Recovery of Iron from Lead Slag with Coal-Based Direct Reduction Followed by Magnetic Separation

被引:16
作者
Wang, Chuanlong [1 ]
Yang, Huifen [1 ]
Jiang, Beiping [1 ]
Zhang, Jinlong [1 ]
Lu, Linfei [1 ]
Tang, Qiongyao [1 ]
机构
[1] Univ Sci & Technol Beijing, Sch Civil & Environm Engn, Beijing 100083, Peoples R China
来源
SELECTED PROCEEDINGS OF THE EIGHTH INTERNATIONAL CONFERENCE ON WASTE MANAGEMENT AND TECHNOLOGY | 2014年 / 878卷
关键词
Solid waste; Lead slag; Direct reduction; Recovery; Metallic iron; ORE;
D O I
10.4028/www.scientific.net/AMR.878.254
中图分类号
X [环境科学、安全科学];
学科分类号
08 ; 0830 ;
摘要
Iron recovery from a lead slag in Henan province was carried out with the technique of coal-based direct reduction followed by magnetic separation. Scanning electron microscopy (SEM) was used to investigate the transformation of iron-containing minerals and the particle size of metallic iron generated by coal reduction. The results showed that technique is feasible for iron recovery from the lead slag. Under the conditions of weight ratio of slag: coal: CaO as 50:15:5, the roasted temperature of 1250 degrees C for 45 min, and then two stage of grinding and twice magnetic separation, the metallic iron powder was obtained with the iron grade of 92.85% and iron recovery of 92.85%. The iron-containing minerals in the forms of hercynite, fayalite and maghemite were mianly transformed into metallic iron and the particle size of metallic iron was more than 50 mu m. Therefore, the metallic iron in roasted product can be dissociated by coarse grinding and further was separated by magnetic separation to recover the metallic iron.
引用
收藏
页码:254 / 263
页数:10
相关论文
共 22 条
  • [1] Effects of pH, pulp density and particle size on solubilization of metals from a Pb/Zn smelting slag using indigenous moderate thermophilic bacteria
    Guo, Zhaohui
    Zhang, Long
    Cheng, Yi
    Xiao, Xiyuan
    Pan, Fengkai
    Jiang, Kaiqi
    [J]. HYDROMETALLURGY, 2010, 104 (01) : 25 - 31
  • [2] Han F., 2001, POWDER METALL TECHNO, V19, P33, DOI [10.19591/j.cnki.cnll-1974/tf.2001.01.008, DOI 10.19591/J.CNKI.CNLL-1974/TF.2001.01.008]
  • [3] He Q., 2008, Jiangxi Nonferr. Met, V22, P29, DOI [10.13264/j.cnki.ysjskx.2008.02.009, DOI 10.13264/J.CNKI.YSJSKX.2008.02.009]
  • [4] Huang Z.C., 2009, METAL MINE, P173
  • [5] Jang X.X., 2010, J CHINA METAL MARKET, V45, P17
  • [6] Li K.M., 2012, China Nonferrous Metall, P70
  • [7] Effect of coal levels during direct reduction roasting of high phosphorus oolitic hematite ore in a tunnel kiln
    Li Yongli
    Sun Tichang
    Zou Anhua
    Xu Chengyan
    [J]. INTERNATIONAL JOURNAL OF MINING SCIENCE AND TECHNOLOGY, 2012, 22 (03) : 323 - 328
  • [8] Thermal investigations of direct iron ore reduction with coal
    Liu, GS
    Strezov, V
    Lucas, JA
    Wibberley, LJ
    [J]. THERMOCHIMICA ACTA, 2004, 410 (1-2) : 133 - 140
  • [9] Liu H.Y., 2008, J SCI TECHNOLOGY INF, V30, P324
  • [10] Lu S.L., 2010, J GOLD SCI TECHNOLOG, V04, P71