Kinetics and 13C NMR Study of Oxygen Incorporation into PVC- and Pitch-Derived Materials

被引:3
作者
Altoe, Gisele F. [1 ]
Freitas, Jair C. C. [1 ]
Cunha, Alfredo G. [1 ]
Emmerich, Francisco G. [1 ]
Smith, Mark E. [2 ]
机构
[1] Univ Fed Espirito Santo, Dept Fis, BR-29075910 Vitoria, ES, Brazil
[2] Univ Warwick, Dept Phys, Coventry CV4 7AL, W Midlands, England
关键词
COAL-TAR PITCH; OXIDATIVE STABILIZATION; MESOPHASE PITCH; CARBON MATERIALS; THERMAL-ANALYSIS; CARBONIZATION; PYROLYSIS; SPECTRA;
D O I
10.1021/ef8009926
中图分类号
TE [石油、天然气工业]; TK [能源与动力工程];
学科分类号
0807 ; 0820 ;
摘要
The kinetics of oxygen incorporation into a PVC-derived material with pitch-like characteristics was studied by isothermal thermogravimetric analysis at temperatures ranging from 200 to 270 degrees C. Activation energy, Ea, pre-exponential factor, A, and rate constants, k(T), were obtained from the weight-gain curves recorded during reactions of the material with molecular oxygen, which were analyzed following a kinetic first-order model. The numerical values obtained were E-a = 100.5 kJ/mol and A = 1.6 x 10(10) h(-1). The extent of the oxidation at a fixed temperature was monitored by elemental analysis, and the chemical changes in the materials were followed by solid-state C-13 NMR. The study was next extended to the chars obtained from three coal tar pitches with different softening points (55, 85, and I 10 degrees C). Comparisons were then established between the determined kinetic parameters and the chemical/structural aspects and compositions of each analyzed material.
引用
收藏
页码:1373 / 1378
页数:6
相关论文
共 23 条
  • [1] Solid state 13C NMR and high temperature 1H NMR determination of bulk structural properties for mesophase-containing semi-cokes prepared from coal tar pitch
    Andresen, JM
    Martin, Y
    Moinelo, SR
    Maroto-Valer, MM
    Snape, CE
    [J]. CARBON, 1998, 36 (7-8) : 1043 - 1050
  • [2] Investigation with 13C NMR, EPR and magnetic susceptibility measurements of char residues obtained by pyrolysis of biomass
    Bardet, Michel
    Hediger, Sabine
    Gerbaud, Guillaume
    Gambarelli, Serge
    Jacquot, Jean F.
    Foray, Marie F.
    Gadelle, Andree
    [J]. FUEL, 2007, 86 (12-13) : 1966 - 1976
  • [3] CHEMICAL-CHANGES DURING THE MILD AIR OXIDATION OF PITCH
    BARR, JB
    LEWIS, IC
    [J]. CARBON, 1978, 16 (06) : 439 - 444
  • [4] BUKHARKINA TV, 1994, PETROL CHEM+, V34, P209
  • [5] THE OXIDATIVE STABILIZATION AND CARBONIZATION OF A SYNTHETIC MESOPHASE PITCH .1. THE OXIDATIVE STABILIZATION PROCESS
    DRBOHLAV, J
    STEVENSON, WTK
    [J]. CARBON, 1995, 33 (05) : 693 - 711
  • [6] Assessment of the oxidative stabilisation of carbonaceous mesophase by thermal analysis techniques
    Fanjul, F
    Granda, M
    Santamaría, R
    Bermejo, J
    Menéndez, R
    [J]. JOURNAL OF ANALYTICAL AND APPLIED PYROLYSIS, 2001, 58 (58-59) : 911 - 926
  • [7] MODIFICATION OF COAL-TAR PITCH BY AIR-BLOWING .1. VARIATION OF PITCH COMPOSITION AND PROPERTIES
    FERNANDEZ, JJ
    FIGUEIRAS, A
    GRANDA, M
    BERMEJO, J
    MENENDEZ, R
    [J]. CARBON, 1995, 33 (03) : 295 - 307
  • [8] SINGLE-PULSE EXCITATION C-13 NMR MEASUREMENTS ON THE ARGONNE PREMIUM COAL SAMPLES
    FRANZ, JA
    GARCIA, R
    LINEHAN, JC
    LOVE, GD
    SNAPE, CE
    [J]. ENERGY & FUELS, 1992, 6 (05) : 598 - 602
  • [9] Effects of ferromagnetic inclusions on 13C MAS NMR spectra of heat-treated peat samples
    Freitas, JCC
    Passamani, EC
    Orlando, MTD
    Emmerich, FG
    Garcia, F
    Sampaio, LC
    Bonagamba, TJ
    [J]. ENERGY & FUELS, 2002, 16 (05) : 1068 - 1075
  • [10] Investigation of biomass- and polymer-based carbon materials using 13C high-resolution solid-state NMR
    Freitas, JCC
    Bonagamba, TJ
    Emmerich, FG
    [J]. CARBON, 2001, 39 (04) : 535 - 545