Overview of accelerated aging and polymer degradation kinetics for combined radiation-thermal environments

被引:84
作者
Celina, Mathew [1 ]
Linde, Erik [1 ]
Brunson, Douglas [1 ]
Quintana, Adam [1 ]
Giron, Nicholas [1 ]
机构
[1] Sandia Natl Labs, Organ Mat Sci Dept 1853, POB 5800,MS 1411, Albuquerque, NM 87185 USA
关键词
Accelerated polymer aging; Radiation-thermal oxidative degradation; Predictive kinetic models; Aging model evaluation; Cable insulation performance under combined environments; MECHANICAL PROPERTY CHANGES; LIMITED OXIDATION PROFILES; NON-ARRHENIUS BEHAVIOR; LOW-DOSE RATE; TIME DEVELOPMENT; TEMPERATURE; DIFFUSION; POLYETHYLENE; CHEMORHEOLOGY; RUBBER;
D O I
10.1016/j.polymdegradstab.2019.06.007
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
Polymer aging under combined radiation-thermal oxidative conditions is intrinsically more convoluted than traditional thermal degradation. Accelerated aging methods for predictive purposes have to include thermal as well as radiative degradation pathways that initially may be regarded as independent parallel processes without additional synergism. Material aging is therefore represented as the sum of a thermal and radiative contribution. Data from accelerated aging may be available as dose to equivalent damage (DED) or degradation rates, yet they require different analytical approaches to yield the underlying temperature dependence and its activation energy. Further, kinetic models that embrace combined pathways can offer guidance for extrapolation of accelerated to ambient conditions, enabling the prediction of material aging behavior or remaining performance margins for requalification purposes. The existing theoretical approaches, their implications and an alternative option for globally fitting experimental data sets to kinetic aging models for combined environments are reviewed. This overview offers a pragmatic approach towards an expanded interpretation of oxidation rate and aging data properties for combined environments, all the way to time-dependence for rates and synergistic contributions. Further evidence is provided that for some material behaviors an additional E-a for the radiative term under high dose rate conditions could be beneficial, as similarly expressed by increases in a synergistic interaction parameter. Improved kinetic aging models are derived and applied to a comprehensive set of experimental oxidation rates for a chlorosulfonated polyethylene material. Emphasized is also the issue that initial oxidation rates versus superposition of oxidation levels (integrated rates) may result in slightly different thermal E-a values through added time dependency. Constant oxidation rates relate to an exponential decay in elongation at break data. Aging predictions can be improved through measured oxidation rates, a systematic understanding of material behavior over a large dose rate - temperature regime, and application of an appropriate aging model. The most general aging model will contain a radiative E-a, time-dependence of rate, and added synergism that may grow with temperature. (C) 2019 Elsevier Ltd. All rights reserved.
引用
收藏
页码:353 / 378
页数:26
相关论文
共 71 条
[1]  
[Anonymous], 2000, IAEATECDOC1188, VI
[2]   Use of a respirometer to measure oxidation rates of polymeric materials at ambient temperatures [J].
Assink, RA ;
Celina, M ;
Skutnik, JM ;
Harris, DJ .
POLYMER, 2005, 46 (25) :11648-11654
[3]  
Audouin L., 2012, POLYMERES AMBIANCE N
[4]   Nylon 6.6 accelerated aging studies: thermal-oxidative degradation and its interaction with hydrolysis [J].
Bernstein, R ;
Derzon, DK ;
Gillen, KT .
POLYMER DEGRADATION AND STABILITY, 2005, 88 (03) :480-488
[5]  
Burnay S. G., 2001, AGEING STUDIES LIFE
[6]  
BURNAY SG, 1991, ACS SYM SER, V475, P524
[7]   CHARACTERIZATION AND DEGRADATION STUDIES OF PEROXIDE AND SILANE CROSS-LINKED POLYETHYLENE [J].
CELINA, M ;
GEORGE, GA .
POLYMER DEGRADATION AND STABILITY, 1995, 48 (02) :297-312
[8]   Oxidation profiles of thermally aged nitrile rubber [J].
Celina, M ;
Wise, J ;
Ottesen, DK ;
Gillen, KT ;
Clough, RL .
POLYMER DEGRADATION AND STABILITY, 1998, 60 (2-3) :493-504
[9]   Correlation of chemical and mechanical property changes during oxidative degradation of neoprene [J].
Celina, M ;
Wise, J ;
Ottesen, DK ;
Gillen, KT ;
Clough, RL .
POLYMER DEGRADATION AND STABILITY, 2000, 68 (02) :171-184
[10]   Anomalous aging phenomena in a crosslinked polyolefin cable insulation [J].
Celina, M ;
Gillen, KT ;
Wise, J ;
Clough, RL .
RADIATION PHYSICS AND CHEMISTRY, 1996, 48 (05) :613-626