The role of vacancy defects and holes in the fracture of carbon nanotubes

被引:313
作者
Mielke, SL
Troya, D
Zhang, S
Li, JL
Xiao, SP
Car, R
Ruoff, RS
Schatz, GC
Belytschko, T
机构
[1] Northwestern Univ, Dept Chem, Evanston, IL 60208 USA
[2] Northwestern Univ, Dept Mech Engn, Evanston, IL 60208 USA
[3] Princeton Univ, Dept Chem, Princeton, NJ 08544 USA
[4] Univ Iowa, Dept Mech & Ind Engn, Iowa City, IA 52242 USA
[5] Univ Iowa, Ctr Comp Aided Design, Iowa City, IA 52242 USA
基金
美国国家科学基金会;
关键词
D O I
10.1016/j.cplett.2004.04.054
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
We present quantum mechanical calculations using density functional theory and semiempirical methods, and molecular mechanics (MM) calculations with a Tersoff-Brenner potential that explore the role of vacancy defects in the fracture of carbon nanotubes under axial tension. These methods show reasonable agreement, although the MM scheme systematically underestimates fracture strengths. One- and two-atom vacancy defects are observed to reduce failure stresses by as much as similar to26% and markedly reduce failure strains. Large holes - such as might be introduced via oxidative purification processes - greatly reduce strength, and this provides an explanation for the extant theoretical-experimental discrepancies. (C) 2004 Published by Elsevier B.V.
引用
收藏
页码:413 / 420
页数:8
相关论文
共 37 条
[11]   Bond-breaking bifurcation states in carbon nanotube fracture [J].
Dumitrica, T ;
Belytschko, T ;
Yakobson, BI .
JOURNAL OF CHEMICAL PHYSICS, 2003, 118 (21) :9485-9488
[12]   Molecular dynamics studies on mechanical properties of carbon nano tubes with pinhole defects [J].
Hirai, Y ;
Nishimaki, S ;
Mori, H ;
Kimoto, Y ;
Akita, S ;
Nakayama, Y ;
Tanaka, Y .
JAPANESE JOURNAL OF APPLIED PHYSICS PART 1-REGULAR PAPERS SHORT NOTES & REVIEW PAPERS, 2003, 42 (6B) :4120-4123
[13]   Production of defects in supported carbon nanotubes under ion irradiation [J].
Krasheninnikov, AV ;
Nordlund, K ;
Keinonen, J .
PHYSICAL REVIEW B, 2002, 65 (16) :1-8
[14]   Defect-induced oxidation of graphite [J].
Lee, SM ;
Lee, YH ;
Hwang, YG ;
Hahn, JR ;
Kang, H .
PHYSICAL REVIEW LETTERS, 1999, 82 (01) :217-220
[15]   Brittle and ductile behavior in carbon nanotubes [J].
Nardelli, MB ;
Yakobson, BI ;
Bernholc, J .
PHYSICAL REVIEW LETTERS, 1998, 81 (21) :4656-4659
[16]   Mechanism of strain release in carbon nanotubes [J].
Nardelli, MB ;
Yakobson, BI ;
Bernholc, J .
PHYSICAL REVIEW B, 1998, 57 (08) :R4277-R4280
[17]   Temperature-dependent morphological evolution og HOPG graphite upon exposure to hyperthermal O(3P) atoms [J].
Nicholson, KT ;
Minton, TK ;
Sibener, SJ .
PROGRESS IN ORGANIC COATINGS, 2003, 47 (3-4) :443-447
[18]   Ideal tensile strength and band gap of single-walled carbon nanotubes [J].
Ogata, S ;
Shibutani, Y .
PHYSICAL REVIEW B, 2003, 68 (16)
[19]   Stiffness of single-walled carbon nanotubes under large strain [J].
Ozaki, T ;
Iwasa, Y ;
Mitani, T .
PHYSICAL REVIEW LETTERS, 2000, 84 (08) :1712-1715
[20]  
Perdew JP, 1997, PHYS REV LETT, V78, P1396, DOI 10.1103/PhysRevLett.77.3865