Enhanced mechanical properties of 70/30 brass joint by rapid cooling friction stir welding

被引:68
作者
Xu, Nan [1 ]
Ueji, Rintaro [1 ]
Fujii, Hidetoshi [1 ]
机构
[1] Osaka Univ, Joining & Welding Res Inst, Ibaraki, Osaka 5670047, Japan
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2014年 / 610卷
基金
日本科学技术振兴机构;
关键词
70/30; Brass; Rapid cooling FSW; Microstructure; Texture; Mechanical properties; ALUMINUM-ALLOY; LIQUID CO2; GRAINED CU; COPPER; NANOSCALE; DUCTILITY; PLATES; STEEL;
D O I
10.1016/j.msea.2014.05.037
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The effect of rapid cooling on the microstructure, texture and mechanical properties of friction stir welded 70/30 brass was investigated. Liquid CO2 was used as the cooling medium during the process. Without the rapid cooling, the welded joint showed many micropores and Zn/Cu oxides in the stir zone accompanied by a relatively wide heat-affected zone. The stir zone showed relatively coarse grains with a mean diameter of 9.7 mu m and these grains had low dislocation density. The crystallographic texture whose dominant component of {1 0 0} (// shear plane) < 0 0 1 >(// shear direction) was also found. On the other hand, when the rapid cooling was carried out during the welding process, a sound joint with no obvious heat-affected zone was achieved. The stir zone showed the fine-grained structure whose mean grain size is 1.2 mu m with high dislocation density. The texture in the stir zone was completely different from that in the joint without the rapid cooling. These differences between the joints with and without the rapid cooling indicate the significant post-annealing effect, including both recovery and static recrystallization can be prohibited by the rapid cooling. As a result, enhanced yield strength with adequate ductility of the stir zone was obtained. (C) 2014 Elsevier B.V. All rights reserved.
引用
收藏
页码:132 / 138
页数:7
相关论文
共 29 条
[1]   Pulsed Nd:YAG laser welding of copper using oxygenated assist gases [J].
Biro, E ;
Weckman, DC ;
Zhou, Y .
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2002, 33 (07) :2019-2030
[2]   DIE DURCH PLASTIZITATSUNTERSUCHUNGEN BESTIMMTE STAPELFEHLERENERGIE VON SILBER IM TEMPERATURBEREICH 172-DEGREES-K BIS 873-DEGREES-K [J].
BUHLER, SE ;
LUCKE, K ;
ROSENBAUM, FW .
PHYSICA STATUS SOLIDI, 1963, 3 (05) :886-900
[3]   Texture development in friction stir welds [J].
Fonda, R. W. ;
Knipling, K. E. .
SCIENCE AND TECHNOLOGY OF WELDING AND JOINING, 2011, 16 (04) :288-294
[4]   Friction stir welding of AISI 1080 steel using liquid CO2 for enhanced toughness and ductility [J].
Fujii, H. ;
Chung, Y. D. ;
Sun, Y. F. .
SCIENCE AND TECHNOLOGY OF WELDING AND JOINING, 2013, 18 (06) :500-506
[5]  
Humphreys F. J., 2004, RECRYSTALLIZATION RE, V2
[6]   Experimental study on Friction Stir Welding of copper metals [J].
Hwang, Y. M. ;
Fan, P. L. ;
Lin, C. H. .
JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2010, 210 (12) :1667-1672
[7]   The joint properties of copper by friction stir welding [J].
Lee, WB ;
Jung, SB .
MATERIALS LETTERS, 2004, 58 (06) :1041-1046
[8]   Effect of tool rotation rate on microstructure and mechanical properties of friction stir welded copper [J].
Liu, H. J. ;
Shen, J. J. ;
Huang, Y. X. ;
Kuang, L. Y. ;
Liu, C. ;
Li, C. .
SCIENCE AND TECHNOLOGY OF WELDING AND JOINING, 2009, 14 (06) :577-583
[9]   Tensile properties and fracture locations of friction-stir-welded joints of 2017-T351 aluminum alloy [J].
Liu, HJ ;
Fujii, H ;
Maeda, M ;
Nogi, K .
JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2003, 142 (03) :692-696
[10]   Strengthening Materials by Engineering Coherent Internal Boundaries at the Nanoscale [J].
Lu, K. ;
Lu, L. ;
Suresh, S. .
SCIENCE, 2009, 324 (5925) :349-352