Effect of test temperature on tensile behavior of Fe-6.5wt.%Si alloy as-cast strip

被引:3
作者
Xuan, Dongpo [1 ]
Zhou, Cheng [1 ]
Zhou, You [1 ]
Jiang, Tianliang [1 ]
Zhu, Biji [1 ]
Fan, Wenhao [1 ]
机构
[1] Univ Sci & Technol Beijing, Sch Mat Sci & Engn, Beijing 100083, Peoples R China
关键词
Twin-roll casting; Fe-6.5wt%Si alloy; Tensile property; Ordered phase; PERCENT-SI ALLOY; MAGNETIC-PROPERTIES; ELECTRICAL STEEL; MECHANICAL-PROPERTIES; MICROSTRUCTURE; DEFORMATION; TEXTURE; DUCTILITY; PHASE;
D O I
10.1016/j.jmmm.2022.169540
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The non-oriented Fe-6.5wt.%Si alloy as-cast strip is prepared by the top side-pouring twin-roll casting (TSTRC) process and the solidification structure of the as-cast strip is a uniform fine equiaxed grain structure. This paper studied the mechanical properties, fracture morphology, ordered phase morphology, and types of Fe-6.5wt.%Si alloy as-cast strips at different temperatures. The results show that the yield and tensile strength of the as-cast strip decreased gradually with the increase of tensile temperature, and the elongation after fracture increased gradually. The temperature rise prevented the formation of cleavage cracks, and the temperature rise is an effective method to improve the plasticity of Fe-6.5wt.%Si alloys. Concurrently, the ambient temperature is the main factor determining the tensile mechanical properties of Fe-6.5wt.%Si alloy at medium temperature. When the stretching temperature exceeds 500 degrees C, the Fe-6.5wt.%Si alloy has apparent plastic deformation ability. The Fe-6.5wt.%Si alloy exhibits excellent elongation when the stretching temperature is 700 degrees C. The serration fluctuations that appear on the 400 degrees C stretch curve should be attributed to the Portevin-Le Chatelier (PLC) effect caused by the reordering of the antiphase domains and the deformation-induced disorder. The Fe-6.5wt.%Si alloy as-cast strip is directly subjected to warm-rolling without the hot-rolling. When the warm-rolling is per -formed at the temperature of 700 degrees C, there are almost no cracks at the edge of the plate, the edge cracks are effectively controlled, and the surface quality of the warm-rolled sheet is fine. The obtained 700 degrees C warm-rolled sheets were cold-rolled at room temperature, and after recrystallization annealing, the sample had good comprehensive magnetic properties. Suppose the TSTRC-warm rolling-cold rolling-annealing process prepares the Fe-6.5wt.%Si alloy cold-rolled sheet. In that case, the production efficiency will be significantly improved, the process flow will be shortened, and the goal of energy-saving and emission reduction will be achieved.
引用
收藏
页数:10
相关论文
共 50 条
[31]   Effect of Sr on microstructure, tensile properties and wear behavior of as-cast Mg-6Zn-4Si alloy [J].
Cong, Mengqi ;
Li, Ziquan ;
Liu, Jinsong ;
Li, Shaohua .
MATERIALS & DESIGN, 2014, 53 :430-434
[32]   High temperature tensile properties of as-cast and forged CrMnFeCoNi high entropy alloy [J].
Sun, Jie ;
Zhao, Wenxiang ;
Yan, Pei ;
Li, Siyu ;
Dai, Zhicheng ;
Jiao, Li ;
Qiu, Tianyang ;
Wang, Xibin .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2022, 850
[33]   Effect of pulsed magneto oscillation and phosphorus on microstructure and tensile properties of as-cast Al-25% Si alloy [J].
Dang, Bo ;
Jian, Zengyun ;
Xu, Junfeng .
INTERNATIONAL JOURNAL OF MATERIALS RESEARCH, 2021, 112 (04) :295-302
[34]   Deformation twinning in an Fe-6.5 wt.% Si alloy with columnar grains during intermediate temperature compression [J].
Xie, Jianxin ;
Fu, Huadong ;
Zhang, Zhihao ;
Jiang, Yanbin .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2012, 538 :315-319
[35]   Effect of friction stir processing on microstructure and tensile properties of as-cast Mg-8Li-3Al-2Sn (wt.%) alloy [J].
Chen, Xiaoyang ;
Zhang, Yang ;
Cong, Mengqi .
VACUUM, 2020, 175
[36]   Influence of hot rolling reduction rate on the microstructure, texture and magnetic properties of a strip-cast Fe-6.5 wt% Si grain-oriented electrical steel [J].
Xu, Haijie ;
Xu, Yunbo ;
He, Youliang ;
Jiao, Haitao ;
Yue, Steve ;
Li, Jianping .
JOURNAL OF MAGNETISM AND MAGNETIC MATERIALS, 2020, 494
[37]   Effects of rolling temperature on microstructure, texture, formability and magnetic properties in strip casting Fe-6.5 wt% Si non-oriented electrical steel [J].
Liu, Hai-Tao ;
Li, Hao-Ze ;
Li, Hua-Long ;
Gao, Fei ;
Liu, Guo-Huai ;
Luo, Zhong-Han ;
Zhang, Feng-Quan ;
Chen, Sheng-Lin ;
Cao, Guang-Ming ;
Liu, Zhen-Yu ;
Wang, Guo-Dong .
JOURNAL OF MAGNETISM AND MAGNETIC MATERIALS, 2015, 391 :65-74
[38]   Effect of 0.5 mass% Cu Addition on Ductility and Magnetic Properties of Fe-6.5Si Alloy [J].
Cheng, Zhao-yang ;
Liu, Jing ;
Chen, Wen-si ;
Zhu, Jia-chen ;
Lin, Xi-feng ;
Xiang, Zhi-dong .
JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2016, 23 (07) :717-721
[39]   Influence of La Addition on Order-Disorder Transformation and Deformation Softening Behavior of Fe-6.5 wt % Si Alloy [J].
Cai, Guojun ;
He, Longting ;
Huang, Yanru .
PHYSICS OF METALS AND METALLOGRAPHY, 2022, 123 (13) :1343-1347
[40]   Gradient Recrystallization Behavior of a Moderate Warm-Rolled Non-Oriented Fe-6.5wt%Si Alloy [J].
Xu, Haijie ;
Xu, Cheng ;
Jiang, Lulan ;
Zhang, Yuanxiang ;
Shu, Xuedao ;
Lin, Xiaogang .
METALS, 2023, 13 (02)