Investigation of Decarburization in Spring Steel Production Process - Part I: Experiments

被引:36
作者
Li, Dejun [1 ]
Anghelina, D. [2 ]
Burzic, D. [1 ]
Zamberger, J. [3 ]
Kienreich, R. [4 ]
Schifferl, H. [5 ]
Krieger, W. [2 ]
Kozeschnik, E. [6 ]
机构
[1] Leoben Forsch GmbH, Mat Ctr, A-8700 Leoben, Austria
[2] Univ Min & Met Leoben, Chair Met, A-8700 Leoben, Austria
[3] Styria Federn GmbH, A-8750 Judenburg, Austria
[4] Voestalpine Austria Draht GmbH, Walzwerk Donawitz, A-8792 St Peter Freienstein, Austria
[5] Voestalpine Stahl Donawitz GmbH & CoKG, A-8700 Leoben, Austria
[6] Vienna Univ Technol, Inst Mat Sci & Technol, A-1040 Vienna, Austria
关键词
decarburization; oxidation; spring steel; LOW-CARBON-STEEL; INTERNAL OXIDATION; HIGH-TEMPERATURES; OXIDE-SCALE; INTERFACE; ALLOYS; GROWTH; STRIP;
D O I
10.2374/SRI08SP069
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Decarburization and oxidation have considerable influence on the product properties of spring steels. The investigations in part I of this paper concentrate on the experimental determination of the influence of different thermal cycles on the decarburization process. With the thermo-mechanical simulator Gleeble 1500, the influence of different process parameters, such as the time between furnace reheating and hot rolling, the hot rolling temperature, finish rolling temperature, laying temperature, and the alpha ->gamma phase transformation temperature range, is systematically investigated. In part II of this paper [15], numerical simulation techniques are applied to simulate the decarburization behavior under the experimental conditions, which are described in the present part I.
引用
收藏
页码:298 / 303
页数:6
相关论文
共 15 条
[1]   Review of the high-temperature oxidation of iron and carbon steels in air or oxygen [J].
Chen, RY ;
Yuen, WYD .
OXIDATION OF METALS, 2003, 59 (5-6) :433-468
[2]   Oxide-scale structures formed on commercial hot-rolled steel strip and their formation mechanisms [J].
Chen, RY ;
Yuen, WYD .
OXIDATION OF METALS, 2001, 56 (1-2) :89-118
[3]   Influence of silicon and aluminum additions on the oxidation resistance of a lean-chromium stainless steel [J].
Dunning, JS ;
Alman, DE ;
Rawers, JC .
OXIDATION OF METALS, 2002, 57 (5-6) :409-425
[4]   Distribution around the oxide-substrate interface of alloying elements in low-carbon steel [J].
Genève, D ;
Confente, M ;
Rouxel, D ;
Pigeat, P ;
Weber, B .
OXIDATION OF METALS, 1999, 51 (5-6) :527-537
[5]   Characterization and growth of oxide films [J].
Graham, MJ ;
Hussey, RJ .
CORROSION SCIENCE, 2002, 44 (02) :319-330
[6]   Internal oxidation and carburisation of heat-resistant alloys [J].
Hänsel, M ;
Boddington, CA ;
Young, DJ .
CORROSION SCIENCE, 2003, 45 (05) :967-981
[7]   Intergranular and internal oxidation during hot-rolling process in ultra-low carbon steel [J].
Kizu, T ;
Nagataki, Y ;
Inazumi, T ;
Hosoya, Y .
ISIJ INTERNATIONAL, 2002, 42 (02) :206-214
[8]  
Kucera J., 2001, Acta Technica CSAV, V46, P51
[9]   Investigation of Decarburization in Spring Steel Production Process - Part II: Simulation [J].
Li, Dejun ;
Anghelina, D. ;
Burzic, D. ;
Krieger, W. ;
Kozeschnik, E. .
STEEL RESEARCH INTERNATIONAL, 2009, 80 (04) :304-310
[10]  
MAYER A, 1963, EISEN, V83, P1169