Transition of solidification path in nonequilibrium solidification of Ti-48Al-8Nb alloy

被引:0
作者
He, Tan [1 ]
Hu, Rui [1 ]
Yang, Jie-Ren [1 ]
Zhang, Tie-Bang [1 ]
Li, Jin-Shan [1 ]
机构
[1] Northwestern Polytech Univ, Sch Mat Sci & Engn, State Key Lab Solidificat Proc, Xian 710072, Peoples R China
关键词
TiAl alloy; Undercooling; Nonequilibrium solidification; Microstructure evolution; HIGH NB; TI-46AL-8NB ALLOY; TIAL ALLOYS; MICROSTRUCTURE; BEHAVIOR; PHASE; MELTS; REFINEMENT; ADDITIONS;
D O I
10.1007/s12598-015-0630-2
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The solidification behavior of Ti-48Al-8Nb alloy under nonequilibrium solidification conditions was studied by electromagnetic levitation technique. The solidification conditions are different undercooling (Delta T) under the same cooling condition and different cooling methods at the same undercooling condition, respectively. In different undercooling conditions, when the undercooling is above a critical value (Delta T* a parts per thousand 211 K), a remarkable morphological transition from typical hypoperitectic solidification to a sole solidification of the beta phase resulting in the suppression of the peritectic reaction occurs. For melts with different cooling conditions at the same undercooling (Delta T a parts per thousand 85 K), the melt was rapidly cooled by quenching them in cooling media. With cooling rate increasing, a transition from beta phase to peritectic alpha phase solidification mode is revealed for Ti-48Al-8Nb alloy.
引用
收藏
页码:48 / 53
页数:6
相关论文
共 25 条
  • [1] Appel F., 2003, Titanium and Titanium Alloys, P89, DOI DOI 10.1002/3527602119.CH4
  • [2] Creep behaviour and related high temperature microstructural stability of Ti-46Al-9Nb sheet material
    Bystrzanowski, S
    Bartels, A
    Clemens, H
    Gerling, R
    Schimansky, FP
    Dehm, G
    Kestler, H
    [J]. INTERMETALLICS, 2005, 13 (05) : 515 - 524
  • [3] Micro segregation in high Nb containing TiAl alloy ingots beyond laboratory scale
    Chen, G. L.
    Xu, X. J.
    Teng, Z. K.
    Wang, Y. L.
    Lin, J. P.
    [J]. INTERMETALLICS, 2007, 15 (5-6) : 625 - 631
  • [4] Suppression of peritectic reaction in the undercooled peritectic Fe-Ni melts
    Chen, Y. Z.
    Liu, F.
    Yang, G. C.
    Liu, N.
    Yang, C. L.
    Zhou, Y. H.
    [J]. SCRIPTA MATERIALIA, 2007, 57 (08) : 779 - 782
  • [5] Design, Processing, Microstructure, Properties, and Applications of Advanced Intermetallic TiAl Alloys
    Clemens, Helmut
    Mayer, Svea
    [J]. ADVANCED ENGINEERING MATERIALS, 2013, 15 (04) : 191 - 215
  • [6] Microstructure development during directional solidification of Ti-45Al-8Nb alloy
    Ding, X. F.
    Lin, J. P.
    Zhang, L. Q.
    Wang, H. L.
    Hao, G. J.
    Chen, G. L.
    [J]. JOURNAL OF ALLOYS AND COMPOUNDS, 2010, 506 (01) : 115 - 119
  • [7] Grain refinement by low boron additions in niobium-rich TiAl-based alloys
    Hecht, U.
    Witusiewicz, V.
    Drevermann, A.
    Zollinger, J.
    [J]. INTERMETALLICS, 2008, 16 (08) : 969 - 978
  • [8] THE EFFECTS OF CR ADDITIONS TO BINARY TIAL-BASE ALLOYS
    HUANG, SC
    HALL, EL
    [J]. METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1991, 22 (11): : 2619 - 2627
  • [9] Huang SC, US Patent, Patent No. 4879092
  • [10] Microstructural control of TiAl-Mo-B alloys by directional solidification
    Johnson, DR
    Chihara, K
    Inui, H
    Yamaguchi, M
    [J]. ACTA MATERIALIA, 1998, 46 (18) : 6529 - 6540