DSC study of morphological changes in segmented polyurethane elastomers

被引:38
|
作者
Bajsic, EG [1 ]
Rek, V
Sendijarevic, A
Sendijarevic, V
Frisch, KC
机构
[1] Univ Zagreb, Fac Chem Engn & Technol, Zagreb 10000, Croatia
[2] Univ Detroit Mercy, Polymer Technol Inc, Detroit, MI 48221 USA
来源
JOURNAL OF ELASTOMERS AND PLASTICS | 2000年 / 32卷 / 02期
关键词
annealing; glass transition; microphase separation; segmented PUR elastomers;
D O I
10.1106/Q4CF-0J7G-0H93-C265
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Annealing studies were carried out to investigate the morphological changes in segmented polyurethane elastomers (PUR) induced by annealing as a function of temperature. Four series of PUR elastomers were studied by varying the hard segment type (MDI/BD and H12MDI/BD), the content of the hard segment (35-57% by weight), the soft segment type (PTMO and PCL) and the soft segment molecular weight (PTMO 1000 and 2000, PCL 1250). Differential scanning calorimetry analyses, DSC, of these materials provided information about morphological changes during annealing at various temperatures (70, 130, 160 and 180 degrees C). The effects of annealing process are visible in PUR elastomers based on the aromatic (MDI/BD) isocyanate and those based on the cycloaliphatic (H12MDI/BD) isocyanate. The values of the soft segment glass transition temperature (T-g) decreased on the higher annealing temperatures in PUR elastomers based on the aromatic isocyanate and on the cycloaliphatic isocyanate. This behaviour was connecting with better phase separation after annealing in both PUR elastomers. A comparison of thermal results shows that the MDI/BD series elastomers exhibit a considerable degree of hard segment crystallinity whereas the H12MDI/BD series elastomers are amorphous. Analyses of the DSC results indicate that increasing of the hard segment content leads to higher T-g values for control samples and samples after annealing, except for some samples whose T-g decreased after annealing at higher temperatures. This behaviour results from partial compatibility and therefore phase mixing of soft and hard segments. Endotherms due to the ordering in the hard segment domains appeared at higher temperature. The T-g of PUR elastomers based on polyether's soft segment phase increased with annealing process. The opposite effect was obtained in PUR elastomers based on polyester's soft segments. The same effect was obtained for elastomers with higher hard segment content. The results showed that the soft segment T-g decreased with increased molecular weight of the soft segments (PTMO 2000). This indicates that the greater degree of phase separation was allowed by the longer soft segment lengths. Endotherms resulting from hard segment ordering appeared at higher temperatures for higher annealing temperatures.
引用
收藏
页码:162 / 182
页数:21
相关论文
共 50 条
  • [41] Capability of conventional Differential Scanning Calorimetry (DSC), temperature modulated DSC (MDSC) and StepScan DSC for the glass transition phenomenon study
    Cernosek, Z.
    Holubova, J.
    Cernoskova, E.
    OPTOELECTRONICS AND ADVANCED MATERIALS-RAPID COMMUNICATIONS, 2007, 1 (06): : 277 - 280
  • [42] THE EFFECT OF MICROPHASE-SEPARATED STRUCTURES ON THE BLOOD CONTACTING PROPERTIES OF A SERIES OF LINEAR SEGMENTED POLY(ETHERURETHANEUREA) ELASTOMERS
    MATTHEWS, KH
    KODAMA, M
    MATERIALS SCIENCE & ENGINEERING C-BIOMIMETIC MATERIALS SENSORS AND SYSTEMS, 1994, 2 (1-2): : 51 - 59
  • [43] Behavior in a humid medium of segmented polyurethane-ureas with dissimilar thermodynamically compatible and incompatible flexible blocks
    M. A. Makarova
    V. V. Tereshatov
    V. N. Strel’nikov
    Russian Journal of Applied Chemistry, 2010, 83 : 1360 - 1366
  • [44] The reinforcing effect of cyclic binary secondary amine chain extenders on the cryogenic performance of thermoplastic polyurethane elastomers
    Geng, Yanfei
    Wang, Meng
    Li, Wenke
    Yi, Pengcheng
    Ji, Yumei
    Stewart, Callum
    Yang, Yike
    Liu, Feng
    JOURNAL OF APPLIED POLYMER SCIENCE, 2022, 139 (27)
  • [45] Microphase-separated structure and mechanical properties of novel polyurethane elastomers prepared with ether based diisocyanate
    Furukawa, M
    Mitsui, Y
    Fukumaru, T
    Kojio, K
    POLYMER, 2005, 46 (24) : 10817 - 10822
  • [46] The effects of different positions of the pyridine functional groups on the dielectric relaxation of the heterocyclic polyurethane-urea elastomers
    Potolinca, Violeta Otilia
    Buruiana, Emil C.
    Oprea, Stefan
    MATERIALS TODAY COMMUNICATIONS, 2017, 10 : 25 - 33
  • [47] Hydrolysis-resistant polyurethane elastomers synthesized from hydrophobic bio-based polyfarnesene diol
    Zhang, Jun
    Chen, Jianjun
    Yao, Ming
    Jiang, Zhiguo
    Ma, Yuhong
    JOURNAL OF APPLIED POLYMER SCIENCE, 2019, 136 (25)
  • [48] Behavior in a Humid Medium of Segmented Polyurethane-Ureas with Dissimilar Thermodynamically Compatible and Incompatible Flexible Blocks
    Makarova, M. A.
    Tereshatov, V. V.
    Strel'nikov, V. N.
    RUSSIAN JOURNAL OF APPLIED CHEMISTRY, 2010, 83 (08) : 1360 - 1366
  • [49] The study of the glass transition by the stepscan DSC technique
    Holubová, J
    Cernosek, Z
    Cernosková, E
    JOURNAL OF OPTOELECTRONICS AND ADVANCED MATERIALS, 2005, 7 (05): : 2671 - 2676
  • [50] The selenium based chalcogenide glasses with low content of As and Sb: DSC, StepScan DSC and Raman spectroscopy study
    Holubova, J.
    Cernosek, Z.
    Cernoskova, E.
    JOURNAL OF NON-CRYSTALLINE SOLIDS, 2009, 355 (37-42) : 2050 - 2053