Crystal orientation-dependent fatigue characteristics in micrometer-sized single-crystal silicon

被引:17
作者
Ikehara, Tsuyoshi [1 ]
Tsuchiya, Toshiyuki [2 ]
机构
[1] Natl Inst Adv Ind Sci & Technol, 1-2 Namiki, Tsukuba, Ibaraki 3058564, Japan
[2] Kyoto Univ, Grad Sch Engn, Dept Micro Engn, Nishikyo Ku, Kyotodaigaku Katsura C3, Kyoto 6158540, Japan
来源
MICROSYSTEMS & NANOENGINEERING | 2016年 / 2卷
关键词
fatigue; fracture; lifetime; MEMS; reliability; resonator; single-crystal silicon; SUBCRITICAL CRACK-GROWTH; HIGH-CYCLE FATIGUE; DUCTILE TRANSITION; POLYSILICON; FRACTURE; STRESS; TEMPERATURE; BEHAVIOR; FAILURE;
D O I
10.1038/micronano.2016.27
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Repetitive bending fatigue tests were performed using five types of single-crystal silicon specimens with different crystal orientations fabricated from {100} and {110} wafers. Fatigue lifetimes in a wide range between 10(0) and 10(10) were obtained using fan-shaped resonator test devices. Fracture surface observation via scanning electron microscope (SEM) revealed that the {111} plane was the primary fracture plane. The crack propagation exponent n was estimated to be 27, which was independent of the crystal orientation and dopant concentration; however, it was dependent on the surface conditions of the etched sidewall. The fatigue strengths relative to the deflection angle were orientation dependent, and the ratios of the factors obtained ranged from 0.86 to 1.25. The strength factors were compared with those obtained from finite element method stress analyses. The calculated stress distributions showed strong orientation dependence, which was well-explained by the elastic anisotropy. The comparison of the strength factors suggested that the first principal stress was a good criterion for fatigue fracture. We include comparisons with specimens tested in our previous report and address the tensile strength, initial crack length, volume effect, and effects of surface roughness such as scallops.
引用
收藏
页数:9
相关论文
共 50 条
  • [41] Measurement of anisotropic fatigue life in micrometre-scale single-crystal silicon specimens
    Ikehara, T.
    Tsuchiya, T.
    MICRO & NANO LETTERS, 2010, 5 (01): : 49 - 52
  • [42] Characteristic features of slip bands in submicron single-crystal gold component produced by fatigue
    Sumigawa, Takashi
    Shiohara, Ryosuke
    Matsumoto, Kenta
    Kitamura, Takayuki
    ACTA MATERIALIA, 2013, 61 (07) : 2692 - 2700
  • [43] Temperature dependent fatigue crack propagation in a single crystal Ni-base superalloy affected by primary and secondary orientations
    Suzuki, Shiyu
    Sakaguchi, Motoki
    Inoue, Hirotsugu
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2018, 724 : 559 - 565
  • [44] A Hydrogen – Vacancy Defect In Single-Crystal Silicon
    V. V. Melnikov
    Russian Physics Journal, 2016, 59 : 618 - 625
  • [45] A study on the etching characteristics of atmospheric pressure plasma for single-crystal silicon wafer
    Guo, Weijia
    Calija, Laurence Michael M.
    Xu, Peng
    Liu, Kui
    Kumar, Senthil A.
    VACUUM, 2021, 190
  • [46] Molecular dynamics simulation on crystal defects of single-crystal silicon during elliptical vibration cutting
    Liu, Changlin
    To, Suet
    Sheng, Xuexiang
    Xu, Jianfeng
    INTERNATIONAL JOURNAL OF MECHANICAL SCIENCES, 2023, 244
  • [47] Effect of crystal orientation on elastic stresses and vibration characteristics of nickel-based single crystal turbine blade
    Li, Lei
    Zeng, Yan
    Li, Jie
    Zhao, Yanchao
    Yuan, Tianyu
    Yue, Zhufeng
    MATERIALS TODAY COMMUNICATIONS, 2023, 35
  • [48] Fracture toughness measurement of a micro-sized single crystal silicon
    Koyama, S
    Takashima, K
    Higo, Y
    ADVANCES IN FRACTURE AND STRENGTH, PTS 1- 4, 2005, 297-300 : 292 - 295
  • [49] Influence of sub-micrometer notches on the fracture of single crystal silicon thin films
    Li, X.
    Kasai, T.
    Nakao, S.
    Ando, T.
    Shikida, M.
    Sato, K.
    FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2007, 30 (12) : 1172 - 1181
  • [50] Anisotropic etching rates of single-crystal silicon for TMAH water solution as a function of crystallographic orientation
    Sato, K
    Shikida, M
    Yamashiro, T
    Asaumi, K
    Iriye, Y
    Yamamoto, M
    SENSORS AND ACTUATORS A-PHYSICAL, 1999, 73 (1-2) : 131 - 137