Alkali-silica reaction mitigation: State of the art and recommendations

被引:0
|
作者
Malvar, LJ [1 ]
Cline, GD
Burke, DF
Rollings, R
Sherman, TW
Greene, JL
机构
[1] USN, Naval Facil Engn Command, Washington, DC 20350 USA
[2] USA, Corps Engineers, TSMCX, Washington, DC 20310 USA
[3] USAF, Civil Engineer Support Agcy, Washington, DC 20330 USA
关键词
alkali-silica reaction; concrete; fly ash; silica fume; slag;
D O I
暂无
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
Alkali-silica reaction (ASR) mitigation techniques from various states in the United States, and from various countries and international organizations, were assessed and summarized. A set of recommended mitigation procedures was developed that requires not only the use of low-alkali cement, but replacement of part of it by Class F fly ash (or Class N pozzolan) (25 to 40% by weight), or ground granulated blast-furnace slag (GGBFS), Grade 100 or 120 (40 to 50% by weight), or a combination of both. The Class F fly ash (or Class, N pozzolan) should also have a maximum of 1.5% available alkali, a maximum 6% loss on ignition, and a maximum of 8% CaO (lime). A modified ASTM C 1260 using the actual mixture is recommended for ASR testing. In addition to mitigating ASR, these recommendations are expected to: 1) reduced concrete costs; 2) enhance the durability of concrete; 3) increase fly ash and GGBFS recycling; and 4) support the 1997 Kyoto protocol by significantly reducing CO2 production. If 25% of all cement was to be replaced, total savings to the United States economy could be in excess of $1 billion every year.
引用
收藏
页码:480 / 489
页数:10
相关论文
共 50 条
  • [2] Mitigation of Alkali-Silica Reaction by Hydrated Alumina
    Szeles, Tiffany
    Wright, Jared
    Rajabipour, Farshad
    Stoffels, Shelley
    TRANSPORTATION RESEARCH RECORD, 2017, (2629) : 15 - 23
  • [3] Mitigation of alkali-silica reaction in US highway concrete
    Folliard, Kevin J.
    Thomas, Michael D. A.
    Fournier, Benoit
    Drimalas, Thano
    Ahlstrom, Gina
    PROCEEDINGS OF THE INSTITUTION OF CIVIL ENGINEERS-CONSTRUCTION MATERIALS, 2016, 169 (04) : 215 - 222
  • [4] Novel admixtures for mitigation of alkali-silica reaction in concrete
    Kaladharan, Gopakumar
    Szeles, Tiffany
    Stoffels, Shelley M.
    Rajabipour, Farshad
    CEMENT & CONCRETE COMPOSITES, 2021, 120
  • [5] Alkali-silica reaction in concrete: Mechanisms, mitigation and test methods
    Figueira, R. B.
    Sousa, R.
    Coelho, L.
    Azenha, M.
    de Almeida, J. M.
    Jorge, P. A. S.
    Silva, C. J. R.
    CONSTRUCTION AND BUILDING MATERIALS, 2019, 222 : 903 - 931
  • [6] Mitigation Effect of Waste Rubber Powder and Silica Fume on Alkali-Silica Reaction
    Gao P.
    Wang Y.
    Xue G.
    Qin Y.
    Gu Y.
    Jianzhu Cailiao Xuebao/Journal of Building Materials, 2023, 26 (04): : 429 - 436
  • [7] Effect of Internal Curing as Mitigation to Minimize Alkali-Silica Reaction Damage
    Beyene, Mengesha A.
    Munoz, Jose F.
    Meininger, Richard C.
    Di Bella, Carmelo
    ACI MATERIALS JOURNAL, 2017, 114 (03) : 417 - 428
  • [8] A mechanistic study on mitigation of alkali-silica reaction by fine lightweight aggregates
    Li, Chang
    Thomas, Michael D. A.
    Ideker, Jason H.
    CEMENT AND CONCRETE RESEARCH, 2018, 104 : 13 - 24
  • [9] Evaluating the Use of Alkali-Silica Reaction Mitigation as a Metric for Assessing Pozzolanicity
    Benkeser, Daniel
    Kurtis, Kimberly
    ADVANCES IN CIVIL ENGINEERING MATERIALS, 2022, 11 (02): : 539 - 554
  • [10] Twenty-year field evaluation of alkali-silica reaction mitigation
    NSERC/Cement Association of Canada, Department of Civil Engineering, University of Toronto, Toronto, ON, Canada
    不详
    不详
    ACI Mater J, 2013, 5 (539-548):