Color changes of dental resin composites by a salivary enzyme

被引:8
作者
Lee, YK
Lim, BS
Powers, JM
机构
[1] Seoul Natl Univ, Coll Dent, Dept Dent Biomat Sci, Seoul, South Korea
[2] Univ Texas, Hlth Sci Ctr, Houston Biomat Res Ctr, Dept Restorat Dent & Biomat,Houston Dent Branch, Houston, TX USA
来源
JOURNAL OF BIOMEDICAL MATERIALS RESEARCH PART B-APPLIED BIOMATERIALS | 2004年 / 70B卷 / 01期
关键词
dental resin composite; porcine liver esterase; enzymatic biodegradation; color stability;
D O I
10.1002/jbm.b.30018
中图分类号
R318 [生物医学工程];
学科分类号
0831 ;
摘要
The objective of this study was to evaluate the color change (DeltaE(ab)*) of dental resin composites immersed in a salivary enzyme of esterase (ETE, porcine liver esterase, 400 mU/ml) compared to those immersed in phosphate-buffered saline (PBS). The colors of three brands of resin composites of 13 shades were measured after polymerization and polishing with 1500-grit SiC paper and after immersion in PBS or ETE up to 9 weeks. Color was measured according to the CIELAB color scale. DeltaE(ab)* after immersion was calculated by the equation DeltaE(ab)* = [(DeltaL*)(2) + (Deltaa*)(2) + (Deltab*)(2)](1/2). Surface roughness (Ra) and Vickers hardness number (VHN) were measured. DeltaE(ab)* values after immersion in ETE was not higher than those in PBS. Immersion in solutions more than 3 weeks resulted in perceivable color changes (DeltaE(ab)* > 3.3) in one material, and immersion in solutions up to 9 weeks resulted in not-perceivable color changes in the other materials. Discoloration generally increased as the immersion period increased. For one composite, the value increased abruptly in the period of 3 days to 3 weeks of immersion. The change in Ra value after immersion was varied by the composite and shade. VHN decreased significantly after immersion in ETE for nine weeks. Immersion in PBS resulted in decreased VHN in two composites. (C) 2004 Wiley Periodicals, Inc.
引用
收藏
页码:66 / 72
页数:7
相关论文
共 27 条
[1]  
ASMUSSEN E, 1986, SCAND J DENT RES, V94, P174
[2]  
Craig RG, 2002, RESTORATIVE DENT MAT, V11th, P38
[3]   Color stability of new-generation indirect resins for prosthodontic application [J].
Douglas, RD .
JOURNAL OF PROSTHETIC DENTISTRY, 2000, 83 (02) :166-170
[4]  
Folwaczny M, 2000, OPER DENT, V25, P251
[5]  
FREUND M, 1990, SCAND J DENT RES, V98, P351
[6]   Effect of storage media on the fluoride release and surface microhardness of four polyacid-modified composite resins ("compomers") [J].
Geurtsen, W ;
Leyhausen, G ;
Garcia-Godoy, F .
DENTAL MATERIALS, 1999, 15 (03) :196-201
[7]   The effects of mouthrinses on microhardness and colour stability of aesthetic restorative materials [J].
Gürdal, P ;
Akdeniz, BG ;
Sen, BH .
JOURNAL OF ORAL REHABILITATION, 2002, 29 (09) :895-901
[8]   Five-year color changes of light-cured resin composites: influence of light-curing times [J].
Hosoya, Y .
DENTAL MATERIALS, 1999, 15 (04) :268-274
[9]  
International Standard Organization (ISO), 2000, 7491 ISO, V2000
[10]  
*ISO CIE, 1991, CIE STAND COL OBS