Nano-scratch testing of (Ti,Fe)Nx thin films on silicon

被引:46
作者
Beake, B. D. [1 ]
Vishnyakov, V. M. [2 ]
Harris, A. J. [1 ]
机构
[1] Micro Mat Ltd, Willow House,Ellice Way, Yale Business Village LL13 7Y1, Wrexham, Wales
[2] Univ Huddersfield, Mat Res Inst, Huddersfield HD1 3DH, W Yorkshire, England
关键词
Crack resistance; Protective coatings; Nano-scratch; Soft inclusions; H-3/E-2; DIAMOND-LIKE CARBON; MECHANICAL-PROPERTIES; NANOCOMPOSITE COATINGS; OXIDATION RESISTANCE; THERMAL-STABILITY; CUTTING TOOLS; HARD; WEAR; FRICTION; INDENTATION;
D O I
10.1016/j.surfcoat.2016.11.024
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Thin films of (Ti,Fe)N-x. have been produced on silicon wafers with a wide range of compositions and mechanical properties to investigate correlations between the mechanical properties measured by indentation and crack resistance in the highly loaded sliding contact in a nano-scratch test. The nano-scratch test data on the thin films using a well-worn Berkovich indenter with similar to 1 mu m end radius were supported by high resolution scanning electron microscopic (SEM) imaging and analytical stress modelling. The results show that mechanical properties of the coating, its thickness and the substrate properties all influence the deformation process. They affect the critical loads required, the type of failures observed and their location relative to the moving probe. The differences in coating mechanical properties affect how the interface is weakened (i.e. by initial substrate or coating yielding or both) and determine the deformation failure mechanism. The load dependence of the friction coefficient provides details of the sliding contact zone and the location of failure relative to the sliding probe. Improved performance was achieved at intermediate hardness and H-3/E-2 in the nano-scratch tests on thin films. The friction and modelling results strongly suggest that failure at low load on the hardest coatings is due to a combination of high tensile stress at the rear of the contact zone and substrate yield. Designing thin films for protective coatings with in-built dissipative structures (such as soft and low elastic modulus inclusions) and mechanisms to combat stress may be a more successful route to optimise their toughness in highly loaded sliding conditions than aiming to minimise plasticity by increasing their hardness. (C) 2016 Elsevier B.V. All rights reserved.
引用
收藏
页码:671 / 679
页数:9
相关论文
共 71 条
[1]  
[Anonymous], 2015, C162405 ASTM
[2]   Development of DLC coating architectures for demanding functional surface applications through nano- and micro-mechanical testing [J].
Beake, B. D. ;
Liskiewicz, T. W. ;
Vishnyakov, V. M. ;
Davies, M. I. .
SURFACE & COATINGS TECHNOLOGY, 2015, 284 :334-343
[3]   Nanoscratch and nanowear testing of TiN coatings on M42 steel [J].
Beake, B. D. ;
Shi, B. ;
Sullivan, J. L. .
TRIBOLOGY-MATERIALS SURFACES & INTERFACES, 2011, 5 (04) :141-147
[4]   Nano-impact testing of TiFeN and TiFeMoN films for dynamic toughness evaluation [J].
Beake, B. D. ;
Vishnyakov, V. M. ;
Colligon, J. S. .
JOURNAL OF PHYSICS D-APPLIED PHYSICS, 2011, 44 (08)
[5]   Relationship between mechanical properties of thin nitride-based films and their behaviour in nano-scratch tests [J].
Beake, B. D. ;
Vishnyakov, V. M. ;
Harris, A. J. .
TRIBOLOGY INTERNATIONAL, 2011, 44 (04) :468-475
[6]   Coating optimisation for high speed machining with advanced nanomechanical test methods [J].
Beake, B. D. ;
Fox-Rabinovich, G. S. ;
Veldhuis, S. C. ;
Goodes, S. R. .
SURFACE & COATINGS TECHNOLOGY, 2009, 203 (13) :1919-1925
[7]   Why can TiAlCrSiYN-based adaptive coatings deliver exceptional performance under extreme frictional conditions? [J].
Beake, Ben D. ;
Fox-Rabinovich, German S. ;
Losset, Yannick ;
Yamamoto, Kenji ;
Agguire, Myriam H. ;
Veldhuis, Stephen C. ;
Endrino, Jose L. ;
Kovalev, Anatoliy I. .
FARADAY DISCUSSIONS, 2012, 156 :267-277
[8]   INVESTIGATION OF THE ELECTRONIC-STRUCTURE OF AN IRON TITANIUM NITRIDE AMMONIA-SYNTHESIS CATALYST [J].
BIWER, BM ;
BERNASEK, SL .
APPLIED SURFACE SCIENCE, 1986, 25 (1-2) :41-52
[9]   Effect of microstructure on the erosion resistance of Cr-Si-N coatings [J].
Bousser, E. ;
Benkahoul, M. ;
Martinu, L. ;
Klemberg-Sapieha, J. E. .
SURFACE & COATINGS TECHNOLOGY, 2008, 203 (5-7) :776-780
[10]  
Bowden FP., 1986, FRICTION LUBRICATION, P374