Characterization of direct ink write pure silk fibroin based on alcohol post-treatments

被引:6
作者
Casanova-Batlle, Enric [1 ]
Guerra, Antonio J. [2 ]
Ciurana, Joaquim [1 ]
机构
[1] Univ Girona, Dept Mech Engn & Ind Construct, C Maria Aurelia Capmany 61, Girona 17003, Spain
[2] Ctr Tecnol Catalunya, EURECAT, Placa Ciencia 2, Manresa 08243, Spain
关键词
Silk fibroin; Direct ink writing; Post-treatments; Additive manufacturing; Materials engineering; DEGRADATION; FILMS; BIOMATERIALS; REGENERATION; SCAFFOLDS;
D O I
10.1016/j.polymertesting.2022.107784
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Silk fibroin (SF) has been successfully used for medical devices due to its biodegradability with non-toxic end products, high tensile strength and mechanical robustness, but also because of its high flexibility potential. Although natural silk fibers have excellent strength and flexibility, regenerated silk materials generally become brittle in the dry state. For this reason, researchers have studied the effects that manufacturing and post-treatment parameters have on their mechanical properties, but they have also studied the impact on other factors such as biodegradability on the environment. This work presents an optimized process for direct ink write a regenerated SF bioink and its possible post-treatments. A simple method to concentrate the aqueous SF has been reported. The technique was then employed to 3D print test specimens for multiple mechanical analysis to characterize the resulting parameters of the processed silk. The effect of post-treating the material with different processes (no-treatment, immersion in ethanol for 24 h, and subsequently immersion in methanol for 30, 60 or 120 min) was explored. The different post-treatments resulted in distinct effects on the silk properties, suggesting that SF molecular structure could be controlled by the post-treatment process. The results showed a transition to phosphate-buffered saline (PBS)-insoluble silk when the silk was treated with alcohols. This resulted in a more brittle material than the untreated group, with a lower strain at break. Nevertheless, the post-treatments enhanced the stability of silk in water, as they reported greater insolubility in PBS than the untreated group. This study characterizes and discusses the mechanical properties of SF processed with a novel additive manufacturing method intended for customization of medical devices.
引用
收藏
页数:10
相关论文
共 39 条
[1]   Ag/silk fibroin nanofibers: Effect of fibroin morphology on Ag+ release and antibacterial activity [J].
Calamak, Semih ;
Aksoy, Eda Ayse ;
Ertas, Nusret ;
Erdogdu, Ceren ;
Sagiroglu, Meral ;
Ulubayram, Kezban .
EUROPEAN POLYMER JOURNAL, 2015, 67 :99-112
[2]  
Casanova-Batlle E., 2021, POST SESS BIOM BIOF
[3]   Preparation and Characterization of Insoluble Silk Fibroin/Chitosan Blend Films [J].
de Moraes, Mariana Agostini ;
Nogueira, Grinia Michelle ;
Weska, Raquel Farias ;
Beppu, Marisa Masumi .
POLYMERS, 2010, 2 (04) :719-727
[4]   Crosslinked fibroin nanoparticles using EDC or PEI for drug delivery: physicochemical properties, crystallinity and structure [J].
Duy Toan Pham ;
Saelim, Nuttawut ;
Tiyaboonchai, Waree .
JOURNAL OF MATERIALS SCIENCE, 2018, 53 (20) :14087-14103
[5]   Tensile strength of 3D printed materials: Review and reassessment of test parameters [J].
Floor, Jim ;
van Deursen, Bas ;
Tempelman, Erik .
MATERIALS TESTING, 2018, 60 (7-8) :679-686
[6]   Direct-write assembly of microperiodic silk fibroin scaffolds for tissue engineering applications [J].
Ghosh, Sourabh ;
Parker, Sara T. ;
Wang, Xianyan ;
Kaplan, David L. ;
Lewis, Jennifer A. .
ADVANCED FUNCTIONAL MATERIALS, 2008, 18 (13) :1883-1889
[7]   Mechanistic evaluation of long-term in-stent restenosis based on models of tissue damage and growth [J].
He, Ran ;
Zhao, Liguo ;
Silberschmidt, Vadim V. ;
Liu, Yang .
BIOMECHANICS AND MODELING IN MECHANOBIOLOGY, 2020, 19 (05) :1425-1446
[8]   The Future of Cardiovascular Stents: Bioresorbable and Integrated Biosensor Technology [J].
Hoare, Daniel ;
Bussooa, Anubhav ;
Neale, Steven ;
Mirzai, Nosrat ;
Mercer, John .
ADVANCED SCIENCE, 2019, 6 (20)
[9]   In vitro degradation of silk fibroin [J].
Horan, RL ;
Antle, K ;
Collette, AL ;
Huang, YZ ;
Huang, J ;
Moreau, JE ;
Volloch, V ;
Kaplan, DL ;
Altman, GH .
BIOMATERIALS, 2005, 26 (17) :3385-3393
[10]   Regulation of Silk Material Structure by Temperature-Controlled Water Vapor Annealing [J].
Hu, Xiao ;
Shmelev, Karen ;
Sun, Lin ;
Gil, Eun-Seok ;
Park, Sang-Hyug ;
Cebe, Peggy ;
Kaplan, David L. .
BIOMACROMOLECULES, 2011, 12 (05) :1686-1696