Al2O3(w)-Al2O3(n)-ZrO2 (TZ-3Y)n multi-scale nanocomposite: An alternative for different dental applications?

被引:26
作者
Nevarez-Rascon, A. [2 ]
Aguilar-Elguezabal, A. [1 ]
Orrantia, E. [1 ]
Bocanegra-Bernal, M. H. [1 ]
机构
[1] CIMAV SC, Ctr Invest Mat Avanzados, Lab Nacl Nanotecnol, Chihuahua 31109, Mexico
[2] Univ Autonoma Chihuahua, Escuela Odontol, Chihuahua 31000, Mexico
关键词
Zirconia toughened alumina; Crack deflection; Hardness; Fracture toughness; REINFORCED CERAMIC COMPOSITES; TOUGHENED ALUMINA CERAMICS; SILICON-CARBIDE WHISKERS; HIGH-TOUGHNESS CERAMICS; FRACTURE-TOUGHNESS; MECHANICAL-PROPERTIES; CRACK DEFLECTION; RESIN COMPOSITES; MICROSTRUCTURE; ZIRCONIA;
D O I
10.1016/j.actbio.2009.06.029
中图分类号
R318 [生物医学工程];
学科分类号
0831 ;
摘要
The influence of the addition of Al2O3 whiskers (2.5 wt.% up to 30 wt.%) on Vickers hardness and fracture toughness in an Al2O3(n)+ZrO2 (TZ-3Y)(n) (90, 80 and 70 wt.%) composite was investigated. Green compacts were obtained by uniaxial pressing at 50 MPa and pressureless sintering at 1500 degrees C in air for 2 h. After sintering, relative densities ranging from 75% to 97% were reached. The whiskers resisted particle rearrangement owing to the extensive sliding distances along the whisker boundaries during sintering and the high length/diameter ratios. Sintering becomes more difficult with increasing whisker content, because whiskers come into contact with each other, forming a rigid network which hinders densification. The 2.5 wt.% Al2O3 whiskers + 27.5 wt.% Al2O3 nanoparticles + 70 wt.% TZ-3Y composite showed a hardness > 13 GPa and a maximum fracture toughness of 6.9 MPa m(-1/2), with an average grain size of 0.4 +/- 0.17 mu m. The observed crack deflection was an important mechanism in the improved fracture toughness of the composite. In addition, the grain size and residual porosity also seem to be factors in obtaining a wide range of hardness as well as fracture toughness by varying the Al2O3 whiskers and ZrO2 (TZ-3Y) content. The use of alumina-whisker-reinforced composites in dental applications could be promising for increasing hardness and fracture toughness compared with other materials. The reported values for these composites can compete with those of commercially available materials in different dental applications. (C) 2009 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:563 / 570
页数:8
相关论文
共 57 条
[1]  
An JW, 2002, J CERAM PROCESS RES, V3, P201
[2]  
[Anonymous], 1999, ANN BOOK ASTM STAND, V03.01
[3]  
ANUSAVICE J, 2004, PHILLIPS SCI DENT MA
[4]  
BECHER PF, 1984, J AM CERAM SOC, V67, pC267, DOI 10.1111/j.1151-2916.1984.tb19694.x
[5]   TOUGHENING BEHAVIOR IN WHISKER-REINFORCED CERAMIC MATRIX COMPOSITES [J].
BECHER, PF ;
HSUEH, CH ;
ANGELINI, P ;
TIEGS, TN .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1988, 71 (12) :1050-1061
[6]   OVERVIEW NO-52 - TOUGHENING BEHAVIOR IN CERAMICS ASSOCIATED WITH THE TRANSFORMATION OF TETRAGONAL ZRO2 [J].
BECHER, PF .
ACTA METALLURGICA, 1986, 34 (10) :1885-1891
[7]  
BENGISU M, 1994, ANNU REV MATER SCI, V24, P83
[8]   HOT ISOSTATICALLY PRESSED ALUMINA SILICON CARBIDE-WHISKER COMPOSITES [J].
BJORK, L ;
HERMANSSON, LAG .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1989, 72 (08) :1436-1438
[9]  
CARTER DH, 1987, J AM CERAM SOC, V70, pC79, DOI 10.1111/j.1151-2916.1987.tb04992.x
[10]   Quantitative evaluation by fractal analysis of indentation crack paths in Si3N4-SiCW composites [J].
Celli, A ;
Tucci, A ;
Esposito, L .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 1999, 19 (04) :441-449