Fatigue testing of glass/epoxy joints in timber up to the endurance limit

被引:2
作者
Claisse, P. A. [1 ]
Davis, T. J. [1 ]
Masse, B. [1 ]
机构
[1] Coventry Univ, Civil Engn Grp, Coventry CV1 5FB, W Midlands, England
关键词
timber; glass fibre; epoxy; fatigue; timber joints;
D O I
10.1016/j.conbuildmat.2005.07.003
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
Concern about fatigue is one of the factors limiting use of glass/epoxy jointing systems for timber in construction. In this paper, a series of high-cycle fatigue tests are reported which indicate that the performance is as good, if not superior to, conventional jointing systems. The performance of the joints was found to produce a straight line on a logarithmic S-N plot and thus be readily predictable for design purposes. (c) 2005 Elsevier Ltd. All rights reserved.
引用
收藏
页码:139 / 149
页数:11
相关论文
共 14 条
  • [1] [Anonymous], 1999, SAND990989
  • [2] [Anonymous], 1996, 5268 BS
  • [3] ANSELL, 1995, TIMBER ENG STEP1 199
  • [4] BAINBRIDGE RJ, 2000, FATIGUE PERFORMANCE, P33
  • [5] BENHAM PP, 1996, MECHANICS ENG MAT
  • [6] *BRIT STAND I, 2004, EN199511 BRIT STAND
  • [7] *BRIT STAND I, 1972, COD BAS DAT DES BUIL
  • [8] High performance jointing systems for timber
    Claisse, PA
    Davis, TJ
    [J]. CONSTRUCTION AND BUILDING MATERIALS, 1998, 12 (08) : 415 - 425
  • [9] Bolted joints in glulam and structural timber composites
    Davis, TJ
    Claisse, PA
    [J]. CONSTRUCTION AND BUILDING MATERIALS, 2000, 14 (08) : 407 - 417
  • [10] Resin-injected dowel joints in glulam and structural timber composites
    Davis, TJ
    Claisse, PA
    [J]. CONSTRUCTION AND BUILDING MATERIALS, 2001, 15 (04) : 157 - 167