Influence of friction stir welding conditions on joinability of oxide dispersion strengthened steel / F82H ferritic/martensitic steel joint

被引:7
作者
Serizawa, Hisashi [1 ]
Murakami, Masakazu [2 ]
Morisada, Yoshiaki [1 ]
Fujii, Hidetoshi [1 ]
Nogami, Shuhei [3 ]
Nagasaka, Takuya [4 ]
Tanigawa, Hiroyasu [5 ]
机构
[1] Osaka Univ, Joining & Welding Res Inst, 11-1 Mihogaoka, Ibaraki, Osaka 5670047, Japan
[2] Osaka Univ, Grad Sch Engn, 2-1 Yamadaoka, Suita, Osaka 5650871, Japan
[3] Tohoku Univ, Grad Sch Engn, 6-6-01-2 Aobayama, Sendai, Miyagi 9808579, Japan
[4] Natl Inst Fus Sci, Fus Syst Res Div, 322-6 Oroshi Cho, Toki, Gifu 5095292, Japan
[5] Japan Atom Energy Agcy, Fus Res & Dev Directorate, 2-166 Oaza Obuchi Aza Omotedate, Rokkasho, Aomori 0393212, Japan
关键词
Friction stir welding; Reduced activation metallic materials; Dissimilar joint; Backside plate; Joinability; MECHANICAL-PROPERTIES; FERRITIC STEEL; MICROSTRUCTURE;
D O I
10.1016/j.nme.2016.09.018
中图分类号
TL [原子能技术]; O571 [原子核物理学];
学科分类号
0827 ; 082701 ;
摘要
As one of the joining methods for the reduced activation materials to realize the fusion reactors with high efficiency in the future, friction stir welding (FSW) is selected for fabricating the dissimilar butt joint between oxide-dispersion strengthened (ODS) alloy and F82H, and the effect of FSW conditions on joinability of this dissimilar joint was examined. The sound dissimilar joint can be produced under the condition that ODS plate is set on the advancing side and the FSW tool is plunged into F82H. As for the mild steel backside plate, the sound joint can be fabricated in the case of 150 rpm rotational speed and 50 mm/min traveling speed. On the other hand, by employing the silicon nitride backside plate, the total heat input should be decreased to obtain the sound joint, where the traveling speed is 100 or 150 mm/min and rotational speed is 150 rpm. In addition, the finite element heat conduction analyses indicate that the influence of traveling speed on the joinability with the mild steel backside plate seems to be smaller than that with the silicon nitride plate and the allowable range of the appropriate traveling speed for the joint becomes to be wider by employing the silicon nitride backside plate. (C) 2016 The Authors. Published by Elsevier Ltd.
引用
收藏
页码:367 / 371
页数:5
相关论文
共 44 条
[41]   The occurrence of deformation induced ferrite transition (DIFT) during back heating assisted friction stir welding pipeline steel: The influence on the toughness of welded joint [J].
Cui, H. B. ;
Lu, Y. ;
Wang, C. X. ;
Tang, X. ;
Liu, Z. G. ;
Misra, R. D. K. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2022, 836
[42]   Investigation of instability of M23C6 particles in F82H steel under electron and ion irradiation conditions [J].
Kano, Sho ;
Yang, Huilong ;
Shen, Jingjie ;
Zhao, Zishou ;
McGrady, John ;
Hamaguchi, Dai ;
Ando, Mamami ;
Tanigawa, Hiroyasu ;
Abe, Hiroaki .
JOURNAL OF NUCLEAR MATERIALS, 2018, 502 :263-269
[43]   Influence of Preheating Source on Mechanical Properties and Welding Residual Stress Characteristics in Ultra Thin Ferritic Stainless Steel Hybrid Friction Stir Welded Joints [J].
Kim, Kyoung-Hak ;
Bang, Han-Sur ;
Ro, Chan-Seung ;
Bang, Hee-Seon .
INTERNATIONAL JOURNAL OF PRECISION ENGINEERING AND MANUFACTURING-GREEN TECHNOLOGY, 2017, 4 (04) :393-400
[44]   Ambient, elevated temperature tensile properties and origin of strengthening in friction stir welded 6 mm thick reduced activation ferritic-martensitic steel plates in as-welded and post-weld normalised conditions [J].
Varghese, Johny ;
Rajulapati, Koteswararao V. ;
Rao, K. Bhanu Sankara ;
Meshram, S. D. ;
Reddy, G. Madhusudhan .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2022, 857