Low cycle fatigue behavior in an orthogonal three-dimensional woven Tyranno fiber reinforced Si-Ti-C-O matrix composite

被引:11
作者
Zhu, SJ
Kaneko, Y
Ochi, Y
Ogasawara, T
Ishikawa, T
机构
[1] Univ Tokyo, Inst Ind Sci, Meguro Ku, Tokyo 1538505, Japan
[2] Univ Electrocommun, Chofu, Tokyo 1828585, Japan
[3] Japan Aerosp Explorat Agcy, Mitaka, Tokyo 1810015, Japan
关键词
ceramic matrix composite; SiC fiber; low cycle fatigue; damage; sliding stress of interface;
D O I
10.1016/j.ijfatigue.2004.03.001
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
The low cycle fatigue tests of an orthogonal three-dimensional (3-D) Tyranno fiber reinforced Si-Ti-C-O (SiC) matrix composites were conducted with a sine wave form under stress and strain controls at room temperature. It was shown that the asymmetric response of strain or stress occurs between tension and compression. There is no stress ratio (R) effect on fatigue life between R = 0. 1 and -1 at 0.02 Hz. The reduction Of Young's modulus and sliding stress of interface during fatigue was analyzed to interpret experimental results. (C) 2004 Elsevier Ltd. All rights reserved.
引用
收藏
页码:1069 / 1074
页数:6
相关论文
共 21 条
[1]   THEORY OF MECHANICAL-PROPERTIES OF CERAMIC-MATRIX COMPOSITES [J].
CURTIN, WA .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1991, 74 (11) :2837-2845
[2]   Fibre and interfacial properties measured in situ for a 3D woven SiC/SiC-based composite with glass sealant [J].
Davies, IJ ;
Ishikawa, T ;
Shibuya, M ;
Hirokawa, T ;
Gotoh, J .
COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING, 1999, 30 (04) :587-591
[3]   RELATIONSHIPS BETWEEN HYSTERESIS MEASUREMENTS AND THE CONSTITUENT PROPERTIES OF CERAMIC-MATRIX COMPOSITES .2. EXPERIMENTAL STUDIES ON UNIDIRECTIONAL MATERIALS [J].
DOMERGUE, JM ;
VAGAGGINI, E ;
EVANS, AG .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1995, 78 (10) :2721-2731
[4]   STRENGTH DISTRIBUTION OF REINFORCING FIBERS IN A NICALON FIBER CHEMICALLY VAPOR INFILTRATED SILICON-CARBIDE MATRIX COMPOSITE [J].
ECKEL, AJ ;
BRADT, RC .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1989, 72 (03) :455-458
[5]   OVERVIEW NO-118 - FATIGUE OF CERAMIC-MATRIX COMPOSITES [J].
EVANS, AG ;
ZOK, FW ;
MCMEEKING, RM .
ACTA METALLURGICA ET MATERIALIA, 1995, 43 (03) :859-875
[6]  
FOHEY WR, 1995, CERAM ENG SCI P, V16, P459
[7]   FREQUENCY-DEPENDENCE OF FATIGUE LIFE AND INTERNAL HEATING OF A FIBER-REINFORCED CERAMIC-MATRIX COMPOSITE [J].
HOLMES, JW ;
WU, X ;
SORENSEN, BF .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1994, 77 (12) :3284-3286
[8]  
Hoshide T., 1994, Journal of the Society of Materials Science, Japan, V43, P902, DOI 10.2472/jsms.43.902
[9]   Experimental stress/strain behavior of SiC-matrix composites reinforced with Si-Ti-C-O fibers and estimation of matrix elastic modulus [J].
Ishikawa, T ;
Bansaku, K ;
Watanabe, N ;
Nomura, Y ;
Shibuya, M ;
Hirokawa, T .
COMPOSITES SCIENCE AND TECHNOLOGY, 1998, 58 (01) :51-63
[10]  
Kaneko Y, 2001, CERAM ENG SCI PROC, V22, P553