The Effect of SiCp Addition on Corrosion and Wear Behavior of Conventionally and Microwave Sintered PM 316L

被引:7
作者
Ertugrul, Onur [1 ]
Willert-Porada, Monika [2 ]
Onel, Kazim [3 ]
机构
[1] Izmir Katip Celebi Univ, Dept Mat Sci & Engn, TR-35620 Izmir, Turkey
[2] Univ Bayreuth, Chair Mat Proc, D-95440 Bayreuth, Germany
[3] Dokuz Eylul Univ, Dept Met & Mat Engn, TR-35370 Izmir, Turkey
关键词
STEEL MATRIX COMPOSITES; AUSTENITIC STAINLESS-STEEL; PARTICLES; MICROSTRUCTURE; FRICTION; AL2O3;
D O I
10.1002/adem.201600680
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In this study, corrosion and wear behaviors of PM 316L matrix composite materials reinforced with SiC particles in amounts of 10 vol% are evaluated. The samples are uniaxially cold pressed, and then sintered by two different methods, conventional sintering and microwave sintering. Corrosion properties are evaluated by both immersion and cyclic polarization tests. Wear properties are evaluated by dry sliding wear tests. Brinell and Vickers microhardness tests are applied, in order to support the wear test results. The results show that 10 vol% SiCp reinforced composite samples have acceptable corrosion properties and improved wear resistence in a similar manner, as they show good mechanical properties. In addition, microwave sintering results in better wear properties compared to conventional method.
引用
收藏
页数:6
相关论文
共 22 条
[1]   Reinforcing 316L stainless steel with intermetallic and carbide particles [J].
Abenojar, J ;
Velasco, F ;
Torralba, JM ;
Bas, JA ;
Calero, JA ;
Marcè, R .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2002, 335 (1-2) :1-5
[2]  
Altinkok N, 2013, ACTA PHYS POL A, V124, P11
[3]   Pressure and sintering temperature influence on the interface reaction of SiCp/410L stainless steel composites [J].
Carvalho, O. ;
Madeira, S. ;
Buciumeanu, M. ;
Soares, D. ;
Silva, F. S. ;
Miranda, G. .
JOURNAL OF COMPOSITE MATERIALS, 2016, 50 (15) :2005-2015
[4]   Structure and properties of SiC and emery powder reinforced PM 316l matrix composites produced by microwave and conventional sintering [J].
Ertugrul, O. ;
Park, H. -S. ;
Onel, K. ;
Willert-Porada, M. .
POWDER METALLURGY, 2015, 58 (01) :41-50
[5]   Effect of particle size and heating rate in microwave sintering of 316L stainless steel [J].
Ertugrul, O. ;
Park, H. -S. ;
Onel, K. ;
Willert-Porada, M. .
POWDER TECHNOLOGY, 2014, 253 :703-709
[6]   Effect of sintering cooling rate on corrosion resistance of powder metallurgy austenitic, ferritic and duplex stainless steels sintered in nitrogen [J].
Garcia, C. ;
Martin, F. ;
Blanco, Y. .
CORROSION SCIENCE, 2012, 61 :45-52
[7]   Corrosion behaviour of duplex stainless steels sintered in nitrogen [J].
Garcia, C. ;
Martin, F. ;
Blanco, Y. ;
de Tiedra, M. P. ;
Aparicio, M. L. .
CORROSION SCIENCE, 2009, 51 (01) :76-86
[8]  
Gradzka-Dahlke M., 2007, WEAR, V263, P7
[9]   Friction and wear behavior of SUS 304 austenitic stainless steel against Al2O3 ceramic ball under relative high load [J].
Hua, Meng ;
Wei, Xicheng ;
Li, Jian .
WEAR, 2008, 265 (5-6) :799-810
[10]  
Klar E., 2007, POWDER METALLURGY ST, P5