Oxidation resistance of silicon carbide whisker reinforced sialon composites

被引:0
作者
Sashida, N [1 ]
Tsukamoto, K [1 ]
Inoue, Y [1 ]
Yamagishi, C [1 ]
机构
[1] Nihon Cement Co Ltd, Cent Res Inst, New Mat Div, Koto Ku, Tokyo 1358410, Japan
来源
SCIENCE OF ENGINEERING CERAMICS II | 1999年 / 2卷
关键词
sialon; composite; SiC whisker; oxidation resistance; strength;
D O I
10.4028/www.scientific.net/KEM.161-163.295
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Oxidation resistance of silicon carbide whisker (SiCw) reinforced and Y-Yb-Al-O as sintering aid contained sialon composites which were sintered with pressureless sintering and hot isostatic pressing were measured in air at 1473 or 1623K. By oxidation, high temperature strength of composites were slightly increased by oxidation comparing with monolithic whose strength after oxidation were less then before oxidation. From observation of 1623K oxidized specimen, the porous layer whose structure was generated by removing glass phase was under the surface oxidized layer. It is considered that this porous layer may act barrier to diffusion. The thickness of this layer was decreased by SiCw. We suggest that the mechanism of oxidation and effects of SiCw. It is considered that SiCw in the grain boundary of composites act a role of barrier to diffusion, then it leads the enhancement of oxidation resistance of composites like above.
引用
收藏
页码:295 / 298
页数:4
相关论文
共 50 条
[31]   Mechanical and tribological behaviour of nano scaled silicon carbide reinforced aluminium composites [J].
Faisal, Nadeem ;
Kumar, Kaushik .
JOURNAL OF EXPERIMENTAL NANOSCIENCE, 2018, 13 :S1-S13
[32]   Zirconia reinforced reaction bonded silicon carbide composites: Microstructure and mechanical properties [J].
Li, Shuang ;
Zhang, Yumin ;
Han, Jiecai ;
Zhou, Yufeng .
INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2012, 35 :257-261
[33]   Formation of silicon carbide nanowire coatings on C/C composites using an in situ catalytic strategy for improved oxidation resistance [J].
Jin, Min ;
Li, Zhuan ;
Li, Ye ;
Wu, Jiaqi ;
Gao, Zonglong ;
Zhao, Yibo ;
Li, Pengtao .
CERAMICS INTERNATIONAL, 2024, 50 (01) :909-919
[34]   SYNTHESIS OF WHISKER REINFORCED MULLITE MATRIX COMPOSITES USING COLLOIDAL PROCESSING [J].
HIRATA, Y ;
TAKESHIMA, K ;
ISHIHARA, Y .
NIPPON SERAMIKKUSU KYOKAI GAKUJUTSU RONBUNSHI-JOURNAL OF THE CERAMIC SOCIETY OF JAPAN, 1992, 100 (04) :353-361
[35]   Oxidation Resistance of Hafnium Diboride Ceramics with Additions of Silicon Carbide and Tungsten Boride or Tungsten Carbide [J].
Carney, Carmen M. ;
Parthasarathy, Triplicane A. ;
Cinibulk, Michael K. .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2011, 94 (08) :2600-2607
[36]   Load-dependent indentation behavior of β-SiAlON and α-silicon carbide [J].
Barick, Prasenjit ;
Jana, Dulal Chandra ;
Saha, Bhaskar Prasad .
JOURNAL OF ADVANCED CERAMICS, 2013, 2 (02) :185-192
[37]   Oxidation of Silicon Carbide Composites for Nuclear Applications at Very High Temperatures in Steam [J].
Steinbrueck, Martin ;
Grosse, Mirco ;
Stegmaier, Ulrike ;
Braun, James ;
Lorrette, Christophe .
COATINGS, 2022, 12 (07)
[38]   Mechanical properties and oxidation behavior of silicon carbide-molybdenum silicides composites [J].
Magnani, Giuseppe ;
Brentari, Alida ;
Burresi, Emiliano ;
Coglitore, Antonino .
CERAMICS INTERNATIONAL, 2013, 39 (03) :3345-3351
[39]   Effect of silicon carbide interlayers on the mechanical behavior of T800-HB-fiber-reinforced silicon carbide-matrix composites [J].
Xin-gui, Zhou ;
Hai-jiao, Yu ;
Bo-yun, Huang ;
Jian-gao, Yang ;
Ze-lan, Huang .
HIGH-PERFORMANCE CERAMICS V, PTS 1 AND 2, 2008, 368-372 :1844-+
[40]   Interface formation and oxidation behaviors of silicon-carbide-based layered composites [J].
Kato, M ;
Fukasawa, T ;
Goto, Y ;
Yonetsu, M ;
Suyama, S ;
Kameda, T .
SCIENCE OF ENGINEERING CERAMICS II, 1999, 2 :461-464