Effects of heat treatment on microstructure and microhardness of linear friction welded dissimilar Ti alloys

被引:25
作者
Zhang, Chuan-chen [1 ,2 ]
Zhang, Tian-cang [1 ]
Ji, Ya-juan [1 ]
Huang, Ji-hua [2 ]
机构
[1] AVIC Beijing Aeronaut Mfg Technol Res Inst, Beijing 100024, Peoples R China
[2] Univ Sci & Technol Beijing, Sch Mat Sci & Engn, Beijing 100083, Peoples R China
关键词
linear friction welding; Ti alloys; heat treatments; microstructure; microhardness; TI-6AL-4V; EVOLUTION;
D O I
10.1016/S1003-6326(13)62898-8
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
A detailed investigation for the influence of post weld heat treatment (PWHT) on the microstructure of TC4 and TC17 dissimilar joints was analyzed. The fully transformed microstructure in the as-welded zone indicated that the peak temperature exceeded the beta-transus temperature at the weld interface during linear friction welding. TC4 side was mainly composed of martensite alpha' phase with random distribution and it was single beta for that of TC17. In the thermomechanically affected zones of TC4 and TC17, the structure undergoes severe plastic deformation and re-orientation, yet without altering the phase fractions. After PWHT, in the weld zone of TC4 alloy, the phase transformation alpha'-> alpha+beta occurred and the acicular alpha was coarsened, which resulted in a decrease in hardness. In the weld zone of TC17 alloy, fine alpha phase precipitated at the grain boundary and within beta grains, which resulted in a sharp increase in hardness.
引用
收藏
页码:3540 / 3544
页数:5
相关论文
共 16 条
  • [1] Solid state joining of metals by linear friction welding: a literature review
    Bhamji, I.
    Preuss, M.
    Threadgill, P. L.
    Addison, A. C.
    [J]. MATERIALS SCIENCE AND TECHNOLOGY, 2011, 27 (01) : 2 - 12
  • [2] Measurement of strain in a titanium linear friction weld by neutron diffraction
    Daymond, MR
    Bonner, NW
    [J]. PHYSICA B-CONDENSED MATTER, 2003, 325 (1-4) : 130 - 137
  • [3] Texture development in Ti-6Al-4V linear friction welds
    Karadge, M.
    Preuss, M.
    Lovell, C.
    Withers, P. J.
    Bray, S.
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2007, 459 (1-2): : 182 - 191
  • [4] Microstructural evolution of a TC11 titanium alloy during linear friction welding
    Lang, B.
    Zhang, T. C.
    Li, X. H.
    Guo, D. L.
    [J]. JOURNAL OF MATERIALS SCIENCE, 2010, 45 (22) : 6218 - 6224
  • [5] Influence of Parent Metal Microstructure and Post-Weld Heat Treatment on Microstructure and Mechanical Properties of Linear Friction Welded Ti-6Al-4V Joint
    Li, Wenya
    Wu, Hui
    Ma, Tiejun
    Yang, Changlin
    Chen, Zhongwei
    [J]. ADVANCED ENGINEERING MATERIALS, 2012, 14 (05) : 312 - 318
  • [6] Effect of post-weld heat treatment on microstructure and property of linear friction welded Ti17 titanium alloy joint
    Ma, T. J.
    Li, W. Y.
    Zhong, B.
    Zhang, Y.
    Li, J. L.
    [J]. SCIENCE AND TECHNOLOGY OF WELDING AND JOINING, 2012, 17 (03) : 180 - 185
  • [7] Impact toughness and fracture analysis of linear friction welded Ti-6Al-4V alloy joints
    Ma, T. J.
    Li, W. -Y.
    Yang, S. Y.
    [J]. MATERIALS & DESIGN, 2009, 30 (06) : 2128 - 2132
  • [8] Microstructure evolution and mechanical properties of linear friction welded 45 steel joint
    Ma, Tiejun
    Li, Wen-Ya
    Xu, Quanzhou
    Zhang, Yong
    Li, Jinglong
    Yang, Siqian
    Liao, Hanlin
    [J]. ADVANCED ENGINEERING MATERIALS, 2007, 9 (08) : 703 - 707
  • [9] Formation mechanism of linear friction welded Ti-6Al-4V alloy joint based on microstructure observation
    Ma, Tiejun
    Chen, Tao
    Li, Wen-Ya
    Wang, Shiwei
    Yang, Siqian
    [J]. MATERIALS CHARACTERIZATION, 2011, 62 (01) : 130 - 135
  • [10] Linear Friction Welding of IN-718 Process Optimization and Microstructure Evolution
    Mary, C.
    Jahazi, M.
    [J]. THERMEC 2006 SUPPLEMENT: 5TH INTERNATIONAL CONFERENCE ON PROCESSING AND MANUFACTURING OF ADVANCED MATERIALS, 2007, 15-17 : 357 - 362