Influence of thermo-mechanical cycling on porcelain bonding to cobalt-chromium and titanium dental alloys fabricated by casting, milling, and selective laser melting

被引:38
作者
Antanasova, Maja [1 ]
Kocjan, Andraz [2 ]
Kovac, Janez [3 ]
Zuzek, Borut [4 ]
Jevnikar, Peter [1 ]
机构
[1] Univ Ljubljana, Fac Med, Dept Prosthodont, Hrvatski Trg 6, SI-1000 Ljubljana, Slovenia
[2] Jozef Stefan Inst, Dept Nanostruct Mat, Ljubljana, Slovenia
[3] Jozef Stefan Inst, Dept Surface Engn & Optoelect, Ljubljana, Slovenia
[4] Inst Met & Technol, Ljubljana, Slovenia
关键词
Metal-ceramic; Bond strength; CAD/CAM; Selective laser melting; Titanium; COMMERCIALLY PURE TITANIUM; METAL-CERAMIC RESTORATIONS; PRESSED COCRMO ALLOY; BIOMEDICAL APPLICATIONS; MECHANICAL-PROPERTIES; CORROSION-RESISTANCE; FATIGUE PERFORMANCE; SURFACE-ROUGHNESS; FLEXURAL STRENGTH; FRACTURE STRENGTH;
D O I
10.1016/j.jpor.2017.08.007
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Purpose: The aim has been to determine the effect of thermo-mechanical cycling on shear-bond-strength (SBS) of dental porcelain to Co-Cr and Ti-based alloys fabricated by casting, computer-numerical-controlled milling, and selective-laser-melting (SLM). Methods: Seven groups (n = 22/group) of metal cylinders were fabricated by casting (Co-Cr and commercially pure-cpTi), milling (Co-Cr, cpTi, Ti-6Al-4V) or by SLM (Co-Cr and Ti-6Al-4V) and abraded with airborne-particles. The average surface roughness (R-a) was determined for each group. Dental porcelain was applied and each metal-ceramic combination was divided into two subgroups - stored in deionized water (24-h, 37 degrees C), or subjected to both thermal (6000-cycles, between 5 and 60 degrees C) and mechanical cycling (10(5)-cycles, 60 N-load). SBS test-values and failure modes were recorded. Metal-ceramic interfaces were analyzed with a focused-ion-beam/scanning-electron-microscope (FIB/SEM) and energy-dispersive-spectroscopy (EDS). The elastic properties of the respective metal and ceramic materials were evaluated by instrumented-indentation-testing. The oxide thickness on intact Ti-based substrates was measured with Auger-electron-spectroscopy (AES). Data were analyzed using ANOVA, Tukey's HSD and t-tests (alpha = 0.05). Results: The SBS-means differed according to the metal-ceramic combination (p < 0.0005) and to the fatigue conditions (p < 0.0005). The failure modes and interface analyses suggest better porcelain adherence to Co-Cr than to Ti-based alloys. Values of R-a were dependent on the metal substrate (p < 0.0005). Ti-based substrates were not covered with thick oxide layers following digital fabrication. Conclusions: Ti-based alloys are more susceptible than Co-Cr to reduction of porcelain bond strength following thermo-mechanical cycling. The porcelain bond strength to Ti-based alloys is affected by the applied metal processing technology. (c) 2017 Japan Prosthodontic Society. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:184 / 194
页数:11
相关论文
共 73 条
[1]   OXIDE ADHERENCE AND PORCELAIN BONDING TO TITANIUM AND TI-6A1-4V ALLOY [J].
ADACHI, M ;
MACKERT, JR ;
PARRY, EE ;
FAIRHURST, CW .
JOURNAL OF DENTAL RESEARCH, 1990, 69 (06) :1230-1235
[2]   Comparison of the bond strength of laser-sintered and cast base metal dental alloys to porcelain [J].
Akova, Tolga ;
Ucar, Yurdanur ;
Tukay, Alper ;
Balkaya, Mehmet Cudi ;
Brantley, William A. .
DENTAL MATERIALS, 2008, 24 (10) :1400-1404
[3]   Metallurgical and interfacial characterization of PFM Co-Cr dental alloys fabricated via casting, milling or selective laser melting [J].
Al Jabbari, Y. S. ;
Koutsoukis, T. ;
Barmpagadaki, X. ;
Zinelis, S. .
DENTAL MATERIALS, 2014, 30 (04) :E79-E88
[4]   Advancements in CAD/CAM technology: Options for practical implementation [J].
Alghazzawi, Tariq F. .
JOURNAL OF PROSTHODONTIC RESEARCH, 2016, 60 (02) :72-84
[5]  
[Anonymous], 2002, 1457712002 DIN EN IS
[6]  
Antanasova M., 2016, Curr. Oral Health Rep, V3, P234, DOI [10.1007/s40496-016-0107-x, DOI 10.1007/S40496-016-0107-X, DOI 10.1007/S40496]
[7]   Fatigue testing of biomaterials and their interfaces [J].
Arola, Dwayne .
DENTAL MATERIALS, 2017, 33 (04) :367-381
[8]   Bond strength of three porcelains to two forms of titanium using two firing atmospheres [J].
Atsü, S ;
Berksun, S .
JOURNAL OF PROSTHETIC DENTISTRY, 2000, 84 (05) :567-574
[9]  
Bae EJ, 2014, J ADV PROSTHODONT, V6, P266
[10]   HEAT TREATMENT OF TI-6AL-4V PRODUCED BY LASERCUSING [J].
Becker, T. ;
van Rooyen, M. ;
Dimitrov, D. .
SOUTH AFRICAN JOURNAL OF INDUSTRIAL ENGINEERING, 2015, 26 (02) :93-103