effects of two types of MMTs on the flame retardation of FR-LOPE were investigated by different measurements. Combustion tests showed that the limiting oxygen index (LOI) of LDPE/IFR28/Fe-MMT2 was increased to 34.6 from 29 of LDPE/IFR30, and the UL-94 rating of the former reached V-2 from no rating of the latter. Cone calorimeter (CC) test demonstrated that both Fe-OMMT and Fe-MMT improved the combustion behaviors of LDPE/IFR at about 2 wt%. LDPE/ IFR/Fe-MMT had a lower heat release rate (HRR), lower total heat release (THR) and more residues than LDPE/IFR/Fe-OMMT at the same loading in the range from 0.5 to 3 wt%. Scanning electron microscopy (SEM) observation showed that both Fe-MMT and Fe-OMMT could promote the formation of continuous and compact intumescent char layer in LDPE/IFR. Both CC and UL-94 tests vitrified that Fe-MMT had better contribution to IFR in fire resistance test. Thermogravimatric (TG) and Mossbauer spectrum etc. revealed that the different efficiency of Fe-OMMT and Fe-MMT should mainly be resulting from the structure difference between Fe-MMT and Fe-OMMT, in which the essential difference might be the different existing state of Fe in two types of MMTs. (C) 2014 Elsevier Ltd. All rights reserved.
引用
收藏
页码:1 / 10
页数:10
相关论文
共 47 条
[11]  
Gallina G, 1998, FIRE MATER, V22, P15, DOI 10.1002/(SICI)1099-1018(199801/02)22:1<15::AID-FAM626>3.0.CO
[12]  
2-3
[13]   Effect of Different Metallic Hydroxides on Flame-Retardant Properties of Low Density Polyethylene/Melamine Polyphosphate/Starch Composites [J].
Gao, Huliang ;
Hu, Shan ;
Han, Hongchang ;
Zhang, Jun .
JOURNAL OF APPLIED POLYMER SCIENCE, 2011, 122 (05) :3263-3269
[14]   TG-MS investigation of brominated products from the degradation of brominated flame retardants in high-impact polystyrene [J].
Grause, Guido ;
Karakita, Daiki ;
Ishibashi, Jun ;
Kameda, Tomohito ;
Bhaskar, Thallada ;
Yoshioka, Toshiaki .
CHEMOSPHERE, 2011, 85 (03) :368-373
[15]   Thermomechanical behavior of polymer/layered silicate clay nanocomposites based on unmodified low density polyethylene [J].
Grigoriadi, K. ;
Giannakas, A. ;
Ladavos, A. ;
Barkoula, N. -M. .
POLYMER ENGINEERING AND SCIENCE, 2013, 53 (02) :301-308
[16]   Effect of incorporation of butyl acrylate-iron chelate resin on the flammability properties of Mg(OH)2-LDPE compositions [J].
Hassan, MA .
POLYMER-PLASTICS TECHNOLOGY AND ENGINEERING, 2004, 43 (05) :1487-1501
[17]   Synthetic hydromagnesite as flame retardant.: Evaluation of the flame behaviour in a polyethylene matrix [J].
Haurie, L ;
Fernández, AI ;
Velasco, JI ;
Chimenos, JM ;
Cuesta, JML ;
Espiell, F .
POLYMER DEGRADATION AND STABILITY, 2006, 91 (05) :989-994
[18]   Compatibilization of polyethylene/aluminum hydroxide (PE/ATH) and polyethylene/magnesium hydroxide (PE/MH) composites with functionalized polyethylenes [J].
Hippi, U ;
Mattila, J ;
Korhonen, M ;
Seppälä, J .
POLYMER, 2003, 44 (04) :1193-1201
[19]   The PBDEs: An emerging environmental challenge and another reason for breast-milk monitoring programs [J].
Hooper, K ;
McDonald, TA .
ENVIRONMENTAL HEALTH PERSPECTIVES, 2000, 108 (05) :387-392
[20]   Synthesis and characterization of a novel nitrogen-containing flame retardant [J].
Hu, XP ;
Li, WY ;
Wang, YZ .
JOURNAL OF APPLIED POLYMER SCIENCE, 2004, 94 (04) :1556-1561